16" plate and 3/4 thick, V-groove, bend test, open root.
So I have been welding for 2 years. I welded with .045 FCAW at my last contract job at around 30 volts and 350 wire speed.
Sometimes higher settings than that or the general setting of 29 volts and 300 wire speed.
I have a test coming up using ceramic tape which I have done a bit of in the past but not as much as id like.
Any suggestions on stick out, machine settings (run colder?), angle?, weave?
Im probably overthinking it but id like to hear some suggestions.
So I have been welding for 2 years. I welded with .045 FCAW at my last contract job at around 30 volts and 350 wire speed.
Sometimes higher settings than that or the general setting of 29 volts and 300 wire speed.
I have a test coming up using ceramic tape which I have done a bit of in the past but not as much as id like.
Any suggestions on stick out, machine settings (run colder?), angle?, weave?
Im probably overthinking it but id like to hear some suggestions.