Discussion starter · #1 ·
Hey guys, I've been welding for several years and have plenty of experience with TIG, MIG, and SMAW (uphill), but I just started learning downhill. I'm working a 5/32" 6010 root, 5/32" 8010 hot pass, and 3/16" 8010 fill & cap. Everything except for the cap is running fine for me so far, when I get to the bottom of the cap (6G position), I keep getting some undercut and considerable droop. The puddle doesn't want to go near the top edge at all.
Are there any good techniques for the bottom of the pipe? I feel like there has to be something I'm missing.