    Zenith carb fuel inlet threads

    I bought a new zenith carb a few months ago and it has been working great. I noticed there was some fuel spilled beneath it today. Figured it was flooding. I found the inlet threads to be cracked where the elbow screws in. Is there anyway to fix it other than buy another carb?

  2. #2
    Join Date
    Oct 2018
    Posts
    51

    Re: Zenith carb fuel inlet threads

    Short a a new carb you might wish to JB weld your elbow in. Just make sure you allow it to fully cure before use.

  3. #3
    Join Date
    Feb 2011
    Posts
    159

    Re: Zenith carb fuel inlet threads

    That’s what I was going to try. Just trying to see if anyone else had any suggestions.

  4. #4
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    2,800

    Re: Zenith carb fuel inlet threads

    You can take it all apart and silver solder the crack. Teflon tape is the chief reason for cracks like that, dont use it.

  5. #5
    Join Date
    Feb 2011
    Posts
    159

    Re: Zenith carb fuel inlet threads

    I went ahead and ordered a new carb. At least I won’t be worried about it leaking and catching fire when I’m away from the truck.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement