    Trying the 221 in stick mode without a lot of luck. Not getting much penetration. Using a 1/8 6011(DCEP) any of you guys tried this and what did you use for your setup?

  2. #2
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,228

    Re: Invertig 221

    Do you have the footpedal plugged into the port in the front of the machine? If so, disconnect it. If you leave it plugged in, the machine is expecting you to use the pedal to modulate the amperage during stick welding. So technically if you buy a slider amptrol, you can control the amperage right at the stinger (or in one hand) on-the-fly as you're stick welding.
    Last edited by Oscar; 11-09-2019 at 12:10 PM.
    1st on WeldingWeb to have a scrolling signature!

    HTP Invertig 221
    HTP ProPulse 300 MIG
    HTP ProPulse 200 MIG x2
    HTP ProPulse 220 MTS
    HTP Inverarc 200 TLP
    HTP Microcut 875SC

  3. #3
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    44

    Re: Invertig 221

    Dumb a$$ mistake Oscar got me fixed up. This machine is the bomb. Doubt I'll ever use the Bobcat again. Make just take the Invertig and plug it into the Bobcat

  4. #4
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    4,228

    Re: Invertig 221

    Let's see pics of whatcha welding!
    1st on WeldingWeb to have a scrolling signature!

    HTP Invertig 221
    HTP ProPulse 300 MIG
    HTP ProPulse 200 MIG x2
    HTP ProPulse 220 MTS
    HTP Inverarc 200 TLP
    HTP Microcut 875SC

  5. #5
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    44

    Re: Invertig 221

    Double Post Sorry

    Dumb a$$ mistake Oscar got me fixed up. This machine is the bomb. Doubt I'll ever use the Bobcat again. Make just take the Invertig and plug it into the Bobcat
    Last edited by txrpls; 11-09-2019 at 01:14 PM.

  6. #6
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    44

    Re: Invertig 221

    It was nothing special. Just running some stringers to get used to the machine.

  7. #7
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    14,105

    Re: Invertig 221

    Quote Originally Posted by Oscar View Post
    Do you have the footpedal plugged into the port in the front of the machine? If so, disconnect it. If you leave it plugged in, the machine is expecting you to use the pedal to modulate the amperage during stick welding. So technically if you buy a slider amptrol, you can control the amperage right at the stinger (or in one hand) on-the-fly as you're stick welding.
    My Invertec v250-s stick welds at a lower amperage if the foot control is plugged in.

    Only thing I don't like about the machine.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement