  1. #11501
    Join Date
    Jun 2016
    Posts
    1,002
    Post Thanks / Like

    Re: Show us what you welded today

    wow, very nice! good work.
    lincoln 125sp
    dayton 250 ac/dc
    miller 211 w/spool gun
    ahp 200 sx tig
    lotos ltp5000d
    kubota b3200 FEL BH
    of course duramax diesel

  2. Likes Munkul liked this post
  3. #11502
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Show us what you welded today

    Nice, looks good
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  4. Likes Munkul liked this post
  5. #11503
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,918
    Post Thanks / Like

    Re: Show us what you welded today

    Nice work

  6. Likes Munkul liked this post
  7. #11504
    Join Date
    Aug 2014
    Location
    BC Canada
    Posts
    14,719
    Post Thanks / Like

    Re: Show us what you welded today

    Geez. It looks too nice to use.
    :

  8. Likes ronsii, Munkul liked this post
  9. #11505
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post
    Geez. It looks too nice to use.
    LOL!, was thinking the same thing

  10. Likes Munkul liked this post
  11. #11506
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,898
    Post Thanks / Like

    Re: Show us what you welded today

    Nice box. Well done.

    Will you add a tray? Will it bow when loaded? Can you stand it?

  12. Likes Munkul liked this post
  13. #11507
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    939
    Post Thanks / Like

    Re: Show us what you welded today

    What's this alum crap? You run out of copper? Very nice work!
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  14. Likes Munkul liked this post
  15. #11508
    Join Date
    Apr 2018
    Posts
    151
    Post Thanks / Like

    Re: Show us what you welded today

    Made a quick and simple brake attachment for the harbor freight 20 ton press.

    Sent from my ONEPLUS A5010 using Tapatalk

  16. #11509
    Join Date
    Nov 2009
    Location
    Pensacola , Fla
    Posts
    1,622
    Post Thanks / Like

    Re: Show us what you welded today

    I made one like that years ago the only difference was no middle angle and there the arrow points I added shims so the inside angle was slightly over 90 to compensate for the spring back.
    Attached Images Attached Images  
    DIY CNC Plasma table USB BOB Price THC
    Hypertherm 65
    Everlast PowerTig 255 EXT
    Miler 180 Mig
    13" metal lathe
    Mill/ Drill
    ECT, ECT,

  17. Likes therider, N2 Welding liked this post
  18. #11510
    Join Date
    Apr 2018
    Posts
    151
    Post Thanks / Like

    Re: Show us what you welded today

    Very interesting. What is a spring back? I did notice that if I press too much I get less than 90 degree even though middle angle is thick.

    Sent from my ONEPLUS A5010 using Tapatalk

  19. #11511
    Join Date
    Jan 2013
    Posts
    24
    Post Thanks / Like

    Re: Show us what you welded today

    I made something just like that for a customer a few years ago.

  20. #11512
    Join Date
    Jan 2013
    Posts
    24
    Post Thanks / Like

    Re: Show us what you welded today

    Name:  IMG_20200822_181648055[5765].jpg
Views: 869
Size:  156.6 KB

  21. #11513
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: Show us what you welded today

    Depending on the thickness you are bending, you need to space the bending die (angle irons) appropriately to get a 90 deg.+ bend. Steel will spring back some so may need to experiment a little to get an accurate 90 deg. bend.

  22. #11514
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Show us what you welded today

    like it, hope you add progress posts
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  23. #11515
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    2,221
    Post Thanks / Like

    Re: Show us what you welded today

    you guys

  24. #11516
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Show us what you welded today

    Made a stand for my metal blade chop saw, using scrap 1¼ " square tube and scrap ½ " OSB.



    Small cutting "station" away from my welders and other machines

    1st on WeldingWeb to have a scrolling sig!



  25. Likes DavidR8, dmcnally, Equilibrium liked this post
  26. #11517
    Join Date
    Feb 2015
    Location
    Texas
    Posts
    353
    Post Thanks / Like

    Re: Show us what you welded today

    Not a lot of welding yet as I wanted to build a proof of concept with cheap materials before I committed to steel. A lot of people build these tables with fishing line so they appear to be floating but I was after a more substantial look and the chain would be able to hold up the table top and have a useful load. I made the top as the Gadsden flag logo out of 11 gauge and the chains are welded to all thread so they have some adjustment. Planning on making the steel one out of 2x3 tubing and the support arms will be 1/4” with lightening holes.

    Name:  C85C921D-51FA-4B4A-83DE-5A1834CBD4F5.jpeg
Views: 872
Size:  117.0 KB

    Name:  A7DA46E7-5485-4C99-A06E-00C977862E20.jpeg
Views: 823
Size:  128.7 KB

    Name:  767D1566-60F5-43DC-88F6-C5E0DA74F099.jpeg
Views: 826
Size:  111.1 KB
    Miller 350 Dynasty
    Miller Trailblazer
    Miller 625 Plasma
    Died and needs a new circuit board so its an expensive boat anchor now
    Lincoln Power MIG
    Victor oxy/acetylene
    Hyperthem 85

  27. #11518
    Join Date
    Apr 2018
    Posts
    151
    Post Thanks / Like

    Re: Show us what you welded today

    Upcycled a scrap SS pipe to a holder in the style of old forts.

    My Ellis 1800 was very helpful in cutting the slices.



    Sent from my ONEPLUS A5010 using Tapatalk

  28. #11519
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    594
    Post Thanks / Like

    Re: Show us what you welded today

    [QUOTE=BluCllrPlt;8765706]Not a lot of welding yet as I wanted to build a proof of concept with cheap materials before I committed to steel. A lot of people build these tables with fishing line so they appear to be floating but I was after a more substantial look and the chain would be able to hold up the table top and have a useful load. I made the top as the Gadsden flag logo out of 11 gauge and the chains are welded to all thread so they have some adjustment. Planning on making the steel one out of 2x3 tubing and the support arms will be 1/4” with lightening holes.

    Name:  C85C921D-51FA-4B4A-83DE-5A1834CBD4F5.jpeg
Views: 872
Size:  117.0 KB


    So the chain links are welded together and the ends welded to all thread for vertical adjustment?????
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  29. #11520
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    643
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by davec View Post
    That's some heavy welding cwby, but I gotta ask ...WHY? Someone screw up the tower design or what?
    Nah - these carriers just keep adding more loading to the existing structures & it is cheaper to upgrade the tower than replace it. Also the standards that determine the structural capacity of the towers has changed a couple of times since the original design making the old design less than required.

  30. #11521
    Join Date
    Jul 2013
    Posts
    488
    Post Thanks / Like

    Re: Show us what you welded today

    [QUOTE=geezer;8765725]
    Quote Originally Posted by BluCllrPlt View Post
    Not a lot of welding yet as I wanted to build a proof of concept with cheap materials before I committed to steel. A lot of people build these tables with fishing line so they appear to be floating but I was after a more substantial look and the chain would be able to hold up the table top and have a useful load. I made the top as the Gadsden flag logo out of 11 gauge and the chains are welded to all thread so they have some adjustment. Planning on making the steel one out of 2x3 tubing and the support arms will be 1/4” with lightening holes.

    Name:  C85C921D-51FA-4B4A-83DE-5A1834CBD4F5.jpeg
Views: 872
Size:  117.0 KB


    So the chain links are welded together and the ends welded to all thread for vertical adjustment?????
    I think it all hangs from the center chain and the four corner chains act in tension to keep the top parallel to the base. Don't think the links are welded.

  31. Likes Shootr, JimmyC liked this post
  32. #11522
    Join Date
    Feb 2015
    Location
    Texas
    Posts
    353
    Post Thanks / Like

    Re: Show us what you welded today

    The center chain is what hold the table top up. The four corner chains just keep it in place.
    Miller 350 Dynasty
    Miller Trailblazer
    Miller 625 Plasma
    Died and needs a new circuit board so its an expensive boat anchor now
    Lincoln Power MIG
    Victor oxy/acetylene
    Hyperthem 85

  33. Likes JimmyC, ronsii liked this post
  34. #11523
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Show us what you welded today

    Made a cover for the battery compartment on the big tex flatbed trailer today. hopefully this keeps the methmaggots from getting another battery from us

    I had welded in this separator to keep the chains/straps away from the battery a year or so ago but never bothered with a cover... hindsight says I should have...
    Name:  bigtex-battery-cover2.jpg
Views: 970
Size:  107.5 KB

    Had some 10 gauge pieces laying around that just needed a little cutting and fitting to throw together a slide in cover, but went to grab the milwaukee grinder I keep in the front of the truck and the switch was gone??? WTH!!! I don't even know what could have 'bumped' it but this is one more thing to add to my list of never buy milwaukee chincrap again!!!
    Name:  milwaukee-m18-grinder-broke2.JPG
Views: 839
Size:  89.7 KB

    Finally got it welded up and painted but forgot to take pics of the process... was too mad at the milwaukee crap
    Name:  bigtex-battery-cover1.jpg
Views: 777
Size:  113.3 KB
    And I also forgot to take a pic of it installed-- I'll add one later it has two bolts - one bottom front and one top back on the left side plus a padlock hole top center

  35. #11524
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Show us what you welded today

    Was also supposed to mount this box under the trailer but had too many other things going on to get to it...

    Any suggestions on how to mount it??? can't go directly to the crossmembers as they are too high so I'll need to drop about 2 inches to clear the side rails and didn't want it flush with the side rails... the box is 18x18x36inches the front door sticks out and inch so 19" deep. Was thinking run a piece of 2.5 angle across the crossmembers in the front... and either drop flat bar down the back to bolt in the lower back of the box like I've seen done before for flatbed truck installs... makes it easy to get to the bolts in the back unless someone has a better... simpler method I'm all ears

    Name:  bigtex-boxnoumt1.jpg
Views: 1018
Size:  57.8 KB

    Name:  bigtex-boxnoumt2.jpg
Views: 1042
Size:  143.3 KB
    Last edited by ronsii; 08-31-2020 at 11:52 PM.

  36. #11525
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    2,221
    Post Thanks / Like

    Re: Show us what you welded today

    I don't think there's a right or wrong answer to that, Ronsii. I'd be making two angle hanging brackets from the crossbars I think.

  37. Likes ronsii liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,298,593.08475 seconds with 21 queries