    I’ve messed around with different methods for saddling pipe for fences. Here is where I am at:

    New pipe: portaband. I know a torch may be a little quicker, but the portaband doesn’t make sparks. I figured this is an important factor when working in someone’s dry pasture.

    Used pipe: definitely portaband. I’ve found the scale inside some of this pipe prevents a clean cut with a torch.

    Anyone have any experience using a Vogel notcher or a Lowbuck on used oilfield pipe? It seems like the required skill level is lower and consistency very high. With the used pipe you never know what grade/hardness you get so I don’t know if the dies will hold up?

    Anybody else have a favorite method?


    Sent from my iPhone using Tapatalk

  2. #2
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    4,687

    Re: Favorite way to field saddle pipe for fence

    I don't think a lowbuck would even wink at OP... I prefer the drycut saws as I don't have all day to wait for bandsaws and yes I know they can spit out some fairly hot bits but so does welding....

  3. #3
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    2,865

    Re: Favorite way to field saddle pipe for fence

    I made a pipe smasher out of a small hydraulic press. Cut to length, smash each end, weld it up.

  4. #4
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,438

    Re: Favorite way to field saddle pipe for fence

    I have owned a manual lowbuck. It will do schedule 40. Take a lot of effort and will wear you out if you have a lot of pipe. The thicker the pipe wall the smaller the nibble. The hydraulic upgrade might be alright, since it takes time to reposition the pipe and you will not need to wait on the machine to reset.


    Seems like the portaband with aggressive blade will be the best option, since you can take it to the pipe. Won't take long to become proficient.
    Last edited by tapwelder; 08-13-2019 at 10:16 AM.

  5. #5
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    20

    Re: Favorite way to field saddle pipe for fence

    Seventy degree angled torch. Find top & bottom of pipe, mark 1/3 of diameter back, lay torch on top of pipe, cut back to mark & roll left then right. Perfect beveled cut every time.

  6. #6
    Join Date
    May 2007
    Posts
    2,815

    Re: Favorite way to field saddle pipe for fence

    torch it. it might give the oil pipe a bit of pre-cleaning for the weld

  7. #7
    Join Date
    Jun 2016
    Location
    Aynor SC
    Posts
    3,966

    Re: Favorite way to field saddle pipe for fence

    Make a mold with a hole saw and thick pipe. Split it. Now you have a torch guide( 2 actually)

  8. #8
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,041

    Re: Favorite way to field saddle pipe for fence

    What size pipe uprights and horizontals ? All used schedule 40 pipe ? I know you don't like sparks, but I would do all the coping off site or in a dedicated safe area. A slide on template and torch is quick. Depending on size, a big old Milwaukee grinder will do the job. You didn't say what process, but I think you'll be using stick. 6010 or 6011 rod will make up for any imperfections , no problem.

  9. #9
    Join Date
    Mar 2018
    Posts
    67

    Re: Favorite way to field saddle pipe for fence

    Quote Originally Posted by BD1 View Post
    What size pipe uprights and horizontals ? All used schedule 40 pipe ? I know you don't like sparks, but I would do all the coping off site or in a dedicated safe area. A slide on template and torch is quick. Depending on size, a big old Milwaukee grinder will do the job. You didn't say what process, but I think you'll be using stick. 6010 or 6011 rod will make up for any imperfections , no problem.
    Generally sch 40, but I’ve seen some thicker wall material occasionally. I’ve got the saddle marker templates for torch cutting and made a similar template for marking for a bandsaw. Some things just have to be cut in place such as posts to get a straight top rail. Everything is welded with 6010 or 6011 depending on what I have in the trailer. Overall the bandsaw is working good, I just wanted to see if I was missing out on some miracle method.


    Sent from my iPhone using Tapatalk

  10. #10
    Join Date
    Jun 2016
    Location
    Aynor SC
    Posts
    3,966

    Re: Favorite way to field saddle pipe for fence

    Aint no miracles when it comes to modding iron.I oughta go chew some 2" sch 40 with my Mikes. Done plenty of 1 1/4. no problem. I wanna say my handrails to my cabin are 2" sch 40. Can't recall. Coconut built those himself.....and portabanded the upright posts .Used that monster swag roller for all the curves and stuff(my part)

  11. #11
    Join Date
    Jul 2016
    Location
    SE New Mexico
    Posts
    106

    Re: Favorite way to field saddle pipe for fence

    Quote Originally Posted by cwby View Post
    Seventy degree angled torch. Find top & bottom of pipe, mark 1/3 of diameter back, lay torch on top of pipe, cut back to mark & roll left then right. Perfect beveled cut every time.
    Late to the show but this is the quickest and easiest way to do it. You don't really have to have a 70 degree torch either. The technique is just a bit different. Scale inside? That's what you have hammer for. Cement lined pipe? Sell it for scrap.

  12. #12
    Join Date
    Aug 2004
    Location
    North Central Indiana
    Posts
    5,376

    Re: Favorite way to field saddle pipe for fence

    Bad order, I forgot how I got each legger line measurement the wrap around passes over.
    Last edited by tackit; 09-16-2019 at 03:07 AM.
    I've been everywhere but the electric chair, seen everything but the wind...the only two things I can't weld is the crack of dawn and a broken heart!

  13. #13
    Join Date
    Mar 2014
    Location
    Wyoming
    Posts
    156

    Re: Favorite way to field saddle pipe for fence

    I realize I'm really late in this response, but for saddle notching posts for the top rail I really like these guides:

    http://www.shurkut.net/

    Makes it really fast and consistent once you get used to it. You'd still be using a torch though. You CAN get used oilfield pipe that doesn't have the nasty coatings inside it, you might want to look into a different supplier. Some of them care and will sell you cleaner pipe, some don't.
    I have one of the manual lowbuck notchers, I haven't tried any pipe in it though. I've notched quite a bit of 14 guage 2.375 OD tubing with it though and that's a pretty good workout, I'd kinda hate to try sch 40 pipe. Maybe I need a longer handle
    Millermatic 252
    1965 SA-200 (burns oil)
    1975 Miller 55g (leaks oil)

  14. #14
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,041

    Re: Favorite way to field saddle pipe for fence

    You're not late. I mentioned a slide on templet awhile ago
    GRET minds think alike



    Sent from my iPhone using Tapatalk

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement