    Can anular cutters drill 304 stainless?

    ??

    I have to price out drilling 1/2" holes in 3/4" thick 304 stainless, any body know if the anular cutters that the mag drills use will work?



    Sent from my moto g(6) plus using Tapatalk

  2. #2
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    3,930

    Re: Can anular cutters drill 304 stainless?

    WHEW..... get on the phone with tech at Hougen

  3. #3
    Join Date
    Apr 2010
    Posts
    2,400

    Re: Can anular cutters drill 304 stainless?


    MetalMan23


    S/S is paradoxically hard and gummy - and will work harden in
    a instant.

    Drilling is not a issue: so long as you maintain constant flood
    lube/coolant, and consistent feed so you alway produce a chip.


    Opus

  4. #4
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    303

    Re: Can anular cutters drill 304 stainless?

    Just curious , Mag Drill ...1/2" hole...3/4" 304 stainless steel plate.... ??? You have a plan ?? Sounds interesting. Even high speed steel should cut stainless, just not a long as cobalt, and carbide . Speed control, and lubrication will make a big difference in tool life. How many holes do you have to make, and is it done in place or at the shop.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches

  5. #5
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,248

    Re: Can anular cutters drill 304 stainless?

    Quote Originally Posted by albrightree View Post
    Just curious , Mag Drill ...1/2" hole...3/4" 304 stainless steel plate.... ??? You have a plan ?? Sounds interesting. Even high speed steel should cut stainless, just not a long as cobalt, and carbide . Speed control, and lubrication will make a big difference in tool life. How many holes do you have to make, and is it done in place or at the shop.
    Done in shop, I know a regular twist bit will work, but I'd have to sharpen it at a lower angle than typical, and probably have to resharpen a lot, lower the rpm to 200ish and lube like crazy

    I was wondering if the anular cutter would help speed it up

    Sent from my moto g(6) plus using Tapatalk

  6. #6
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    303

    Re: Can anular cutters drill 304 stainless?

    I've used the carbide tipped hole saws from mcmaster on thicker stainless, and they last a long time in the drill press(with a hand drill the break very easily if you dont keep it straight). It should save a fair amount of time, you won't have to drill with 3 different sizes, and won't need sharpening either(depending on the quantity). Make sure you add a little cushion for extra cutters, the carbide are brittle. You never know what you'll find when your drilling thicker plate, every once in a while you find something uncuttable in there.

    Good luck
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches

  7. #7
    Join Date
    Dec 2018
    Posts
    1,717

    Re: Can anular cutters drill 304 stainless?


  8. #8
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    303

    Re: Can anular cutters drill 304 stainless?

    https://hougen.com/downloads/Hougen_...tter_Guide.pdf

    page 13, and page 16 have some good advice too.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches

  9. #9
    Join Date
    Oct 2011
    Location
    Hamlin, NY
    Posts
    1,294

    Re: Can anular cutters drill 304 stainless?

    Speed and feed. It's always slower. Lots of oil/coolant. Annular cutter yes but not sure I'd want to do that with a mag drill....

    Sent from my LM-Q710.FG using Tapatalk
    Ryan

    Miller Multimatic 200 tig/spool gun/wireless remote
    Millermatic 350P, Bernard/XR Python guns
    Miller Dynasty 350, Coolmate 3.5 & wireless remote
    CK WF1 TIG wire feeder
    Miller Spectrum 375 Xtreme
    Optrel e684
    Miller Digital Elite
    Miller Weld-Mask

  10. #10
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    4,237

    Re: Can anular cutters drill 304 stainless?

    Shouldn't be an issue. Stock up on anchor lube.
    Miller xmt304, Miller S22 p12, Miier Maxstar SD, Miller 252 w 30A, Miller super32p12, Lincoln Ranger 9, Thermal Arc 181I with spoolgun, Hypertherm 10000 ,Smith torches. Esab 161lts miniarc.

  11. #11
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,207

    Re: Can anular cutters drill 304 stainless?

    I’ve seen anular cutters/mag drill used on stainless. Not sure what
    type of stainless.(it was on a seawater intake at a power plant).
    It looked and sounded like it was a little tough on the cutting tool.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  12. #12
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,248

    Re: Can anular cutters drill 304 stainless?

    Quote Originally Posted by xryan View Post
    Speed and feed. It's always slower. Lots of oil/coolant. Annular cutter yes but not sure I'd want to do that with a mag drill....

    Sent from my LM-Q710.FG using Tapatalk
    Yeah the mag drill isn't the best way, it won't stick to the 304, but right now that's the only way I can use an anular cutter

    Quote Originally Posted by M J D View Post
    Shouldn't be an issue. Stock up on anchor lube.






    Sent from my moto g(6) plus using Tapatalk

  13. #13
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    1,709

    Re: Can anular cutters drill 304 stainless?

    We have the Hougen 904 mag drill at work and have the vacuum base for non ferrous materials. The vacuum base works great and holds the drill securely on the material.
    It just uses shop air to create the vacuum.
    If you have access to a mill you can get an adapter for annualar cutters.
    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 375 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  14. #14
    Join Date
    Oct 2011
    Location
    Hamlin, NY
    Posts
    1,294

    Re: Can anular cutters drill 304 stainless?

    Quote Originally Posted by MetalMan23 View Post
    Yeah the mag drill isn't the best way, it won't stick to the 304, but right now that's the only way I can use an anular cutter









    Sent from my moto g(6) plus using Tapatalk
    You need the optional 304/316/6061 magnet.

    Sent from my LM-Q710.FG using Tapatalk
    Ryan

    Miller Multimatic 200 tig/spool gun/wireless remote
    Millermatic 350P, Bernard/XR Python guns
    Miller Dynasty 350, Coolmate 3.5 & wireless remote
    CK WF1 TIG wire feeder
    Miller Spectrum 375 Xtreme
    Optrel e684
    Miller Digital Elite
    Miller Weld-Mask

  15. #15
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,227

    Re: Can anular cutters drill 304 stainless?

    You can mount an annular cutter in a Bridgeport mill and have at it. Or you can clamp the bar into a Kurt vise and magnatize to the sliding jaw. Or you can clamp a steel plate on the stainless and then magnatize to the steel and go to work.

    Thread cut dark is my cutting oil of choice for stainless.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX3ea,Dynasty200DX,Th ermalArc400GTSW,LincolnSW2002ea., MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig4ea,MigMax1ea.

  16. #16
    Join Date
    Oct 2016
    Location
    Delavan WI
    Posts
    437

    Re: Can anular cutters drill 304 stainless?

    How about a jig and a plasma cutter?

  17. #17
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,248

    Re: Can anular cutters drill 304 stainless?

    Quote Originally Posted by flushcut View Post
    How about a jig and a plasma cutter?
    That's too much mess for me, besides my 45xp would have a very hard time with that

    Sent from my moto g(6) plus using Tapatalk

  18. #18
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,248

    Re: Can anular cutters drill 304 stainless?

    Quote Originally Posted by xryan View Post
    You need the optional 304/316/6061 magnet.

    Sent from my LM-Q710.FG using Tapatalk
    I've been keeping my eye out for that, haven't seen one available yet

    Sent from my moto g(6) plus using Tapatalk

  19. #19
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    2,317

    Re: Can anular cutters drill 304 stainless?

    We went to almost exclusively spade drills in our machine shop, probably one of the best moves we ever made, especially when dealing with 316L and some of the other exotics we had to deal with.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  20. #20
    Join Date
    Apr 2010
    Posts
    2,400

    Re: Can anular cutters drill 304 stainless?


    MetalMan23


    Quote Originally Posted by shovelon View Post
    You can mount an annular cutter in a Bridgeport mill and have at it . . .
    The first accessory I bought for my Mill was a Hougen 12,000 Series R8
    arbor - 49849 or 49853 [they spec. the same?] 205.00$ - 1999.

    https://hougen.com/cutters/magdrill/annular-cutter-accessories.html


    I have drilled 260 - .625" holes in .250" wall S/S tube without a resharp.
    It has 'a build-in' interior flood galley. It activates [opens] when the
    'retractable center' is depressed [= no-flow when not drilling].

    This system really makes 'shop-life' good - If you have access to a mill
    don't hesitate on this option . . .


    Opus



  21. #21
    Join Date
    Jan 2005
    Posts
    3,958

    Re: Can anular cutters drill 304 stainless?

    Mill is a good way to go. I use flood coolant on tough ones.. Most cutters up to 1 inch will fit in a TG-100 collet very well. up to 1.5 a TG-150 collet works. I also modded a #40 tool holder to work with some of my 2 inch cutters.. I use the power knee to drill them. Works perfect. Although my Mag drill is awesome on my mill table too..
    Attached Images Attached Images  
    Esab 2200i-TA34
    Esab 160i caddy
    Thermal Arc LM-200 Lincoln feeders
    Thermal Arc Pee-Wee 85s
    2-Thermal 60i- 3phase (Beast)
    Thermal 38XL
    Klutch P-300i/ 120 volt













    If I agreed with you, we'd both be wrong!

  22. #22
    Join Date
    Oct 2015
    Posts
    2,320

    Re: Can anular cutters drill 304 stainless?

    depends on the room you have . !. if you have the room. clamp a steel plate to the stainless with a piece of plastic between them . Then use your mag drill on the steel plate. very slow speed and lube the cutter as you should with any annular cutter. There are several brands of annular cutters with carbide teeth. It would just be extra insurance to use one. A regular annular cutter will work and if you just have a few holes to do I would use it. If you have several holes to do it would be worth getting a carbide tipped cutter. Run the cutter much slower than you would on steel. ss work hardens very quickly so be very careful not to let the cutter have contact with the ss unless it is making a chip.

  23. #23
    Join Date
    Dec 2003
    Location
    Fairfield,CT
    Posts
    1,286

    Re: Can anular cutters drill 304 stainless?

    I made an annular cutter adapter for my Bpt. I have used a 1" hougen cutter on .500" stainless with no problems. Cuts nice. Lube or coolant as others have mentioned is needed.
    www.tjsperformance.com
    Dynasty 300 DX
    HTP 240
    HTP Microcut 380
    Hyperthem 85
    JD2 Hyd Bender and HF Hyd Ring Roller all in one =(Frankenbender)
    Bpt. Mill/DRO
    4' x 8' CNC Plasma Table
    Instagram: tjsperformance
    YT: TJS Welding and Fabrication

  24. #24
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    499

    Re: Can anular cutters drill 304 stainless?

    You can buy Morse taper to 19mm weldon shank adapters. I have one for my pillar drill. Anything over 14mm I always reach for the annular cutters now.

    Having said that, if you have a lot of holes to drill and less than ideal setup on a pillar drill/improv mag base on stainless, then I'd probably rather go for a handful of twist drills - sharpening twist drills is a LOT cheaper and easier than sharpening annular cutters. It's rather easy to burn out small cutters like 1/2" too, and gets expensive after a few breakages.

    Either annular cutter with a good rigid setup, right speed and lots of coolant, or do it with a twist drill after a 3/16 pilot.

  25. #25
    Join Date
    May 2011
    Posts
    373

    Re: Can anular cutters drill 304 stainless?

    I use annular cutters all the time on 304 and 316. I bought the R8 to annular adapter from McMaster for like $80 years ago for the Bridgeport. When I drill in place, I just put a wypeall (heavy duty paper towel) between the stainless and a 1/2" steel plate. Clamp it good and I have never had a problem. Just dont put the clamp in the back since the plate will rise and break the bit.

    I use a water heavy oil mix to keep the stainless cool. It will heat up fast, but with practice you can see when it is about to cut through, then stop and let it cool a couple seconds and oil it up, finish your cut and the slug will pop out. If you drill through while pretty hot, the slug can be a pita to remove.



    Sent from my SM-G960U using Tapatalk

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement