    Discharging from USN and ?'s about real world welding

    Hey all, discharging from the military, got over 3 years in, worked at norfolk naval shipyard for 2.5 years, did alot of shipfitting and sheet metal work and alot of experience in all processes, went to a 4 month high pressure pipe welding "C" school which consisted of alot of restricted socket welding and consumable rings. Just a little background there, i know i'm still a rookie but need some guidance on picking and choosing jobs as a welder. Any input will help, thanks so much
    -Caleb

  2. #2
    Join Date
    May 2013
    Location
    Virginia
    Posts
    423
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Go back to the shipyard as a civilian and do more restricted welding. Pipe welding.

    You will probably be fast tracked with military service and familiarity with the work.

  3. #3
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,075
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Try Huntington Ingalls Industries (formerly known as Northrop Grumman Shipbuilding) in Newport News. http://en.wikipedia.org/wiki/Hunting...lls_Industries
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  4. #4
    Join Date
    Oct 2013
    Location
    Sasebo, Japan
    Posts
    7
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Oldendum and akabadnews...Any other ideas aside from yard work?? In my eyes its too slow for me...no offense to anybody who does work in yards but i just want to work somewhere a lil more fast paced

  5. #5
    Join Date
    Jun 2010
    Location
    in the shadow of the sears tower
    Posts
    253
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Caleb checkout helmetstohardhats.org
    Be worth your time to see what can be offered across the U.S.

  6. #6
    Join Date
    Sep 2013
    Location
    Costa Rica
    Posts
    2,324
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Cruise Lines
    Bubble gum
    Tooth pix
    Duct tape
    Black glue
    GBMF hammer
    Screw gun --bad battery (see above)

  7. #7
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,287
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Quote Originally Posted by caleb.mcanulty View Post
    In my eyes its too slow for me...no offense to anybody who does work in yards but i just want to work somewhere a lil more fast paced
    I've worked in several Navy yards on construction projects. I always laughed, nice sun shinny day the yards would look like an ant farm, people every where. Cold rainy day, you couldn't find a soul!
    What their schedule changes with the weather?
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  8. #8
    Join Date
    May 2013
    Location
    Virginia
    Posts
    423
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    You are correct.

    I'll PM you.

  9. #9
    Join Date
    Nov 2012
    Location
    Smithville, TN
    Posts
    173
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    My take is that ideally you want to work for yourself. If done right there is money to be made (and lost if not done correctly). Also if you can locate in an area where there are multifaceted (different types) industries you will come out ahead over the years. Example: In other words, what good would it be to be the best aluminum aircraft welder in the world if the airline industry is in a slump. You need to "arm" yourself with a variety of welding skills. The more you know and are skilled at the more marketable you are. Sounds like you are a good learner and can pick up things quickly - as you already have good experience in a short period of time. For me, the money is in pipe. Stainless pipe, tig welding, x ray quality.
    P.S. be careful about throwing around phrases like, "skilled in all process". I am sure you meant to say "all processes used in a ship yard". How many welding process are there? 75, 100, 150 somewhere in there. Most of us, if we count ourselves lucky can say we are proficient in 3 or 4 and have used one or two more.
    Some kind of Big Blue constant current welding machine
    Another smaller yet, Blue machine (it's got wire in it)

  10. #10
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,075
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Quote Originally Posted by caleb.mcanulty View Post
    ...In my eyes its too slow for me...
    Well, Huntington Ingalls is not government, it is private industry. So I would expect the pace to be a bit more rapid.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  11. #11
    Join Date
    May 2013
    Location
    Virginia
    Posts
    423
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    The production is, slightly. There's a lot of down time waiting for the welds to cool, waiting for QA/QC to show up from the other side of the yard, and weather disruptions. Most departments do get rained out.

    Sounds like he would be more interested in energy/oil/gas work.

  12. #12
    Join Date
    Oct 2013
    Location
    Sasebo, Japan
    Posts
    7
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Dale, idealy that's where i'm at right now, still always willing to learn, looking for areas of the country where i can learn and work as much as i can. My knowledge lacks as to where to even start working. And yes haha you are correct about the processes aspect, looking back at what i said now i sound arrogant.
    Ironman, thank you the website has already been of great use to me.
    And CEP...them boys at the yard will go out of their way to push a job back a week haha
    Thanks all for the input it's a world of help, God knows i need it right now

  13. #13
    Join Date
    Oct 2013
    Posts
    10
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Good luck brother, just remember that the other skills you learned while you we "in" will help you once you get that civilian job

    Mike (20 year vet)

  14. #14
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,287
    Post Thanks / Like

    Re: Discharging from USN and ?'s about real world welding

    Quote Originally Posted by caleb.mcanulty View Post
    CEP...them boys at the yard will go out of their way to push a job back a week haha
    Oh I know I've seen some amazing things in those yards! I've been in Hunters Point, Mare Island, PSNS, Bangor, Key Port, and Everett.
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,665,468.38652 seconds with 13 queries