    Pretty welds don’t mean a good weldName:  448F4853-38F1-4047-84C5-3AA1491EF9B6.jpg
Views: 3243
Size:  105.7 KBName:  7C0C2675-F6A9-4563-8D1D-4B559AF97E0E.jpg
Views: 3325
Size:  93.5 KB

  2. Likes Joegreen02, bfjou812 liked this post
  3. #2527
    Join Date
    Sep 2020
    Location
    South Texas
    Posts
    154
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Bls repair View Post
    Pretty welds don’t mean a good weldName:  448F4853-38F1-4047-84C5-3AA1491EF9B6.jpg
Views: 3243
Size:  105.7 KBName:  7C0C2675-F6A9-4563-8D1D-4B559AF97E0E.jpg
Views: 3325
Size:  93.5 KB
    Terex machine? I’ve fixed a group of these quick hitches with similar issues


    Sent from my iPhone using Tapatalk

  4. #2528
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,918
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Cat brandedName:  5256800C-06EE-40C3-8FE6-0FB8AA72EFB6.jpg
Views: 3196
Size:  99.3 KB

  5. Likes Joegreen02 liked this post
  6. #2529
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Name:  AE4CB618-BFB7-4D43-A84B-2AE334B86F89.jpg
Views: 2822
Size:  163.7 KBName:  228080F8-112B-4F6C-A6FC-E260AB8E5D6D.jpg
Views: 2873
Size:  145.6 KBmy dad broke this and he is 65 years old. I made sure it wouldn’t come off again

  7. Likes ronsii, Albin liked this post
  8. #2530
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,894
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Great photos
    This why you do not to use solid wire.

    Dave

    Quote Originally Posted by Bls repair View Post
    Pretty welds don’t mean a good weldName:  448F4853-38F1-4047-84C5-3AA1491EF9B6.jpg
Views: 3243
Size:  105.7 KBName:  7C0C2675-F6A9-4563-8D1D-4B559AF97E0E.jpg
Views: 3325
Size:  93.5 KB

  9. Likes Joegreen02 liked this post
  10. #2531
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Just gota turn up the heat

  11. Likes snowbird liked this post
  12. #2532
    Join Date
    Mar 2021
    Location
    italy
    Posts
    2
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    It is not welding. It is like sponge. You can find any kind of weld defects including gas pore, under cut, less penetration, cracks...))
    Only a micro crack inside the weld bead can ruin HUGE projects! Do you know?

  13. #2533
    Join Date
    Dec 2018
    Location
    Southern California
    Posts
    1,127
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Don't even need to gouge or grind that one out, just peel it off like slag.

    I bet a cold chisel or air hammer could take that weld out in one solid caterpillar (pun intended). I would mail it to CAT corporate and tell them to frame it as a monument to their proud heritage of craftsmanship (sarcasm intended).

  14. Likes snowbird, DLHCC liked this post
  15. #2534
    Join Date
    Jun 2018
    Location
    NC
    Posts
    1,561
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    This guy told me he paid some shop a hundred bucks to reweld the expanded metallic on his drop-down ramp because it had come loose last year....... It didn't last very long.

    Name:  20210307_204053-COLLAGE.jpg
Views: 2222
Size:  223.9 KB
    ***********************

    CR

  16. #2535
    Join Date
    Jun 2014
    Location
    Winter Haven ,Fl.
    Posts
    136
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by William McCormick View Post
    He took one bead at a time in a whole new way.

    Sincerely,

    William McCormick
    I read a little of the original post, at least the person owns the welds
    as being terrible . Gotta give him some credit for that...............

  17. #2536
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: Welding Fail! post pics here.


    Bls repair


    Quote Originally Posted by Bls repair View Post
    Pretty welds don’t mean a good weld

    Name:  7C0C2675-F6A9-4563-8D1D-4B559AF97E0E.jpg
Views: 3325
Size:  93.5 KB
    This is classic 'Hinge [joint] Failure' - the weld peeled,
    because it was unrestrained = welded on the wrong
    side . . .

    Pretty . . . and not uncommon on OEM equipment . . .



    motolife313


    Quote Originally Posted by motolife313 View Post
    Name:  228080F8-112B-4F6C-A6FC-E260AB8E5D6D.jpg
Views: 2873
Size:  145.6 KB

    . . . I made sure it wouldn’t come off again
    An 8X+ . . . 'wash-pass with under-cut' on sections
    this thin = guaranteed/refailure . . .

    hth


    Opus



    .

  18. Likes snowbird liked this post
  19. #2537
    Join Date
    Jan 2009
    Location
    Sonoma County, Northern California
    Posts
    1,140
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by CrookedRoads View Post
    This guy told me he paid some shop a hundred bucks to reweld the expanded metallic on his drop-down ramp because it had come loose last year....... It didn't last very long.

    Name:  20210307_204053-COLLAGE.jpg
Views: 2222
Size:  223.9 KB
    Good grief.
    * Amico MIG-130A Flux, Dual Voltage. Truly portable!
    * HF MIG-180 with all the mods. Heavy.
    * Grizzly H8153 Stick/Tig 130/160.
    * Wards PowrKraft AC-230. Stick & carbon arc.

  20. #2538
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,894
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    It look great for next welder.
    I too have had repair bad welds on trailers.
    Easy money for a good welder.

    Dave

    Quote Originally Posted by CrookedRoads View Post
    This guy told me he paid some shop a hundred bucks to reweld the expanded metallic on his drop-down ramp because it had come loose last year....... It didn't last very long.

    Name:  20210307_204053-COLLAGE.jpg
Views: 2222
Size:  223.9 KB

  21. #2539
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,918
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    What I do is start the puddle on the tube then quickly drag the puddle to the stretched steel then quickly pull out of the puddle.

  22. Likes snowbird liked this post
  23. #2540
    Join Date
    Jun 2018
    Location
    NC
    Posts
    1,561
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by Bls repair View Post
    What I do is start the puddle on the tube then quickly drag the puddle to the stretched steel then quickly pull out of the puddle.
    I don't think the guy who welded it knows what a puddle is.
    ***********************

    CR

  24. Likes California, snowbird liked this post
  25. #2541
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by CrookedRoads View Post
    I don't think the guy who welded it knows what a puddle is.
    That wasn't a guy... That was a bird.

  26. Likes DLHCC liked this post
  27. #2542
    Join Date
    Jan 2010
    Posts
    33
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Nice tow hook

    Sorry the pictures loaded sideways
    Attached Images Attached Images   

  28. #2543
    Join Date
    Mar 2004
    Location
    hueytown, ala
    Posts
    214
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Name:  hook1.jpg
Views: 1767
Size:  85.6 KBName:  hook2.jpg
Views: 1769
Size:  70.0 KB
    Last edited by jniolon; 03-25-2021 at 12:51 PM.

  29. Likes ckr427 liked this post
  30. #2544
    Join Date
    Mar 2021
    Posts
    1
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by ckr427 View Post
    Nice tow hook

    Sorry the pictures loaded sideways
    Someone tried overhead 7018 the first time right there me thinks.

  31. #2545
    Join Date
    Nov 2014
    Location
    North Readung, MA
    Posts
    105
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by sea2summit View Post
    Someone tried overhead 7018 the first time right there me thinks.
    I vote for an idiot with a MIG/FC welder who watches too many interweb videos of other ****ty welders making a bunch of tack welds and calling it a good weld instead of laying a nice long bead (thin sheet metal work not withstanding but in that case I could argue to get a pulsed MIG welder or use TIG)
    Miller Dynasty 200 DX
    Millermatic 211
    Lincoln X-Tractor 1GC
    Hypertherm Powermax 1000

  32. Likes 12345678910 liked this post
  33. #2546
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    939
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Well the first pick of the tow hook had me worried but then the second pic made it all better!
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  34. Likes bfjou812 liked this post
  35. #2547
    Join Date
    May 2020
    Location
    Arizona
    Posts
    1,477
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    I feel (almost) compelled to reply "Wasn't me" to a lot of these...
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  36. Likes 12345678910 liked this post
  37. #2548
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    New coping method.


    .

    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  38. Likes California, 12V71, whtbaron liked this post
  39. #2549
    Join Date
    Nov 2010
    Posts
    131
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    it hasn't failed yet...

  40. #2550
    Join Date
    Jan 2009
    Location
    Sonoma County, Northern California
    Posts
    1,140
    Post Thanks / Like

    Re: Welding Fail! post pics here.

    Quote Originally Posted by jmm03 View Post
    it hasn't failed yet...
    WTF???

    MIG except he didn't have any gas?
    * Amico MIG-130A Flux, Dual Voltage. Truly portable!
    * HF MIG-180 with all the mods. Heavy.
    * Grizzly H8153 Stick/Tig 130/160.
    * Wards PowrKraft AC-230. Stick & carbon arc.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,247,520.88717 seconds with 21 queries