    Old Stick Electrodes Worth Keeping?

    Hi Guys,

    I ran across some old stick electrodes the other day cleaning out my garage. I don't know much about stick welding, nor do I own one, but I do plan to get one at some point in the future. Are these welding rods worth keeping to use at some point or are they junk? No idea what kind of electrodes they are, but I did include a number of pictures to help identify. If they are junk, can you scrap them or do they go straight in the dumpster? Thanks!
    Attached Images Attached Images     

  2. #2
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,868

    Re: Old Stick Electrodes Worth Keeping?

    What numbers are on the side of the rods near the bare end?

  3. #3
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    999

    Re: Old Stick Electrodes Worth Keeping?

    Most work it work great.
    I would put in oven for few hours just dry out the rod.

    Dave

    Quote Originally Posted by WeldCrazyDude View Post
    Hi Guys,

    I ran across some old stick electrodes the other day cleaning out my garage. I don't know much about stick welding, nor do I own one, but I do plan to get one at some point in the future. Are these welding rods worth keeping to use at some point or are they junk? No idea what kind of electrodes they are, but I did include a number of pictures to help identify. If they are junk, can you scrap them or do they go straight in the dumpster? Thanks!
    HF 170 welder
    HF 4x6 band saw
    South Bend 9N
    Mill
    B&D mag drill
    Victor torch

  4. #4
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    266

    Re: Old Stick Electrodes Worth Keeping?

    Heck yeah you should keep those! Obviously you wouldn't want to use them for code work, but for most anything else they should be fine. If the flux isn't crumbling off they should still work. That McKay Hardalloy 55 is a hard-facing rod for building up things like loader bucket cutting edge and teeth. Buying that sort of rod is pretty expensive, and handy to have around just in case you get an oddball project. I don't recognize the other packaging, but the rods should be marked. Worst case they'll be great for practicing when you get a stick welder.
    Check out my bench vise website:
    http://mivise.com


    Millermatic 252
    Miller Syncrowave 250DX
    Miller Dialarc 250
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  5. #5
    Join Date
    Jul 2008
    Posts
    2,395

    Re: Old Stick Electrodes Worth Keeping?

    Quote Originally Posted by G-ManBart View Post
    That McKay Hardalloy 55 is a hard-facing rod for building up things like loader bucket cutting edge and teeth. Buying that sort of rod is pretty expensive, and handy to have around just in case you get an oddball project.
    Just don't try to use it for anything structural, because it has like zero ductility!

  6. #6
    Join Date
    Jan 2020
    Location
    Cincinnati
    Posts
    32

    Re: Old Stick Electrodes Worth Keeping?

    Looked a bit closer and the markings i see on different rods are:

    6013
    11018M
    6012
    7011

  7. #7
    Join Date
    Jul 2008
    Posts
    2,395

    Re: Old Stick Electrodes Worth Keeping?

    Quote Originally Posted by WeldCrazyDude View Post
    Looked a bit closer and the markings i see on different rods are:

    6013
    11018M
    6012
    7011
    https://www.red-d-arc.com/pdf/Weldin...ifications.pdf

  8. #8
    Join Date
    Oct 2012
    Location
    East Van BC
    Posts
    1,119

    Re: Old Stick Electrodes Worth Keeping?

    Ooh eleventy eighteen! That’s a keeper! I would keep them all. Those are perfectly good rods.


    Sent from my iPhone using Tapatalk
    SqWave 200
    Millermatic 190
    Airco 200 AC
    Hypertherm PM45
    Boice-Crane Band Saw
    Victor O/A

  9. #9

    Re: Old Stick Electrodes Worth Keeping?

    Hardfacing rods are usually more tricky to run in my opinion. Probably not the best to practice with

    Sent from my SM-G970W using Tapatalk

  10. #10
    Join Date
    Apr 2016
    Location
    CA
    Posts
    6,712

    Re: Old Stick Electrodes Worth Keeping?

    7011 is that like a 6011 with 10k more tensil strength?
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  11. #11
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    5,242

    Re: Old Stick Electrodes Worth Keeping?

    Quote Originally Posted by N2 Welding View Post
    7011 is that like a 6011 with 10k more tensil strength?
    Well.... not necessarily

  12. #12
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    266

    Re: Old Stick Electrodes Worth Keeping?

    Quote Originally Posted by Kelvin View Post
    Just don't try to use it for anything structural, because it has like zero ductility!
    True....I should have been more specific. An oddball project that calls for a hard-facing rod
    Check out my bench vise website:
    http://mivise.com


    Millermatic 252
    Miller Syncrowave 250DX
    Miller Dialarc 250
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  13. #13
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    1,033

    Re: Old Stick Electrodes Worth Keeping?

    I make stuff from them.

  14. #14
    Join Date
    Mar 2015
    Posts
    228

    Re: Old Stick Electrodes Worth Keeping?

    Quote Originally Posted by Sberry View Post
    I make stuff from them.
    You betchee,they never get too bad for that,,,,,,,,,unless they rust,and I just sand it off and useum anyhow. Old and partially used rods in various diameteirs are my go to for gap fill backer.

  15. #15
    Join Date
    Apr 2016
    Location
    CA
    Posts
    6,712

    Re: Old Stick Electrodes Worth Keeping?

    Quote Originally Posted by Jax View Post
    You betchee,they never get too bad for that,,,,,,,,,unless they rust,and I just sand it off and useum anyhow. Old and partially used rods in various diameteirs are my go to for gap fill backer.
    Interesting. I bet that'd make a good Youtube vid, Shade Tree Welders gone crazy j/k sounds like something I'd try now that I've read about it on the forums.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  16. #16
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    1,033

    Re: Old Stick Electrodes Worth Keeping?

    The hard rods are really strong. Put old piece of hose over, bend, lots of ways to hang or attach them.
    Attached Images Attached Images   

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement