WeldingWeb - Welding Community for pros and enthusiasts banner

Ua-22

7.3K views 17 replies 5 participants last post by  camorobb  
Camorobb, I have ua 60, 63 and 67. 22 is the same as 63 except its the super coupon. I once tried the 3/32 gap and was promptly scolded. Go to 1/8 gap and 1/8 rod at 98 to 100 amps. I use a #6 or7 cup for this with about 3/16 of stick out and works great. The instructors in my UA shop are some of the best in the country.
good luck
 
UA21 and 22 are tests on schedule 120, and the super coupon is schedule 160 and super cedes all the other. Its just basically a unlimited thickness cert and you will most likely not weld pipe like that very often. Its like an endurance test.