Re: Welding Fail! post pics here.
Pretty welds don’t mean a good weld
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding Fail! post pics here.

Originally Posted by
Bls repair
Pretty welds don’t mean a good weld


Terex machine? I’ve fixed a group of these quick hitches with similar issues
Sent from my iPhone using Tapatalk
-
Re: Welding Fail! post pics here.
Cat branded
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding Fail! post pics here.

my dad broke this and he is 65 years old. I made sure it wouldn’t come off again
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding Fail! post pics here.
Great photos
This why you do not to use solid wire.
Dave

Originally Posted by
Bls repair
Pretty welds don’t mean a good weld


-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Welding Fail! post pics here.
Just gota turn up the heat