    Quote Originally Posted by bfjou812 View Post
    At leas tthey used what appears to be a 2x6 to mount the ball on...................



    Attachment 1717201




    I hope that's not Home Depot lumber
    ***********************

    CR

  2. Likes ronsii liked this post
  3. #3277
    Join Date
    Apr 2017
    Location
    Long Island, NY
    Posts
    345
    Post Thanks / Like

    Re: Trailer fail pics

    I don't understand why this hitch is a fail. It's solidly attached to the vehicle, it's got a nice new ball on it and the builder was even smart enough to add those nice eye bolts for securing the trailer with I'm guessing brand new HF bungee cords.

    It's a heck of a lot better than some of those rusted factory hitches I see being used with the wrong sized ball, no safety chains and no lights or brakes.

    Ok, seriously, I hope that a LEO pulls that idiot over and impounds both his vehicle and trailer.
    Lincoln Invertec V205-T Tig/stick
    Miller Coolmate 1.3 Coolant System
    Millermatic 211 Mig Welder
    Speedglas Adflo PAPR 9100 FX-Air
    CertiFlat FB2430 fabBlock U-Weld Kit Welding Table
    FW3012 CertiFlat fabWing 30" X 12" Extension Table

  4. Likes ronsii liked this post
  5. #3278
    Join Date
    Apr 2016
    Posts
    333
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by ronsii View Post
    And.... it's got a safety chain holder!!! that makes it safe


    Plus mounting the ball behind the grain lines where the carriage bolts go through will prevent the trailer from breaking the board and ramming into the car!!! a lot of thought went into this project
    Sorry to disappoint everyone, but they got the crown on the 2x6 facing the wrong way. If you're going to use interior lumber, at least put it on right side up.

  6. Likes ronsii liked this post
  7. #3279
    Join Date
    Dec 2014
    Location
    Northern California
    Posts
    227
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Weldalittle View Post
    Sorry to disappoint everyone, but they got the crown on the 2x6 facing the wrong way. If you're going to use interior lumber, at least put it on right side up.
    You idiot...that should be Pressure treated lumber

  8. #3280
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,005
    Post Thanks / Like

    Re: Trailer fail pics

    It is PT. Yellow Pine to be exact. It'll cause corrosion.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  9. #3281
    Join Date
    Apr 2012
    Location
    Montreal area Canada
    Posts
    1,082
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Willie B View Post
    It is PT. Yellow Pine to be exact. It'll cause corrosion.
    Quote Originally Posted by Weldalittle View Post
    Sorry to disappoint everyone, but they got the crown on the 2x6 facing the wrong way. If you're going to use interior lumber, at least put it on right side up.

    that welding forum is extremely educative about ...lumber thank-you

  10. #3282
    Join Date
    Oct 2014
    Posts
    2,761
    Post Thanks / Like

    Re: Trailer fail pics

    Wonder what the trailer looks like???

  11. Likes Weldalittle liked this post
  12. #3283
    Join Date
    Aug 2015
    Location
    West Michigan
    Posts
    82
    Post Thanks / Like

    Re: Trailer fail pics

    Here's a beauty I saw at dairy queen yesterday. No fail yet, but the pallet rack frame is certainly interesting

    Sent from my SM-G930P using Tapatalk

  13. Likes 12V71 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,607,060,394.20011 seconds with 14 queries