Threw this concoction together tonight and thought I'd share. Victor torch tip, bicycle brake cable, 5/16 flat washer, uni strut clamp and a level vile. Enjoy





I have an extra one if anyone is interested. Not sure if this is appropriate here but PM me.This is what I use http://www.magna-matic.com/mag-1000.html only mine is a bazillion years old.
We run 15 1/2 foot fine cut rotary mowers (small by turf farm standards) with 60HP spinning nine 6 pound+ blades.All I ever do is measure, scribe a line and grind to the mark. Has worked for me for over 30 years