Nothing like a good welding fail pic or video... so here is one I just happened to run across
the whole thread is here
For the lazy folks here are the pics.
![]()
Nothing like a good welding fail pic or video... so here is one I just happened to run across
the whole thread is here
For the lazy folks here are the pics.
![]()
Tiger Sales: AHP Distributor www.tigersalesco.com
AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; Thermal Dynamics 60i plasma.
For Sale: Cobra Mig 250 w/ Push-pull gun. Lincoln Wirematic 250
It seems that the really bad welds are always on something that moves.
Looks like my brother started another project. LOL![]()
I hate being bi-polar it's awsome
My Heroes Have Always Been Cowboys
Who welds this and says "ok thats looks about right"?
Adam M
Morales Ranch
I may never be the same. I went to the blog. I can't believe there are people in the gene pool like this. I need to go purge my brain with a hammer.
poor lincoln
^ haha it only took me 10 rods...
Adam M
Morales Ranch
Lincoln Idealarc 250 (circa 1962)
Lincoln Weldpak 155 w/Mig Kit
Lincoln Squarewave TIG 175
ZTFab, guess we cannot have a welding fail thread without Danny making an appearance.
For those who don't know, that is Danny (the redneck welding expert) in the second video
![]()
Tiger Sales: AHP Distributor www.tigersalesco.com
AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; Thermal Dynamics 60i plasma.
For Sale: Cobra Mig 250 w/ Push-pull gun. Lincoln Wirematic 250
Festering pus pocket hemorrhoid of a weld.
OK guys..
Let's leave Danny out of this..
We had to deal with him already once here and I do not want a repeat..
Therefore I am about to edit the posts with his likeness in them to prevent more "Stalking"from him and his peers....
Sorry guys I have had enough of this gentleman..
OK with you?
...zap!
I am not completely insane..
Some parts are missing
Professional Driver on a closed course....
Do not attempt.
Just because I'm a dumbass don't mean that you can be too.
So DON'T try any of this **** l do at home.
I am not completely insane..
Some parts are missing
Professional Driver on a closed course....
Do not attempt.
Just because I'm a dumbass don't mean that you can be too.
So DON'T try any of this **** l do at home.
This was a cage on a class 5 that was racing up till last month when it was brought to me to get a little update... I ripped everything out and started over..
I am not completely insane..
Some parts are missing
Professional Driver on a closed course....
Do not attempt.
Just because I'm a dumbass don't mean that you can be too.
So DON'T try any of this **** l do at home.
Last edited by dumb as a stump; 07-10-2012 at 08:22 PM.
Miller thunderbolt 250
Decastar 135E
Recovering tool-o-holic
ESAB OA
I have been interested or involved in Electrical, Fire Alarm, Auto, Marine, Welding, Electronics ETC to name a just a few. So YES you can own too many tools.
[ame]http://www.youtube.com/watch?v=mH2PoF10lFQ&feature=player_detailpage[/ame]
Miller Synchrowave 180 SD
Lincoln PowerMig 255
Hypertherm Powermax 45
Torchmate 2x2
Victor O/A
There are so many things wrong with that viseo, I can't even begin to count.
You didn't build that.
'85 Miller AEAD-200LE
We can all aspire to have fitup like that.![]()
An attempt to attach new rear axle brackets and some sort of bracing by a friend of mine.
Car still drives to work almost daily with a BBC and 4 speed.