I have a 250 square wave at home. I bought it from the place I worked at, complete with a foot pedal,18 torch,20 torch, chiller,new regulator,and a thumb control for the small torch. I know I didnt pay 800 for it. Its a good welder, no problems as of yet.
You'll be happy with it, I'm sure,