    How to tell ductile from gray iron?

    Can anyone here tell me how to tell the difference
    between ductile and gray cast iron? Maybe by chip/
    powder made by turning or drilling? My spark testing
    attempts haven’t really worked.
    Last edited by jpump5; 06-09-2019 at 10:20 AM.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  2. #2
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    1,725

    Re: How to tell ductile from gray iron?

    Fireball tools just made a video on this subject.



    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 375 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  3. #3
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,079

    Re: How to tell ductile from gray iron?

    If you can afford it get yourself an XRF gun they are the handiest thing since gloves with fingers!!!!

  4. #4
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,221

    Re: How to tell ductile from gray iron?

    Quote Originally Posted by psacustomcreations View Post
    Fireball tools just made a video on this subject.



    Sent from my SM-G930V using Tapatalk
    Thanks , I’ll give that a try.
    Last edited by jpump5; 06-09-2019 at 11:56 AM.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  5. #5
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,221

    Re: How to tell ductile from gray iron?

    That’s the first I’ve seen of the XRF gun.
    I’m guessing it’s a bit pricey.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  6. #6
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,079

    Re: How to tell ductile from gray iron?

    Pricey is all relative They are very handy!!! especially the newer ones.. have used em' in the scrap yard now and then... best way to shut some tweaker up when he starts howling about some cool exotic metal he wants to sell us

  7. #7
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,221

    Re: How to tell ductile from gray iron?

    Quote Originally Posted by ronsii View Post
    Pricey is all relative They are very handy!!! especially the newer ones.. have used em' in the scrap yard now and then... best way to shut some tweaker up when he starts howling about some cool exotic metal he wants to sell us
    I didn’t see a price on the site.
    Just out of curiosity, more than $1k?
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  8. #8
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    2,996

    How to tell ductile from gray iron?

    Quote Originally Posted by jpump5 View Post
    I didn’t see a price on the site.
    Just out of curiosity, more than $1k?
    Well more. Used beaten up ones on eBay are selling in the several thousands.

  9. #9
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,079

    Re: How to tell ductile from gray iron?

    Oh yeah!!!! way more

  10. #10
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,079

    Re: How to tell ductile from gray iron?

    a decent one will run you in the neighborhood of 50k

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement