    Re: Trailer fail pics

    I don't understand why this hitch is a fail. It's solidly attached to the vehicle, it's got a nice new ball on it and the builder was even smart enough to add those nice eye bolts for securing the trailer with I'm guessing brand new HF bungee cords.

    It's a heck of a lot better than some of those rusted factory hitches I see being used with the wrong sized ball, no safety chains and no lights or brakes.

    Ok, seriously, I hope that a LEO pulls that idiot over and impounds both his vehicle and trailer.
    Lincoln Invertec V205-T Tig/stick
    Miller Coolmate 1.3 Coolant System
    Millermatic 211 Mig Welder
    Speedglas Adflo PAPR 9100 FX-Air
    CertiFlat FB2430 fabBlock U-Weld Kit Welding Table
    FW3012 CertiFlat fabWing 30" X 12" Extension Table

  2. Likes ronsii liked this post
  3. #3277
    Join Date
    Apr 2016
    Posts
    342
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by ronsii View Post
    And.... it's got a safety chain holder!!! that makes it safe


    Plus mounting the ball behind the grain lines where the carriage bolts go through will prevent the trailer from breaking the board and ramming into the car!!! a lot of thought went into this project
    Sorry to disappoint everyone, but they got the crown on the 2x6 facing the wrong way. If you're going to use interior lumber, at least put it on right side up.

  4. Likes ronsii liked this post
  5. #3278
    Join Date
    Dec 2014
    Location
    Northern California
    Posts
    247
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Weldalittle View Post
    Sorry to disappoint everyone, but they got the crown on the 2x6 facing the wrong way. If you're going to use interior lumber, at least put it on right side up.
    You idiot...that should be Pressure treated lumber

  6. #3279
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,146
    Post Thanks / Like

    Re: Trailer fail pics

    It is PT. Yellow Pine to be exact. It'll cause corrosion.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  7. #3280
    Join Date
    Apr 2012
    Location
    Montreal area Canada
    Posts
    1,085
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Willie B View Post
    It is PT. Yellow Pine to be exact. It'll cause corrosion.
    Quote Originally Posted by Weldalittle View Post
    Sorry to disappoint everyone, but they got the crown on the 2x6 facing the wrong way. If you're going to use interior lumber, at least put it on right side up.

    that welding forum is extremely educative about ...lumber thank-you

  8. #3281
    Join Date
    Oct 2014
    Posts
    3,042
    Post Thanks / Like

    Re: Trailer fail pics

    Wonder what the trailer looks like???

  9. Likes Weldalittle liked this post
  10. #3282
    Join Date
    Aug 2015
    Location
    West Michigan
    Posts
    84
    Post Thanks / Like

    Re: Trailer fail pics

    Here's a beauty I saw at dairy queen yesterday. No fail yet, but the pallet rack frame is certainly interesting

    Sent from my SM-G930P using Tapatalk

  11. Likes 12V71 liked this post
  12. #3283
    Join Date
    Jun 2016
    Location
    Texas Hill Country
    Posts
    185
    Post Thanks / Like

    Re: Trailer fail pics

    Name:  20201115_212755.jpg
Views: 1605
Size:  80.4 KB

    Not a trailer but... Anyone here want to own this one?

  13. Likes ronsii liked this post
  14. #3284
    Join Date
    Feb 2010
    Location
    TX / MN
    Posts
    592
    Post Thanks / Like

    Re: Trailer fail pics

    I'll have to keep an eye out for that one when I'm in town.

  15. #3285
    Join Date
    Feb 2016
    Location
    W. Texas
    Posts
    191
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by mbarasing View Post
    Name:  20201115_212755.jpg
Views: 1605
Size:  80.4 KB

    Not a trailer but... Anyone here want to own this one?
    Looks like the original bolt on hitch didn't work.

    Zach

  16. Likes ronsii liked this post
  17. #3286
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,051
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by bfjou812 View Post
    At leas tthey used what appears to be a 2x6 to mount the ball on...................



    Attachment 1717201

    Had they simply used the copper treated (green) PT boards the copper would work harden and the hitch would get stronger the more it was used.

  18. #3287
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,660
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by WTXBTUMOVER View Post
    Looks like the original bolt on hitch didn't work.

    Zach
    Had a guy pull out a pear stump after I cut the tree down. Back tires about came off the ground

  19. #3288
    Join Date
    Dec 2014
    Location
    Northern California
    Posts
    247
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by WTXBTUMOVER View Post
    Looks like the original bolt on hitch didn't work.

    Zach
    Yeah it did...it was that damn plastic bumper that the bolts pulled out of that was the problem.

  20. Likes mbarasing, whtbaron liked this post
  21. #3289
    Join Date
    Jun 2014
    Posts
    103
    Post Thanks / Like

    Re: Trailer fail pics

    Here is an interesting one. At least they are using chains......................
    https://www.facebook.com/sketchcityg...3623457006818/

  22. Likes Bruce liked this post
  23. #3290
    Join Date
    Dec 2016
    Posts
    273
    Post Thanks / Like

    Re: Trailer fail pics

    at least it's not chinese wood......

  24. Likes Bruce liked this post
  25. #3291
    Join Date
    Sep 2014
    Posts
    80
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by bfjou812 View Post
    Here is an interesting one. At least they are using chains......................
    https://www.facebook.com/sketchcityg...3623457006818/
    Texas plates, that’s probably part of a Mexican Caravan, see it all the time. The Mexican car dealers come up in a minivan pulling a few car dollies, then buy a couple of cars at auction and daisy chain them to the minivan and pull them back to Mexico. They get by with it somehow, DPS would jail a Texas resident lol.

    I’ve even seen them with a minivan full of these types of “dollies” and helpers at the auctions. They buy a bunch of cars, with one Run-and-Drive to every two immobile vehicles, then pull the two non drivers with the one run-and-drive. They end up with a 9 or so cars in total, all riding together in the slow lane doing 55, hence the name.
    Last edited by Mike_L; 2 Weeks Ago at 05:47 PM.

  26. Likes ronsii liked this post
  27. #3292
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,887
    Post Thanks / Like

    Re: Trailer fail pics

    Not sure if this is a 'trailer fail' or tractor... either way the trailer is failed now Saw this morning while headed north.

    Looks like this guy missed the off ramp a half mile back and decided to try to go up the bank
    Name:  semiroll512-canyon1-6jan2021.jpg
Views: 793
Size:  58.5 KB

    Name:  semiroll512-canyon2-6jan2021.jpg
Views: 797
Size:  75.3 KB

    Tractor was gone when I came back through a bit later.
    Name:  semiroll512-canyon3-6jan2021.jpg
Views: 795
Size:  67.8 KB

    Name:  semiroll512-canyon4-6jan2021.jpg
Views: 795
Size:  66.7 KB

    Name:  semiroll512-canyon5-6jan2021.jpg
Views: 797
Size:  67.9 KB

  28. Likes California liked this post
  29. #3293
    Join Date
    Jan 2009
    Location
    Sonoma County
    Posts
    874
    Post Thanks / Like

    Re: Trailer fail pics

    Oops!

    HF MIG-180 with all the mods.
    Grizzly H8153 Stick/Tig Pulse 130/160.
    Wards PowrKraft AC-230. Stick & carbon arc.

  30. Likes Bruce liked this post
  31. #3294
    Join Date
    Nov 2009
    Location
    Seward, Ak
    Posts
    353
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by ronsii View Post
    And.... it's got a safety chain holder!!! that makes it safe


    Plus mounting the ball behind the grain lines where the carriage bolts go through will prevent the trailer from breaking the board and ramming into the car!!! a lot of thought went into this project
    Well Mass is a community that is run by rules and regulations..

  32. Likes ronsii liked this post
  33. #3295
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,887
    Post Thanks / Like

    Re: Trailer fail pics

    Some more 'mass' issues with this trailer today from the tractor pulling it

    He definitely should have sprung for the extra high flotation tires on this rig
    Name:  semi-float0-12jan2021.jpg
Views: 360
Size:  67.6 KB

    Name:  semi-float1-12jan2021.jpg
Views: 361
Size:  52.2 KB

    The little wrecker showed up first and I thought to myself... Hmmmm, you might want to get a bigger tow truck!!! then about 10 minutes later his big brother rolled in
    Name:  semi-float2-12jan2021.jpg
Views: 361
Size:  62.6 KB

    Name:  semi-float3-12jan2021.jpg
Views: 363
Size:  64.5 KB

  34. Likes 12V71, Bruce liked this post
  35. #3296
    Join Date
    Jan 2015
    Posts
    79
    Post Thanks / Like

    Re: Trailer fail pics

    Wow. Iím guessing that was a dug out loading dock filled with water


    Sent from my iPhone using Tapatalk

  36. #3297
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,887
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Tmtbob View Post
    Wow. I’m guessing that was a dug out loading dock filled with water


    Sent from my iPhone using Tapatalk
    No, just a soft shoulder and crappy soil down here in the valley it floods a lot this time of year... I didn't see him put it in there but only happened about 15 minutes before I got on site... probably came out of the industrial park and went wide!!! but with all the water couldn't see the 3-4 foot deep culverts

  37. Likes Bruce, Tmtbob liked this post
  38. #3298
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,530
    Post Thanks / Like

    Re: Trailer fail pics

    I was with a buddy of mine when he got called out with a 1 ton tow truck. We get to the site and a semi is stuck. He had the front tires 3 ft off the ground but he got it out. Yes, we were 19.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  39. Likes ronsii, Bruce, 12V71 liked this post
  40. #3299
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    9,887
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Tmtbob View Post
    Wow. I’m guessing that was a dug out loading dock filled with water


    Sent from my iPhone using Tapatalk
    Here's a pic from the next day: water receded and the fence is barely leaning

    Name:  semi-ditch-flood1.jpg
Views: 173
Size:  55.8 KB

  41. Likes 12V71, Bruce, California liked this post
  42. #3300
    Join Date
    Jan 2015
    Posts
    79
    Post Thanks / Like

    Re: Trailer fail pics

    First pics full of water look like a parking lot. I had to go back and see them for it to make sense. Looked like he was gonna get towed to the shop for repairs but now doesnít look as bad as I originally thought


    Sent from my iPhone using Tapatalk

  43. Likes ronsii liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,611,242,501.76668 seconds with 13 queries