12K views 13 replies 8 participants last post by  castweld  
There is a way to repair that tank but it does not involve welding,..

There are many "gas tank liners" - that is a chemical that will reline the tank, covering and sealing the fuel from the metal.

To cover the pinholes - using a high temparature soldering iron and some lead to melt a lead coat on the outside and then a bit of body filler.

The reason for doing this is sometimes the bike is old enough that you can't find a suitable tank.