    In the spirit of buiding everything cheesy and cheap, how difficult is it to machine my own bender die for 1 1/2 inch Alum tubes ,

    I have a 9 inch south bend lathe and I'm going to need 4x 90 deg bends for a boat frame, I'd like to do it with minimum sweep of the curve.
    Its for a one off project that will only see one use then be junked.

    I was thinking of trying the 12 ton HF bender but hear they ought to be called Tube kinkers. Can I get 90 degs from the HF unit?
    Is it possible to buy 90 deg pre-bent tube ?
    If so, that would probably solve it for me, the other bends I need are very gentle and I can cobble something up for that.
    Last edited by jonesg; 01-31-2010 at 02:51 PM.

  2. #2
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,886
    Post Thanks / Like

    Re: homemade bender dies

    For a bending die your lathe is probably too small. I made some steel pnes for my ring roller wihich are smaller those on my bending dies. The die will be larger than the radius/diameter desired since it is usually center line.

    You need a radius tool. Not too difficult to make the tool or die.

  3. #3
    Join Date
    Nov 2009
    Location
    Pensacola , Fla
    Posts
    1,115
    Post Thanks / Like

    Re: homemade bender dies

    Hi
    Not sure what size of arc you waht but with a ring roller you are able to make about any size. You can make your own dies for rolling with the lathe you have but you will need aradius cutter to make them. and they are easy to make also.
    have fun
    Tom
    Attached Images Attached Images   

  4. #4
    Join Date
    Sep 2007
    Location
    Yorkshire
    Posts
    339
    Post Thanks / Like

    Re: homemade bender dies

    I like that Tom, Question is which came first the Hand wheel or the ring roller

  5. #5
    Join Date
    Dec 2008
    Posts
    235
    Post Thanks / Like

    Re: homemade bender dies

    I have no clue what the proper terminology is in machining things because I have never done any machining, but somewhere on this forum or on "hotrodders" there's a guy who made his own dies on a lathe, I do believe it was for a roller but you could do the same for a tube bending die if your lathe was big enough... he had kinda what looked like a boring bar on his tool post with the cutter in the bar. the cutter extends out of the bar the radius of the die he was making, the bar would rotate the cutter to make a perfect radius on his work piece. I know I'm fu@#ing up explaining this so maybe someone smarter than myself can explain it if you don't understand me.
    "Obstacles are those frightful things you see when you take your eyes off your goal" -Henry Ford

  6. #6
    Join Date
    Jan 2010
    Posts
    16
    Post Thanks / Like

    Re: homemade bender dies

    theres videos on youtube that shows one person maken a jig to turn out dies just search for homemade tube dies

  7. #7
    Join Date
    Feb 2009
    Location
    Melbourne, Australia
    Posts
    1,495
    Post Thanks / Like

    Re: homemade bender dies

    Quote Originally Posted by eyeball engineer View Post
    I have no clue what the proper terminology is in machining things because I have never done any machining, but somewhere on this forum or on "hotrodders" there's a guy who made his own dies on a lathe, I do believe it was for a roller but you could do the same for a tube bending die if your lathe was big enough... he had kinda what looked like a boring bar on his tool post with the cutter in the bar. the cutter extends out of the bar the radius of the die he was making, the bar would rotate the cutter to make a perfect radius on his work piece. I know I'm fu@#ing up explaining this so maybe someone smarter than myself can explain it if you don't understand me.
    I think it was Jackalop? ( can not quite remember his name. sorry no offence )that posted pics of turning his own dies on a lathe.

    Your explanation was not bad. It was very much like you described from what i can remember.

  8. #8
    Join Date
    Apr 2005
    Location
    Granite Falls, NC
    Posts
    242
    Post Thanks / Like

    Re: homemade bender dies

    For one time 4 bends a muffler shop may be the cheapest.
    Lincoln SA200, HH135, Lencospot, HF80 Inverter, Rockwell 11x35 lathe, HF drill mill, Kama 554 tractor w/ FEL & BH, Belarus 250AS, lot's of Chinese tools

  9. #9
    Join Date
    Nov 2009
    Location
    Boston
    Posts
    92
    Post Thanks / Like

    Re: homemade bender dies

    I saw that ring bender at HF, it might be better suited for making a car port frame.

  10. #10
    Join Date
    Dec 2005
    Location
    Charlotte, NC
    Posts
    1,644
    Post Thanks / Like

    Re: homemade bender dies

    Try any of the racing fab shops in your area. A JD2 bender or similar should be able to make those bends, and it will probably cost you less than the materials to make a die will.

  11. #11
    Join Date
    Jan 2004
    Location
    St. Peters, MO
    Posts
    366
    Post Thanks / Like

    Re: homemade bender dies

    Last edited by jackalope; 02-04-2010 at 04:48 PM.
    http://jackalopefab.com/
    MM210
    Synchrowave 200DX
    Miller XMT350 w/60series feeder
    Miller Bobcat 250 with SGA 100 and spoolgun
    HTP Plasma
    Full Machine shop with everything

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,495,071.81040 seconds with 14 queries