    Quote Originally Posted by kb0thn View Post
    I've certainly been with a few stuck pins. One trick that I've learned is that you can use an electric hammer drill on impact only mode to drive a stuck pin out. I have a $150 Bosch SDS+ and use a masonry point with it. It makes little tiny taps and before long it gets the pin moving. Pins that I can't hit out with a sledge hammer.
    I havent tried that before. Ill give it shot next time. Im sure it wont be long lol


    Sent from my iPhone using Tapatalk

  2. #11977
    Join Date
    Sep 2020
    Location
    South Texas
    Posts
    95
    Post Thanks / Like

    Re: Show us what you welded today

    Made this little get up today. Its a drag apparently.




    I had this 37 chunk of .71 wall 4.5 pipe

    We cut a 10 drop off and added a couple tabs for them to hook up to a chain.

    He originally wanted a railroad rail but at 32.5 lbs/ft this seemed to fit the Bill.


    Sent from my iPhone using Tapatalk

  3. Likes Bls repair, Capt B, albrightree liked this post
  4. #11978
    Join Date
    Jul 2013
    Posts
    305
    Post Thanks / Like

    Re: Show us what you welded today

    Working on a tank for buddy.
















  5. #11979
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    881
    Post Thanks / Like

    Re: Show us what you welded today

    Nice work!
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  6. #11980
    Join Date
    Sep 2020
    Location
    South Texas
    Posts
    95
    Post Thanks / Like

    Re: Show us what you welded today

    Gonna be a fine looking piece!


    Sent from my iPhone using Tapatalk

  7. #11981
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    721
    Post Thanks / Like

    Re: Show us what you welded today

    smr--really nice work.

  8. #11982
    Join Date
    Feb 2009
    Location
    Central CA
    Posts
    296
    Post Thanks / Like

    Re: Show us what you welded today

    Made some more redneck cookware. Actually, I have been watching this guy's videos on Youtube:

    https://www.townsends.us/

    He has a series on 18th century cooking, using period recipes and cookware, often over an open fire. He sells most of the implements on his web site, but since I can weld (sort of) I said to myself "Hey, I bet I could make something like that myself!" So with only a thousand dollars or so in tools and materials I saved myself a couple hundred bucks.

    Name:  IMG_0069.jpg
Views: 841
Size:  171.5 KB

    Name:  IMG_0070.jpg
Views: 840
Size:  171.0 KB

    Truth be told, I wanted an excuse to buy one of those cheepo Harbor Freight ring rollers.

    https://www.harborfreight.com/gear-d...ler-36790.html

    As has been noted here before, that tool leave knurling marks on the workpiece, so when I made the frying pan side I had to grind off the marks. Now I have grinding marks. What the hell, it's a frying pan.

    Tim

  9. Likes Joegreen02, albrightree, 12V71 liked this post
  10. #11983
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    590
    Post Thanks / Like

    Re: Show us what you welded today

    Sanitary Stainless steel fitting with .080" wall thickness welded into a 22ga polished stainless hopper for new single serve hot chocolate drink powder. Used 3/32" gold tungsten with 1/16 " 312 filler.


    Name:  009.jpg
Views: 824
Size:  102.3 KB



    With level control (tuning fork style)


    Name:  012.jpg
Views: 827
Size:  91.8 KB


    My holesaw was about .030" oversize to begin with (19mm) which made filling the gap a little bit of a challenge.


    Name:  013.jpg
Views: 827
Size:  116.8 KB
    Last edited by albrightree; 11-21-2020 at 05:31 PM.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  11. Likes ezduzit, ronsii liked this post
  12. #11984
    Join Date
    Oct 2014
    Posts
    3,035
    Post Thanks / Like

    Re: Show us what you welded today

    I don't think 312 is rated as a food grade stainless.

  13. #11985
    Join Date
    Sep 2020
    Location
    South Texas
    Posts
    95
    Post Thanks / Like

    Re: Show us what you welded today

    Little gate repair today 1x1 1/8 wall tubing

    Has the ole lady helper today. Shes a fine picture taker.


    I cut all the crooked bits out of there



    Cut some new stuff



    Clamped it in place so my picture taker could keep her hands clean.




    Spread a little peanut butter here and there.



    Then just like that she is primed and ready for paint.




    Sent from my iPhone using Tapatalk

  14. Likes N2 Welding, ronsii, Shootr, VaughnT liked this post
  15. #11986
    Join Date
    Sep 2015
    Location
    West coast of Florida
    Posts
    465
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by albrightree View Post
    Sanitary Stainless steel fitting with .080" wall thickness welded into a 22ga polished stainless hopper for new single serve hot chocolate drink powder. Used 3/32" gold tungsten with 1/16 " 312 filler.


    Name:  009.jpg
Views: 824
Size:  102.3 KB

    My holesaw was about .030" oversize to begin with (19mm) which made filling the gap a little bit of a challenge.

    Did you purge the inside?
    Richard
    West coast of Florida

  16. #11987
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    590
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by LtBadd View Post
    Did you purge the inside?
    No, I didn't , used some aluminum backers. It is a bit of a rush job, and the other argon tank was three buildings away. I should probably buy a dual output regulator/Flowmeter. Weldmonger has one that seems reasonably priced.

    Quote Originally Posted by Welder Dave View Post
    I don't think 312 is rated as a food grade stainless.
    The fitting is 304, and the hopper is unknown, but probably 304 as are most of the dry food ingredients machinery my company has purchased. E308 would have been the correct filler wire to use.
    I couldn't find any 308 in the shop where I was working other than the 5/32" stick welding rod. 312 is a High Ferrite wire, and in situations with high temp, and or corrosive liquids there is the possibility of rusting. Its been passivated, and monday will go for cleaning, and sanitizing. Its an alkali cleaner followed by an acidic sanitizer Peroxiacetic Acid (dilute). Its a mixture of Vinegar, and Hydrogen Peroxide. If we don't show rust there we'll be good to go. I have used 312 before in pinch, and usually on the cracks in the tanks that have fittings sticking out from thin wall container, and or have shakers. There are no materials that are not food grade like lead cadmium, or arsenic, in the msds. just less corrosion resistance. The main uses for 312 listed are for castings, and armor plate, where post weld cracking is a problem.

    Monday I'll order some 308 tig wire, and some argon.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  17. Likes ronsii liked this post
  18. #11988
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    721
    Post Thanks / Like

    Re: Show us what you welded today

    Made some more progress on the outboard bracket. My helper, Jesse, got a lot more of the welding completed. And we have the swim step top plates ready to install. Also got a chance to try out the new iPhone 12 Pro's camera. Seems to be quite a nice improvement over the old 5s.





  19. #11989
    Join Date
    Feb 2019
    Location
    Pittsburgh pa.
    Posts
    13
    Post Thanks / Like

    Re: Show us what you welded today

    Did this at work this summer. We had to upsize a compressor, but the bigger compressor would not fit because of the bypass loop directly behind it. I welded on extensions to the channel (6011 root and 7018 cover) and drilled new mounting holes. I am not a professional welder, I know the welds aren't perfect. Had to rework discharge and oil lines on right side. Other than sitting a few inches out than the other compressors you would never know. I had fun doing this one.

    Name:  KIMG0782.jpg
Views: 438
Size:  213.6 KB
    Name:  KIMG0784.jpg
Views: 431
Size:  225.4 KB
    Name:  KIMG0785.jpg
Views: 434
Size:  214.4 KB
    Name:  KIMG0786.jpg
Views: 415
Size:  248.3 KB

  20. Likes whtbaron, Shootr liked this post
  21. #11990
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,660
    Post Thanks / Like

    Re: Show us what you welded today

    You preheating that boat deck? Looks like some thick aluminum

  22. Likes ezduzit liked this post
  23. #11991
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    721
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by motolife313 View Post
    You preheating that boat deck? Looks like some thick aluminum
    The thickness is way overkill and probably unnecessarily heavy. No pre-heating involved. Construction is 1/4" 6061-t651. Tube is 1-1/2" od x 1/4" wall. Mounting flange is 3/8" x 2-1/2" flat bar. Aft vertical corners of tub are 5/8" rod.

  24. #11992
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,660
    Post Thanks / Like

    Re: Show us what you welded today

    Wow. I’d be using preheat. Your probably just brazing that aluminum in my opinion

  25. Likes ezduzit liked this post
  26. #11993
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    721
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by motolife313 View Post
    Wow. I’d be using preheat. Your probably just brazing that aluminum in my opinion
    Running a Miller Dynasty 200DX at wide open throttle (showing 195-amps) so I think it is slightly better than brazing. Seriously, should I be concerned? My helper is a certified welder.

  27. #11994
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,660
    Post Thanks / Like

    Re: Show us what you welded today

    Yes that job takes over 300 amps probably without preheat. 200 with out not a chance!! The guy bumped the tungsten about 12 times too. Maybe a couple but not that many meaning he’s not very good. Failed bad on the weld on the bottom pic to the right on the tube. Adding rod before the puddle was hot enough or bad rod angle. Possibly wind but that’s a rookie doing that job
    Last edited by motolife313; 11-29-2020 at 02:29 PM.

  28. Likes ronsii, ezduzit liked this post
    Dislikes Munkul disliked this post
  29. #11995
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    590
    Post Thanks / Like

    Re: Show us what you welded today

    repeat
    Last edited by albrightree; 11-29-2020 at 03:22 PM.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  30. #11996
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    590
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by ezduzit View Post
    The thickness is way overkill and probably unnecessarily heavy. No pre-heating involved. Construction is 1/4" 6061-t651. Tube is 1-1/2" od x 1/4" wall. Mounting flange is 3/8" x 2-1/2" flat bar. Aft vertical corners of tub are 5/8" rod.
    I think that weld in the back is a little more challenging than it might appear. I would have trouble getting my helmet close enough to use my cheater lens, and then you gotta get both arms in there while getting a good view of the weld. It looks to me like a very small area to weld in. Is the middle part a casting ? Castings can be difficult wetting out, and often have surprise materials that pop to the surface when welding. Definitely working that Dynasty hard. Is he using a foot pedal or a finger switch ? would like to see what the finished part comes out like, Keep us posted.

    Best of luck
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  31. Likes ezduzit liked this post
  32. #11997
    Join Date
    May 2020
    Location
    Arizona
    Posts
    423
    Post Thanks / Like

    Re: Show us what you welded today

    After my mig gun hit the floor for umpteenth time I stopped what I was doing and slapped together a holder.

    Name:  20201129_115651-01.jpg
Views: 400
Size:  202.7 KB
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  33. #11998
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    721
    Post Thanks / Like

    Re: Show us what you welded today

    Using a foot pedal.

    So you think this will fall apart?

  34. #11999
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,143
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by ezduzit View Post
    Using a foot pedal.

    So you think this will fall apart?
    It's an awful lot of metal to heat. Mine is Dynasty 280DX, I believe it's too much mass for my machine. If I tried that I'd either put a great deal of pre heat in it or add 5 CFH helium. 4943 would also help.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  35. Likes motolife313, ezduzit liked this post
  36. #12000
    Join Date
    Apr 2010
    Posts
    2,891
    Post Thanks / Like

    Re: Show us what you welded today


    sand_man_red


    Quote Originally Posted by sand_man_red View Post
    Working on a tank for buddy.
    Pics & work ^ ^ ^ - what does the tank feed . . . ?


    Opus



    .

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,611,174,067.36441 seconds with 15 queries