66K views 65 replies 27 participants last post by  vwguy3  
230/210/200 mig, tig, stick amp outputs I'm pretty sure. The 200 is 150 on tig and stick I believe. The way I looked at it it's like the new 215 is a 211 mig machine with a maxstar 200 built in, the 200 is a 211 with a maxstar 150 built in. The biggest difference is the 215 looks like a new inverter 211 and mainly to stay inside the shop. The 200 definitely has a more durable case and made to fall off trucks doing 60mph, with the really nice Bernard mig gun included. I can't find much info on 215 but did see one listed for pre-sale on cyber weld and baker gas. I honestly don't think you can beat the price for the amperage you're getting, plus the duty cycle looks great as well. I'm gonna get a 15' Bernard gun and use it in my shop, for $1300 I don't see how it could be beat, it's a miller! The 200 is nice, plus has a $200 REBATE but it's not as high of an output. I think miller got tired of people buying a Lincoln 210 and esab rebel, they've apparently been testing and working the bugs out for awhile to be coming out with a competitive version of these machines this late to the game, but I'm glad I waited, this is gonna be one of those machines that will be back ordered a few months. The big screen and higher amps makes me think about folks waiting in line for Apple iPhones when they come out lol, but all jokes aside, call me crazy but I'm really looking forward to getting this welder in my shop, IMHO, it'll set sales records for miller..
High frequency start would be the deal breaker for someone wanting use it everyday for tig and mig. Do any dual voltage multi welders have it? Be nice to have one with a bottle of argon and 75/25 ready to go and just have to flip a switch.