    Hey zank Jody on welding tips and tricks gave you a shout out. Here's the video

    Will Supports Autism Awareness
    My Toys
    BobCat 225 PLus
    Millermatic 130
    Miller Spectrum 300 Cutmate
    Everlast Power Tig 185 Micro

    April is Autism Month .

  2. #52
    Join Date
    Nov 2011
    Posts
    295
    Post Thanks / Like

    Re: The bicycle thread

    Figured that you guys will like this. Just finished this earlier today...
    Motorboating...in the Cleavage of the Tetons

  3. #53
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    Still hot.


    Mark O by Zanconato Custom Cycles, on Flickr

  4. #54
    Join Date
    Dec 2009
    Location
    Las Vegas, Nevada, USA
    Posts
    534
    Post Thanks / Like

    Re: The bicycle thread

    Mike, As always, gorgeous weld. Nice job.

    That last photo sparks a couple of questions.
    --Do you make an attempt to control the direction of the "stacks of dimes" on the weld? do you go all the way around the joint in the same direction, ending up with the last round 'dime' in the most non-visible location? (((((((((O(((((((((
    --Isn't there enough room in the Anvil jig to weld complete joints, or is that strictly a tack up holding fixture?

    --Zip
    Last edited by zipzit; 04-13-2013 at 06:31 PM.

  5. #55
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    Thanks, LB. I do best going clockwise around the joint. I break the joint up into quadrants and do 10:30 to 1:30 and 4:30 to 7:30 first. I do this on the three joints (I leave the BB for last) of the frame. This helps keep the alignment pretty straight. In most cases, it's nearly the same as just tacked. Then I'll do the ears. Basically it pulls to the side you do second. So if I need to pull the DT/HT joint to the drive side, I'll do the non drive side ear first. All that said, each joint will have two stops, and I orient them off-axis at about 10:30 and 4:30.

    I only tack in the fixture. The metal is going to do what it's going to do as it reacts to the heat. So I think it's best to weld it on the bench rather than constrain it in the jig. In terms of access, I could braze a whole joint in the jig, but I couldn't weld one in it. There just isn't enough room or line of sight for me.

    Hope that helps. And I will take some pictures of the beer bottle drill this week.

  6. #56
    Join Date
    Nov 2011
    Posts
    295
    Post Thanks / Like

    Re: The bicycle thread

    Wow, those welds are humbling. That is some hand-eye mastery.
    Not nearly in the same league, but this is what I have been up to...

    Here is the beginning of a whole new product line, using cogs tig welded together to create really unique, memorable items. I will be doing a lot with lights, including sconces, outdoor lighting, hotel/restaurant lighting, tea lights, and more. Here is a little taste of much, much more to come. This one can be hung, put on a table, mounted as a sconce, or used to throw incredible shadows. I haven't seen anyone doing exactly this. I will be adding fused and stained glass to the insets, check it out!




    This is hung as a corner light, porch light, or sconce.


    Here is the bottom (for on a table) or top (chandelier)


    And here is a cute little tea light. I will be adding fused glass to the cogs. (it's not totally welded together yet)
    The ladies are gonna dig this one by the bath...



    MUCH more on the way
    Motorboating...in the Cleavage of the Tetons

  7. #57
    Join Date
    Nov 2011
    Posts
    295
    Post Thanks / Like

    Re: The bicycle thread

    Glass is next on the 'to learn' list.
    I will be cutting and soldering the fused glass, that's not too hard.
    Right now I am all about figuring out Tig!
    Motorboating...in the Cleavage of the Tetons

  8. #58
    Join Date
    Dec 2009
    Location
    Greenville TX
    Posts
    942
    Post Thanks / Like

    Re: The bicycle thread

    hi zank, here's some of my wet paint.. a couple of close-ups on fillet brazed frames, if you dont mind me posting in your thread
    Attached Images Attached Images    
    thermal arc 252i - millermatic 350P - miller XMT, cp300ts, 30a 22a feeders, buttload of other millers, handfull of lincolns, couple of esabs - Hypertherm 1250 G3

  9. #59
    Join Date
    Nov 2011
    Posts
    295
    Post Thanks / Like

    Re: The bicycle thread

    Gary would approve.
    Motorboating...in the Cleavage of the Tetons

  10. #60
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    Beautiful paint. And please post more. This thread is for everyone!

    rideit, I love the disk rotor. Great touch. All of your stuff looks sweet.

  11. #61
    Join Date
    Oct 2012
    Location
    East Van BC
    Posts
    1,124
    Post Thanks / Like

    Re: The bicycle thread

    Nice seat tube cluster! That colour change paint shows it off well.
    SqWave 200
    Millermatic 190
    Airco 200 AC
    Hypertherm PM45
    Boice-Crane Band Saw
    Victor O/A

  12. #62
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread


  13. #63
    Join Date
    Nov 2011
    Posts
    295
    Post Thanks / Like

    Re: The bicycle thread

    BEAUTIFUL!
    Are you doing a 'sleeve' at the seatpost junction (seperate seat tube) for strength, or manufacture ease? (Matching ideal post size to tube set?)
    I think I see why, but I would love to hear your take?
    Motorboating...in the Cleavage of the Tetons

  14. #64
    Join Date
    Jun 2012
    Posts
    67
    Post Thanks / Like

    Re: The bicycle thread

    Quote Originally Posted by rideit View Post
    Figured that you guys will like this. Just finished this earlier today...
    Do you weld each chain link to keep the chain like that?

  15. #65
    Join Date
    Nov 2011
    Posts
    295
    Post Thanks / Like

    Re: The bicycle thread

    Quote Originally Posted by Hanzelz View Post
    Do you weld each chain link to keep the chain like that?
    Yup. Little Tig tack, four per 1" link. It's kind of time consuming, but everyone asks about it, so it's pretty unique.
    Motorboating...in the Cleavage of the Tetons

  16. #66
    Join Date
    Apr 2012
    Location
    Athens - Greece
    Posts
    505
    Post Thanks / Like

    Re: The bicycle thread

    Nice touch on the seat tube zank. I wonder why most manufacturers don't do this (outside from cost and extra work of course but we are talking expensive frames anyway).
    I have seen way too many frames crack in that area

  17. #67
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    Exactly. I used to epoxy in a composite shim, but have gotten away from that. The welded-in extension serves three purposes.
    1) it allows me to use a 27.2 mm seatpost with a 31.8 mm seat tube. I hate forcing customers into an oddball post size.
    2) it really beefs up that area, especially at the bottom of the slot and relief hole.
    3) it makes doing a repair a lot easier than trying to remove a shim that has been bonded in with 3M DP420.

    And it's only about 25 grams heavier overall. It's more work, but I like it better.

  18. #68
    Join Date
    May 2012
    Location
    Fishers, IN
    Posts
    51
    Post Thanks / Like

    Re: The bicycle thread

    Nice work. Do you finish your bikes with components?

    If so, do you buy them retail or have you found a wholesaler that will sell to frame builders who do not have a retail store?

    Thanks

  19. #69
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    As many complete bikes as I can. Yes, the big wholesalers will work with framebuilders, but we have to put together a pretty good case without a store front.

  20. #70
    Join Date
    Jun 2011
    Location
    Boise, ID
    Posts
    283
    Post Thanks / Like

    Re: The bicycle thread

    Here's a bike I built about 4 years ago. It was a fun little project. Wish I wouldn't have sold it.....
    Attached Images Attached Images   
    Miller Dynasty 200
    Millermatic 211
    Instagram?.... find me @ WELD_MEDIC

  21. #71
    Join Date
    Feb 2010
    Posts
    20
    Post Thanks / Like

    Re: The bicycle thread

    Do you guys have trouble with the threads after welding. I noticed the welds were close to the crank threads.

  22. #72
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    I have some bronze heatsinks really cut down on the distortion of the bottom bracket shell, seat tube, and head tube. I can usually still thread a BB in by hand after welding.

  23. #73
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: The bicycle thread

    Back from powdercoat.


    Aaron B by Zanconato Custom Cycles, on Flickr


    Aaron B by Zanconato Custom Cycles, on Flickr


    Aaron B by Zanconato Custom Cycles, on Flickr


    Aaron B by Zanconato Custom Cycles, on Flickr

  24. #74
    Join Date
    Oct 2012
    Location
    East Van BC
    Posts
    1,124
    Post Thanks / Like

    Re: The bicycle thread

    Quote Originally Posted by kevinstj View Post
    Do you guys have trouble with the threads after welding. I noticed the welds were close to the crank threads.
    Mere mortals have to chase the threads a bit. Nice work Zank
    SqWave 200
    Millermatic 190
    Airco 200 AC
    Hypertherm PM45
    Boice-Crane Band Saw
    Victor O/A

  25. #75
    Join Date
    Jun 2012
    Posts
    67
    Post Thanks / Like

    Re: The bicycle thread

    Quote Originally Posted by rideit View Post
    Yup. Little Tig tack, four per 1" link. It's kind of time consuming, but everyone asks about it, so it's pretty unique.
    Close up please.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,607,092,620.85164 seconds with 12 queries