    Radiation concerns and 2% Thoriated Tungsten

    Thanks to Wildcat, here is a chart that shows the radiation levels and it's estimated effect on lifespan.

    As Taken from Wildcat's original post:

    Thoriated tungsten measurement is in microrads.

    So to Clarify smoking =8000 milirads
    Thoriated tungsen =1600microrads

    Here are a few stats to compare it to
    8000 milirads = 8 rads
    1600 microrads = .0016 rads
    1 rad = 1 rem

    Comparative risk exposure estimated days of life lost
    20% overweight 985 days
    Average alcohol consumption 130 days
    Occupational radiation exposure@
    5.0 rem/year 32 days
    0.5 rem/year 3 days
    0.0016/year 6.912 minutes


    Therefore if you worked with Thoriated Tungsten for 45 years 5 days a week, 8 hours a day you would loose 5.18 hrs off your life.

    This is assuming all appropriate precations are taken.
    Reference for the data here (accept Thoriated Tungsten, I had to calculate the dose rate myself)is
    THE LOS ALAMOS RADIATION MONITORING NOTEBOOK
    Last edited by ZTFab; 07-31-2007 at 08:25 PM.
    http://all-a-cart.com

    Welding Cart Kits and accessories
    Quick reply to this message Reply  

Closed Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,292,047.20146 seconds with 17 queries