Reply to Thread

Post a reply to the thread: Wazer water jet

Your Message

 

You may choose an icon for your message from this list

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Additional Options

  • Will turn www.example.com into [URL]http://www.example.com[/URL].

Topic Review (Newest First)

  • 04-28-2021
    Mac's Crew

    Re: Wazer water jet

    Quote Originally Posted by N2 Welding View Post
    Water jet looks pretty neat. Do they have a max cut depth like plasma? Also do they have a cleaner cut line that is not angled like plasma?
    We have 2 water jets and a plasma table in our department at work, yeah we get some cool toys. Max cut? I have seen the flowmax cut 6" 4130 and it was OK, but it runs at 27k psi. The Omax took on the same job about a week later, ran underwater, and under half the time. Pristine waterjet kerf marks... differenct 30 years of technology and 23K psi as in it runs at 50K psi. They are a cleaner cut line by far, but higher cost of consumables for what we do at work. I haven't seen too much AL cut on a plasma that didn't take the same amount of time to grind off the slag that was left on it. Our welders take the waterjetted parts knock the scale off them and weld, or buff for AL.

    As a machinist they both suck for true square cuts, but higher pressure on the waterjet is better than plasma. You get deflection with both processes, but it all depends on thickness of material, material type, and psi of the waterjet for your finish. Our Omax is 5 axis, and can have very little deflection on 1/2" but 1 inch... forget it, there will be deflection.
  • 04-27-2021
    bassboy1

    Re: Wazer water jet

    Quote Originally Posted by jrw159 View Post
    I know. Just went through a bit of it and tried to mill it. LOL

    We took it to a water jet company. Took awhile. Just wondered if this one had the capacity to handle it.

    jrw159
    Definitely cheaper to sub it out. The wazer machine uses glorified pressure washer components, so it cuts incredibly slow, and uses an insane amount of garnet to make up for the lack of pressure. There's a reason the 'starter kit' comes with a literal pallet of garnet.

    Take a look at the cut time and garnet use on their sample part for various metals. I don't see the dimensions listed, but I think I remember reading that the part is less than 3 x 4".

    https://www.wazer.com/materials#.category-metal
  • 04-27-2021
    jrw159

    Re: Wazer water jet

    Quote Originally Posted by walker View Post
    Just about any process will cut it, just a matter of how long it takes.
    I know. Just went through a bit of it and tried to mill it. LOL

    We took it to a water jet company. Took awhile. Just wondered if this one had the capacity to handle it.

    jrw159
  • 04-27-2021
    N2 Welding

    Re: Wazer water jet

    Water jet looks pretty neat. Do they have a max cut depth like plasma? Also do they have a cleaner cut line that is not angled like plasma?
  • 04-27-2021
    Lis2323

    Re: Wazer water jet

    Quote Originally Posted by cwby View Post
    That one sold for $2000. Would have been a great deal - If I had $2k!
    No kidding. If I knew you personally I would have loaned you the money! (Or maybe not! [emoji23])


    Sent from my iPad using Tapatalk
  • 04-26-2021
    cwby

    Re: Wazer water jet

    That one sold for $2000. Would have been a great deal - If I had $2k!
  • 04-26-2021
    walker

    Re: Wazer water jet

    Quote Originally Posted by jrw159 View Post
    Will it cut Hardox 450?

    jrw159
    Just about any process will cut it, just a matter of how long it takes.
  • 04-26-2021
    jrw159

    Re: Wazer water jet

    Will it cut Hardox 450?

    jrw159
  • 04-17-2021
    VaughnT

    Re: Wazer water jet

    Looks like a pretty decent machine if you want a water jet.





    I thought about getting one so I could cut out pre-forms to forge into hinge straps or bottle openers. Never pulled the trigger, though, because even that low-level price tag is way out of my budget.

    It certainly looks like it'd be great for a small shop when you compare it to similarly sized laser and plasma cutting tables.
  • 04-16-2021
    Mac's Crew

    Re: Wazer water jet

    Fireball Tool did a review of it, I don't remember when, or what he said just that Jason did a review
  • 04-16-2021
    cwby

    Wazer water jet

    Anyone ever heard of a Wazer Desktop Water Jet? Looks pretty cool & ONLY $8k.

    https://www.wazer.com/

    There is one in an auction I am watching - wonder what it will sell fpr?