Reply to Thread

Post a reply to the thread: Argh! Must buy new welder.... Must buy....

Your Message

 

You may choose an icon for your message from this list

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Additional Options

  • Will turn www.example.com into [URL]http://www.example.com[/URL].

HTML

Topic Review (Newest First)

  • 08-10-2020
    Broccoli1

    Re: Argh! Must buy new welder.... Must buy....

    interesting that the IM240 states that about running off a generator but the MM252 does not.

    I've run my Mm252 off of a Honda EU 6500
  • 08-07-2020
    Louie1961

    Re: Argh! Must buy new welder.... Must buy....

    I believe it is phase angle controlled or a combined phase angle/zero current crossover controlled firing pattern. Just my wild *** guess though.

    http://www.freepatentsonline.com/3883714.html
  • 08-07-2020
    Beuford

    Re: Argh! Must buy new welder.... Must buy....

    Quote Originally Posted by Willie B View Post
    Inverter VS Transformer?
    That is NOT a statement, I don't know.
    No, they are both transformer units.

    I think I answered this question myself. The schematics for the 240 shows a pair of SCR (silicon controlled rectifiers) on the output circuit. These can be phase-modulated to control current flow, but because of how they accomplish this the voltage/current gets pushed out of phase (more so than just from the induction of the transformer). The resulting phase shift reduces power transfer for a given input voltage and current.

    You can see this in the specifications as an increase in peak current requirements for a given output. From the Hobart spec sheets for these products you can see that the Ironman 240 does put out a somewhat higher rated welding current (200A vs 175A for the Ironman 230), but it requires a much larger input current to achieve that output (~51A @ 240VAC for the Ironman 240 vs ~31A @ 240VAC for the Ironman 230).

    The benefit of having the SCRs is that you can control output voltage with an electronic circuit rather than a tap switch, and they can replace a contactor (big relay) on the output that can wear out. The drawback is that more input current is required for a given output. The use of these SCRs is also probably why Hobart does not recommend running the Ironman 240 from a generator.

    Beuford
  • 08-07-2020
    Willie B

    Re: Argh! Must buy new welder.... Must buy....

    Inverter VS Transformer?
    That is NOT a statement, I don't know.
  • 08-06-2020
    Beuford

    Argh! Must buy new welder.... Must buy....

    I hate when something I want is discontinued - it makes me go buy one before they disappear. I'm now the proud owner of a Hobart Ironman 230.

    I looked at the new Ironman 240, and I did note that the 240 specs were very close to the Miller 252 which was interesting. But for me simple beats complicated; I prefer taps over one more circuit board to fail. The other thing that swayed me is that the new 240 spec sheet had this note (where the 230 did not):

    "Note: Running off of generator power is not recommended for the IronMan 240."

    I don't like limitations like this, particularly since I've had to run off generators before. Sometimes it's just more convenient than a REALLY long extension cord. I wonder if this is a function of the infinitely variable voltage system on the 240?

    BTW - does anyone know how the infinitely variable voltage output systems actually work? I'm wondering if its an inductance or phase control type system. I ask this because I noted that the KVA of the 252 and new 240 are MUCH higher than the 230. The 230 has a KVA of 7.4 for an output of 6.3KW (85%), while the 240/252 has a KVA 11.4 for an output of 7.1KW (62%). It seems that the power factor on the 230 is much better at rated load than the 240/252, and the only thing I can think of is if they are somehow manipulating input voltage/current phase on the 240/252 as a means of controlling output voltage.

    Anyone know what's going on here?

    Just curious.

    Beuford

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,251,810.73123 seconds with 22 queries