Results 1 to 6 of 6

Thread: A little rust problems

  1. #1
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,831
    Post Thanks / Like

    A little rust problems

    A customer called and told me he had a rust problem with his truck ,can I look at it Name:  9AD212A3-5F56-4214-B802-932FFB68624F.jpg
Views: 379
Size:  75.7 KBName:  E888370A-1B71-4031-8A5A-500D05F6D501.jpg
Views: 376
Size:  87.7 KBName:  22063859-F180-4879-B9E7-F38AD1AEE7AF.jpg
Views: 378
Size:  83.1 KB

  2. #2
    Join Date
    Jan 2016
    Location
    northeast USA
    Posts
    9,198
    Post Thanks / Like

    Re: A little rust problems

    looks like there was an attempt to fix and plate the chassis once before..time for a new chassis section...

  3. #3
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,831
    Post Thanks / Like

    Re: A little rust problems

    His mechanics took the brackets off . I clean them up made new uprights ,welded together ,added mounting bracket Name:  C6CA92D7-6AB1-4A64-A962-F0A722901E7F.jpg
Views: 371
Size:  125.0 KBName:  B770B3B0-057A-47BF-A81C-820AD6BBF0EF.jpg
Views: 371
Size:  111.5 KBName:  A7C76BA7-7D45-4AEB-9240-939723D4D552.jpg
Views: 369
Size:  101.2 KBName:  7409242A-DCEB-4539-ADBE-F3C0561D36B1.jpg
Views: 374
Size:  131.0 KBName:  7409242A-DCEB-4539-ADBE-F3C0561D36B1.jpg
Views: 374
Size:  131.0 KB

  4. #4
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,831
    Post Thanks / Like

    Re: A little rust problems

    They put it back together and painted itName:  DDD6C018-3A48-427B-B680-61AB2BD86877.jpg
Views: 367
Size:  94.0 KBName:  8121CF94-1F93-4E6C-9960-28C64D43275D.jpg
Views: 370
Size:  99.3 KB

  5. Likes 12V71, Mikel_24, docwelder liked this post
  6. #5
    Join Date
    Dec 2018
    Posts
    3,221
    Post Thanks / Like

    Re: A little rust problems

    The stack support on my IH is made of open sections. Won't rust, but not as strong.

    But, ya know........I don't deal with salt here. Sure, they salt the roads, but my truck never sees blacktop during the Winter.

  7. #6
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,831
    Post Thanks / Like

    Re: A little rust problems

    They go crazy with salt around here any more . You go to the food store and back (15 minutes ) you can’t tell what color your car is

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,604,000,818.46213 seconds with 15 queries