1.6L Miata EFR Manifold by HellaFab, on Flickr
Welding away in my little shop.
Lincoln Precision Tig 185
Lincoln Power Mig 256
Hypertherm PM 45
Everlast 140ST
Smith O/A
12v battery, jumper cables, and a 6013.
I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829
Last edited by teachagmech; 10-24-2014 at 03:54 PM.
Teach Ag Mech - Mike
At Home:
Lincoln Electric AC225
Miller Challenger 172
Gas Axe
Work:
eclectic bunch of 90's vintage blue boxes
First hour of having a go at aluminium tig, got a new Unimig ac/dc 200 with foot pedal.
1/8 ali, er5356 2.4mm
It's different to mild thats for sure
Teach Ag Mech - Mike
At Home:
Lincoln Electric AC225
Miller Challenger 172
Gas Axe
Work:
eclectic bunch of 90's vintage blue boxes
2.4mm tungsten, no7 cup, had it on 200a but feathering a bit,first ime using a foot pedal too.
It's been a while since I've run on .100 material, but I think 200A might be a little high. Can you post pics of the back side?
Teach Ag Mech - Mike
At Home:
Lincoln Electric AC225
Miller Challenger 172
Gas Axe
Work:
eclectic bunch of 90's vintage blue boxes
Thats the back side, I did another run there too, you can see on the right where I had a slight blow out at the end.
I wasn't at 200 for much if any of the time, just using the pedal
Try to set max amperage where you are running around 2/3 pedal or more at least for the majority of the weld.
Looks like you need more filler. It'll cool the puddle better and add more reinforcement.
Keep up the good work
Teach Ag Mech - Mike
At Home:
Lincoln Electric AC225
Miller Challenger 172
Gas Axe
Work:
eclectic bunch of 90's vintage blue boxes
Nothing new to post up so I'll post some more pics that I've been meaning to from that twin turbo corvette build I was doing the welding on (back from page 12)...
chopped the back off for cowl clearancing
re-powdercoated
Bigger intercooler outlet was needed and at a specific angle to match the next pipe
some bungz too
![]()
Last edited by MikeGyver; 10-25-2014 at 06:59 AM.
Welding/Fab Pics: www.UtahWeld.com
Continued...
shortened the ends of the headers and welded on V-band clamps
had to slightly re-route a header primaty tube for brake booster clearance
![]()
Welding/Fab Pics: www.UtahWeld.com
That is art work Mikegyver!!
Brian
Miller Thunderbolt 225 AC/DC
Everlast 255 EXT with water cooler
H.F. 170 Mig/Flux welder
Kent 3h.p. 9x42 milling machine
Home Built 2"x72" variable speed 2 h.p. belt grinder
Home built 9" variable speed 2 h.p. disc grinder
Very very nice Mike!
12v battery, jumper cables, and a 6013.
I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829
That ride may have some problems but air flow ain't gonna be one of them!
Can I drive?
Lincoln Electric:
Ranger GXT 250
SA-200
LN-25
Pro MiG 256
Pro Mig 180
Esab CV 251
Invertec 160
Victor Torches”
and purged..very nice..i do some of that for the diesel crowd
Wow ****ing nice work mike!
Sent from my iPhone using Tapatalk
Man that's a lot of stuff under the hood of the vette, very cool build. Nice work, really nice.
Quality work is never Cheap, and Cheap work is never Quality!!
If it's broke, and you're not, we can fix it!!
Lincoln Idealarc sp200
Century 230amp ac/dc
Smith O/A Torches
Huth Hyd. Pipe Bender
other misc "cool" tools
these are clipper racks for the barber shop. made from stainless flats drilled and countersunk for plug welding from the reverse side. hooks are scrap bolts with the thread removed and bent in a press.
i.u.o.e. # 15
queens, ny and sunny fla
Helped do this a couple of months ago with a friend.