When I used to pull containers, occasionally I had to take them to the repair yard. They never bent them back............they always cut out the bad...
Serial KB119205 has 700 Hrs on it.
Low voltage output. Will barely make a Grinder turn on. Also will barely strike an arc but wont continue. Already...
Thank you all for the answers. Right now I just have fluxcore and regular steel for mig and some aluminum that I tried with argon quite unsuccessful...
I am running my Esab cV-353 from a phase converter. Works great for Spray arc, but has trouble in the short-arc.. Might try it on 460 Thermal power.....
Triggered a couple tacks at the bottom for a shelf to start on then just slowly worked my way up kinda going up 1/8 maybe and pause for a millisecond...