    Re: Trailer fail pics

    That single low grade bolt is also a HINGE POINT...sideways in this case. When he hits the brakes or goes around a corner...that assembly is going to swing to one side or the other...

    Idiot

  2. Likes jfh liked this post
  3. #3252
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by rugrat View Post
    I think it will eventually wreck many trailers as well due to its weak link.
    He's good!!!!! don't worry-- it's double nutted those nuts ain't comin' off

  4. #3253
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    1,534
    Post Thanks / Like

    Re: Trailer fail pics

    Same idiots, same place, same trailer (two different trucks over time)...they pull it there every day. I don't know how they can drive there every day and never get pulled over for being so grossly overloaded but it's there day after day for months now. It seems like half the time I see someone pulling a trailer something is wrong....and nobody cares that they put everyone else on the road at risk.

    Name:  IMG_9934.jpg
Views: 2337
Size:  122.2 KB
    Last edited by G-ManBart; 09-15-2020 at 08:54 PM.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  5. #3254
    Join Date
    Jan 2015
    Posts
    84
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by ronsii View Post
    He's good!!!!! don't worry-- it's double nutted those nuts ain't comin' off
    Plus the wiring will act like a safety chain if it does break so I see no problems


    Sent from my iPhone using Tapatalk

  6. Likes ronsii liked this post
  7. #3255
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Tmtbob View Post
    Plus the wiring will act like a safety chain if it does break so I see no problems


    Sent from my iPhone using Tapatalk
    Exactly!!!!!

  8. #3256
    Join Date
    Jan 2004
    Location
    South Central Kansas
    Posts
    462
    Post Thanks / Like

    Re: Trailer fail pics

    Saw a good one earlier tonight but didn't think to get pictures. Wife and I was driving down a street in town and there was a pickup pulling a goose neck trailer loaded with the large round hay bales in front of us. We kept our distance as we followed it about a half mile as the bales were not secured and the bales on the top were rocking back and forth badly, but then we turned at an intersection to drive to our destination. We were only at our destination a few minutes and we decided to drive back to the route the truck was taking when we last saw it. We thought if it made it to the highway which was only about 3/4 mile up the road, if it hadn't lost any bales by that time, it surely would after it got on the highway. We made it to the highway intersection and hadn't seen it yet, but within less than a mile up the highway there the truck and trailer set just off the road and one of the bales had rolled off and was several feet away from the trailer. Sure glad it hadn't struck any vehicles when it rolled off the trailer.

  9. Likes ronsii liked this post
  10. #3257
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by bfjou812 View Post
    Saw this little gem.........................At least he has the ball locked...............


    Attachment 1716169
    3 balls are better than 2.

  11. Likes ronsii, mcspeed liked this post
  12. #3258
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Welder Dave View Post
    3 balls are better than 2.
    LOL!!! that's just wrong


  13. #3259
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    1,534
    Post Thanks / Like

    Re: Trailer fail pics

    Another gem I saw not long ago...

    Name:  IMG_0009.jpg
Views: 2255
Size:  109.3 KB
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  14. #3260
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    642
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Tarmstrong View Post
    That single low grade bolt is also a HINGE POINT...sideways in this case. When he hits the brakes or goes around a corner...that assembly is going to swing to one side or the other...

    Idiot
    Swinging tow bar. Use 'em on the tractor all the time!

  15. Likes ronsii liked this post
  16. #3261
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    1,414
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by rugrat View Post
    I think it will eventually wreck many trailers as well due to its weak link.

    The things that make me wonder ?

    1) It looks like he's using the 1-7/8" ball, and most of the paint is still there. Probably a small trailer, of log splitter ?
    2) Possibly a 3/4" x 6" bolt, has some marking on top, probably Grade 5. Looks larger than the 5/8"pin in the hitch. ?
    3) He has a pin lock for the ball hitch ?
    4) how long did it take him to find all the parts at Tractor supply and to figure out that the 2" ball adapter would fit inside the 2-1/2" ball adapter?

    I don't think he'll ruin more than one trailer, it might stay in place for a while. Once the bolt gets loose, and the and the trailer begins to swing, they'll more than likely hit the brakes. When they hit the brakes, the hitch will swivel hard into the plastic license plate light, and the chrome sheet metal of the bumper. I think the damage would get his attention, but you never know. The fact that its black, and protrudes 24" out from the tailgate, and about 16" off the ground make it knee cap ready. I have a 3/4 ton dodge, and when I forget to take my hitch out, I still catch it every now and then. Mine is still the factory receiver. Not a good idea, even if its just to use moving a small trailer in the back yard. It migh work a little bit, then they'll get brave and moving something big on the Highway.Might be smart enough to be dangerous, too dumb to care.

    Well just hope no one runs into him https://www.weldingweb.com/images/smilies/laughing.gif
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  17. #3262
    Join Date
    Mar 2009
    Posts
    3,560
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Timothy Swain View Post
    Had to grab a picture of this yesterday. Very happy it didn't go into the other lane. No idea the story but you can figure it out.
    My cousin's boy (17y.o.) guided his dad back to the trailer and proceded to hook it up. Lights, chains, jack, latch pintle (uh oh). I rode shotgun to pick up a tractor. Over 70 miles to get tractor. Dropped the ramps and I made it up to top of ramps with front wheels and pop goes the weasel. Trailer came off the pintle hook and rolled up under the truck. This was about 3 months ago. It was awesome.
    "You can't out puke a buzzard"

  18. Likes ronsii liked this post
  19. #3263
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,585
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Pipeliner View Post
    My cousin's boy (17y.o.) guided his dad back to the trailer and proceded to hook it up. Lights, chains, jack, latch pintle (uh oh). I rode shotgun to pick up a tractor. Over 70 miles to get tractor. Dropped the ramps and I made it up to top of ramps with front wheels and pop goes the weasel. Trailer came off the pintle hook and rolled up under the truck. This was about 3 months ago. It was awesome.
    Twenty some years ago my uncle had a boat he kept in the water. In winter It lived on dry land, near where it was docked. Nearest boat ramp was 6 miles away. Spring & fall it had to be transported by trailer. Three of us were involved. I had the truck, but these were experienced men you could count on to do it right. One trip they failed to latch the trailer winch. I lost the boat part way to the ramp. Still hitched to the strap, I believe I dragged it a few feet before getting stopped. Damage was light scratching of the underwater part of the hull.

    A few years later, time had passed. Thousands of uneventful tows without problems, I wasn't on my toes. I towed an empty trailer to the boat ramp. As the boat came up the trailer, the coupler popped off the ball. A new van got its first ding.

    Now one person, the driver is responsible for checking all aspects of the hitch.
    Last edited by Willie B; 09-17-2020 at 04:06 PM.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  20. Likes ronsii, Pipeliner liked this post
  21. #3264
    Join Date
    Oct 2009
    Location
    Foley, Al
    Posts
    464
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Pipeliner View Post
    My cousin's boy (17y.o.) guided his dad back to the trailer and proceded to hook it up. Lights, chains, jack, latch pintle (uh oh). I rode shotgun to pick up a tractor. Over 70 miles to get tractor. Dropped the ramps and I made it up to top of ramps with front wheels and pop goes the weasel. Trailer came off the pintle hook and rolled up under the truck. This was about 3 months ago. It was awesome.
    I had a customer show up to drop a boat off with a similar situation. Somehow he managed to close the coupler latch on top of the ball, instead of around the ball, and tows it 50 miles to my shop. Made it just fine, and he had no clue until I went to unhitch it for him.
    Who is John Galt?

  22. #3265
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,717
    Post Thanks / Like

    Re: Trailer fail pics

    Farmers. LOL
    Name:  egxnj44bvzn51.jpg
Views: 1970
Size:  72.7 KB

  23. Likes ronsii liked this post
  24. #3266
    Join Date
    Jan 2009
    Location
    Sonoma County, Northern California
    Posts
    1,140
    Post Thanks / Like

    Re: Trailer fail pics

    That one is more a case of 'ya do what ya gotta do' when he lost the pin. With no chains or wiring there's no evidence that this will go on the highway where its a hazard to to others. He's just pulling some implement around the farm. But it looks like he could have made more welds between that tab and the trailer structure.

    Shame to botch up a good wrench.
    * Amico MIG-130A Flux, Dual Voltage. Truly portable!
    * HF MIG-180 with all the mods. Heavy.
    * Grizzly H8153 Stick/Tig 130/160.
    * Wards PowrKraft AC-230. Stick & carbon arc.

  25. Likes hddnis liked this post
  26. #3267
    Join Date
    Jul 2013
    Posts
    488
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by California View Post
    That one is more a case of 'ya do what ya gotta do' when he lost the pin. With no chains or wiring there's no evidence that this will go on the highway where its a hazard to to others. He's just pulling some implement around the farm. But it looks like he could have made more welds between that tab and the trailer structure.

    Shame to botch up a good wrench.

    Is it a good wrench or a piece of chicom that has been frustrating him ever since he bought it and now he really hopes it breaks being used as a hitch pin?

  27. Likes California liked this post
  28. #3268
    Join Date
    Jan 2016
    Location
    northeast USA
    Posts
    11,394
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Fnord5 View Post
    Farmers. LOL
    Name:  egxnj44bvzn51.jpg
Views: 1970
Size:  72.7 KB
    lol..I had a farmer that hayed one of my fields on a steep grade and whatever he used for a pin in a chopper wagon let loose..that wagon went down the hill, crashed through about 50 feet of trees and stopped in the middle of the road in a pile of scrap metal, luckily no car was coming..the town had to come with a pay loader to push it to the side till he could flat bed it home..total lose on the wagon it went end over end as it went down hill..

  29. Likes ronsii, California liked this post
  30. #3269
    Join Date
    Aug 2018
    Posts
    223
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by bfjou812 View Post
    Saw this little gem.........................At least he has the ball locked...............


    Attachment 1716169
    AZ...Obviously tweakers....
    Welds last longer than Love...

  31. Likes ronsii liked this post
  32. #3270
    Join Date
    Jun 2014
    Location
    Winter Haven ,Fl.
    Posts
    136
    Post Thanks / Like

    Re: Trailer fail pics

    At leas tthey used what appears to be a 2x6 to mount the ball on...................



    Name:  119917565_10221915872318794_3812253474793012708_n.jpg
Views: 1606
Size:  80.2 KB

  33. Likes ronsii liked this post
  34. #3271
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,549
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by bfjou812 View Post
    At leas tthey used what appears to be a 2x6 to mount the ball on...................



    Name:  119917565_10221915872318794_3812253474793012708_n.jpg
Views: 1606
Size:  80.2 KB
    And.... it's got a safety chain holder!!! that makes it safe


    Plus mounting the ball behind the grain lines where the carriage bolts go through will prevent the trailer from breaking the board and ramming into the car!!! a lot of thought went into this project
    Last edited by ronsii; 10-02-2020 at 10:35 PM.

  35. #3272
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,894
    Post Thanks / Like

    Re: Trailer fail pics

    First stop and the wrench run away.

    Dave

    Quote Originally Posted by Fnord5 View Post
    Farmers. LOL
    Name:  egxnj44bvzn51.jpg
Views: 1970
Size:  72.7 KB
    HF 170 welder
    HF 4x6 band saw
    South Bend 9N
    Mill
    B&D mag drill
    Victor torch

  36. #3273
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,894
    Post Thanks / Like

    Re: Trailer fail pics

    But no welding
    Taking away our jobs or maybe want something made in the USA

    Dave

    Quote Originally Posted by ronsii View Post
    And.... it's got a safety chain holder!!! that makes it safe


    Plus mounting the ball behind the grain lines where the carriage bolts go through will prevent the trailer from breaking the board and ramming into the car!!! a lot of thought went into this project
    HF 170 welder
    HF 4x6 band saw
    South Bend 9N
    Mill
    B&D mag drill
    Victor torch

  37. #3274
    Join Date
    Sep 2012
    Location
    Utopia,TX / Pasadena, TX
    Posts
    448
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by ronsii View Post
    And.... it's got a safety chain holder!!! that makes it safe


    Plus mounting the ball behind the grain lines where the carriage bolts go through will prevent the trailer from breaking the board and ramming into the car!!! a lot of thought went into this project
    The bumper sticker says it all.

  38. Likes ronsii, Gump, timrb, LtBadd, mcspeed liked this post
  39. #3275
    Join Date
    Jun 2018
    Location
    NC
    Posts
    1,561
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by bfjou812 View Post
    At leas tthey used what appears to be a 2x6 to mount the ball on...................



    Name:  119917565_10221915872318794_3812253474793012708_n.jpg
Views: 1606
Size:  80.2 KB




    I hope that's not Home Depot lumber
    ***********************

    CR

  40. Likes ronsii liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,256,770.34745 seconds with 21 queries