So you guys know I re-did my little Bobcat over the winter and have been making attachments for it. The old bucket is full of holes and there really isn't anything to save. It's been driving me nuts looking at it. So I cashed in some scrap and bought material today.
Finished bucket will be 36 1/2" wide and the angles are roughly based on the original with little changes here and there. I'm using 10 ga for the bucket, 1/4" for the quick attach, and a 3/8" by 3" blade. Material cost is roughly $100.
Pics of the old bucket and the material...
Finished bucket will be 36 1/2" wide and the angles are roughly based on the original with little changes here and there. I'm using 10 ga for the bucket, 1/4" for the quick attach, and a 3/8" by 3" blade. Material cost is roughly $100.
Pics of the old bucket and the material...