Page 3 of 4 FirstFirst 1234 LastLast
Results 51 to 75 of 95

Thread: 09 wrangler one ton build

  1. #51
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    So, minor setback.
    Built a "shoe" to flatten the bottom of my crossmember where the upper wishbone brackets are going.

    The main bracket runs right where the driveshaft will be after only 2" of up travel.
    So, I stalled out on the project trying to think of a solution.

    The more I looked at the shoe, the more I hated it.
    Looked like a redneck fix, even if I made it work.
    The cuts I did, didn't match the contours of the crossmember, and yea, just ugly. (Pic attached of it clamped in place)

    So, to get the flat bottom., and enough meat to mount the brackets on the face, I'm going to be cutting g the crossmember out completely, and replacing with 2x2x1/4 square tube with flanges on the ends to mount to the frame.

    This project is way more in depth than I expected.


    This is the shoe/brackets that are a $100+ fail
    Name:  IMG_20151201_184930_01.jpg
Views: 675
Size:  64.5 KB

  2. #52
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    New crossmember and flanges
    Christmas and new years are taking priority, so I'll be working on it the next weekend after.
    Crossmember with new brackets and joints, just to see how the brackets fit
    Name:  IMG_20151220_121834.jpg
Views: 615
Size:  47.6 KB
    Foam core flange prototype
    Name:  IMG_20151220_123024.jpg
Views: 607
Size:  30.3 KB

    Got the flanges cut
    Name:  IMG_20151224_074449_01.jpg
Views: 613
Size:  63.7 KB

  3. #53
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Name:  IMG_20160103_123203.jpg
Views: 681
Size:  52.2 KB

    Name:  IMG_20160103_124854.jpg
Views: 681
Size:  41.4 KBName:  IMG_20160103_125356.jpg
Views: 687
Size:  34.8 KB

  4. #54
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    1/4' square tube gussets...because......gussets.
    Name:  IMG_20160124_131221.jpg
Views: 598
Size:  63.5 KB

  5. #55
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    9/16 all thread to secure and align tabs with joints , 16" apart.
    Name:  IMG_20160131_102412.jpg
Views: 574
Size:  73.7 KB

    3/8 tabs beveled on both sides to about 1/16 for full penetration.
    Name:  IMG_20160131_102509.jpg
Views: 576
Size:  44.5 KB

  6. #56
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Welded up
    Name:  IMG_20160131_115316.jpg
Views: 467
Size:  38.6 KB
    Factory versus "full retard" control arm tube.
    Name:  IMG_20160131_154245.jpg
Views: 543
Size:  29.4 KB

    Name:  IMG_20160131_155400.jpg
Views: 551
Size:  75.5 KB

  7. #57
    Join Date
    Mar 2006
    Location
    Yuma, Arizona
    Posts
    3,356
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Name:  retard.jpg
Views: 472
Size:  10.8 KB
    Lincoln Power Mig 350MP - MIG and Push-Pull
    Lincoln Precision TIG 275,Undercart cooler,Foot/Finger Amptrollers
    Lincoln Hobby-Weld 110v
    Lincoln SP-200 MIG and Hi-Freq Tig
    CK TIG TORCH, gas diffuser, pyrex cup
    Thermal Dynamics Cutmaster 101

  8. #58
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Quote Originally Posted by Joker11 View Post
    Name:  retard.jpg
Views: 472
Size:  10.8 KB
    What fun is doing things half retard?

  9. #59
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Name:  IMG_20160131_155510.jpg
Views: 516
Size:  31.4 KB

  10. #60
    Join Date
    Mar 2006
    Location
    Yuma, Arizona
    Posts
    3,356
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Weld that bad boy up already!

    Sent from my SM-N900V using Tapatalk
    Lincoln Power Mig 350MP - MIG and Push-Pull
    Lincoln Precision TIG 275,Undercart cooler,Foot/Finger Amptrollers
    Lincoln Hobby-Weld 110v
    Lincoln SP-200 MIG and Hi-Freq Tig
    CK TIG TORCH, gas diffuser, pyrex cup
    Thermal Dynamics Cutmaster 101

  11. #61
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Kinda the layout
    Name:  IMG_20160219_202700.jpg
Views: 403
Size:  48.3 KB
    The lo g left hand tube is going to be bent to form a wishbone, approximately where the level is then plated in the middle.
    Name:  IMG_20160219_205634.jpg
Views: 400
Size:  42.4 KB

  12. #62
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Quote Originally Posted by Fnord5 View Post
    Name:  IMG_20160131_155510.jpg
Views: 516
Size:  31.4 KB
    Had the tube beveled for welding.
    Name:  IMG_20160219_205050.jpg
Views: 400
Size:  23.3 KB

  13. #63
    Join Date
    Oct 2008
    Location
    New Jersey (yeah it sucks)
    Posts
    693
    Post Thanks / Like

    Re: 09 wrangler one ton build

    What do you do to keep the control arm threads from distorting during welding??? Any plug weld from the side??? How do you position the arm for welding???
    When do you think the rig will be ready for wheeling?? Nice build!!!

  14. #64
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    I've coated the joint stud with anti-seize (loctite copper)
    Going to weld the circumference, then gently rotate the joint to make sure everything stays kosher as it cools.
    Haven't figured out how I'll position the arms, Probably make some v grooves in wood, grease them up slick, then rotate by hand as I weld.
    No plug welds, thought about it, but I honestly don't think it will be needed.
    Last edited by Fnord5; 02-21-2016 at 11:20 AM.

  15. #65
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    This is about how it will sit.

    Name:  IMG_20160220_132304.jpg
Views: 378
Size:  76.7 KB

  16. #66
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    More progress today.
    Tacked all my arms up, didn't do full welds because things change and schite happens.
    Will only have 3-4" of up travel before the center upper link hits, so I'm going to have to build yet another replacement crossmember.
    Coilovers have gone from inboard, to outboard, and now back to inboard for clearance.
    Still need my wishbone bent and notched so I can really center the axle.
    I'm ending up at 18" of stretch, where my original plan was only 8. Lol.
    Will be a beast of a jeep though.
    Name:  IMG_20160221_150217.jpg
Views: 354
Size:  77.7 KB
    Name:  IMG_20160221_150429.jpg
Views: 367
Size:  67.4 KB
    Name:  IMG_20160221_151425.jpg
Views: 358
Size:  64.4 KB
    Name:  IMG_20160221_170227.jpg
Views: 359
Size:  67.3 KB
    Toolbox area gone. Ha!
    Name:  IMG_20160220_153030.jpg
Views: 352
Size:  75.4 KB
    Last edited by Fnord5; 02-21-2016 at 10:45 PM.

  17. #67
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Name:  IMG_20160220_154624.jpg
Views: 347
Size:  38.0 KB
    Name:  IMG_20160220_153705.jpg
Views: 356
Size:  59.4 KB

  18. #68
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Just about done. Need a new ECU, some sensor brackets and a ton of detail/cosmetic work.
    After playing with some springs, I got it to 43" up travel in the front, 42" in the rear

    Name:  IMG_20200308_121311.jpg
Views: 236
Size:  124.0 KBName:  IMG_20200308_124459.jpg
Views: 237
Size:  125.8 KBName:  IMG_20200308_144549.jpg
Views: 227
Size:  118.6 KB

  19. #69
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Stupid phone put them sideways.

  20. #70
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    A two door that's got 3.5" more wheelbase than the 4 door
    Name:  IMG_20200126_114144_01.jpg
Views: 201
Size:  134.6 KB
    Had to get creative with my trackbar in the front.
    Name:  IMG_20200125_153418_01.jpg
Views: 200
Size:  194.7 KB
    The front is a mess, but it works a treat.
    Name:  IMG_20200105_152000_01.jpg
Views: 201
Size:  201.6 KB

  21. #71
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    New (reman) ECU ordered and on the way. Hopefully that clears up my check engine light so I can get it smogged and legal.

    Corners drilled for mounting bolts, drilled and tapped for my taillights. Going to weld on some tabs to mount heavy rubber fender flares so when I rub trees they don't break Name:  IMG_20200403_162449.jpg
Views: 189
Size:  192.4 KB
    Name:  IMG_0348_01.jpg
Views: 186
Size:  199.0 KB

  22. #72
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    18" limit straps installed on the rear.
    Name:  IMG_20200412_163446.jpg
Views: 172
Size:  138.7 KB

  23. #73
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Armor mounted with success.
    Problem with custom one off parts is they don't always fit like production, off the shelf parts with tons of R&D behind them.
    No complaints though, 1/4" plate will do quite well.

    Name:  IMG_20200426_111510.jpg
Views: 124
Size:  135.2 KB
    Name:  IMG_20200426_111526.jpg
Views: 124
Size:  132.4 KB

  24. #74
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,388
    Post Thanks / Like

    Re: 09 wrangler one ton build

    Could someone rotate my pics for me?

  25. #75
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,263
    Post Thanks / Like

    Re: 09 wrangler one ton build

    You gota takes pics with your phone horizontally. That looks like a nice toy. Is it stick shift?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments