    DC stick = easiest aluminum casting ever

    This is so simple it may blow your mind. I'm using a DC arc welder, a graphite crucible and kinetic sand (it's a kids toy) to cast aluminum parts.


  2. #2
    Join Date
    Aug 2014
    Location
    Temecula, CA
    Posts
    33
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Did the sand return to its original state after it cooled down? Just want to know if it would be reusable.

    Oh! Awesome idea by the way! Has some potential, I just happen to have some kinetic sand, a dc stick welder and some scrap aluminium... Hmmm... Off to the LWS to grab some carbon gouging rods!

  3. #3
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,987
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    superuk; very cool. btw, loved the interruption during the narration.
    i.u.o.e. # 15
    queens, ny and sunny fla

  4. #4
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,767
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    I found this very interesting

    Would it have been easier to use an AC welder and two carbon arc rods?
    Basically the old carbon arc torch used to heat bolts and such.

    If you did this you'd have a nice steady arc that wouldn't go out.

    Your video led me to look up this DIY crucible process.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  5. #5
    Join Date
    Jul 2013
    Location
    Pine City mn.
    Posts
    2,503
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Wow!!! That is incredible. I doubt I'll ever have reason to use that, but I have some carbon rods laying on the shelf
    Yeah, I know, but it'll be ok!

    Lincoln Square wave 255
    Miller Vintage mig
    30a spoolgun
    Thermal Dynamics Pacmaster 100xl plasma
    Smith mc torch
    Ellis 1600 band saw

  6. #6
    Join Date
    Aug 2014
    Posts
    3
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Quote Originally Posted by Sheyda36 View Post
    Did the sand return to its original state after it cooled down? Just want to know if it would be reusable.
    The dye in the sand has turned grey, but otherwise flows the same as before.

  7. #7
    Join Date
    Aug 2014
    Location
    Temecula, CA
    Posts
    33
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Quote Originally Posted by superUnknown View Post
    The dye in the sand has turned grey, but otherwise flows the same as before.
    Cool! I will have to try this!

  8. #8
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,241
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Basically a miniature version of an electric arc furnace like they use to melt steel. ( I can't find the really good video some one here posted up a while back.)




    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  9. #9
    Join Date
    Oct 2011
    Location
    Elkhorn, WI
    Posts
    1,715
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Where does a person get graphite crucibles?

  10. #10
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,241
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Jewelry supply houses or casting suppliers have them available. Also check art supply places.


    Quick one I pulled off my saved list when I was thinking about making a gas fired furnace to cast alum. I may have other suppliers on my other computer.

    http://www.budgetcastingsupply.com/F...les-s/1830.htm
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  11. #11
    Join Date
    Mar 2010
    Location
    Morton, Washington
    Posts
    4,997
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    I saw this the other day... I'm definitely going to try it.

  12. #12
    Join Date
    Aug 2014
    Posts
    3
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Quote Originally Posted by drujinin View Post
    Where does a person get graphite crucibles?
    I got mine on flea bay. Aliexpress also has 'em.

  13. #13
    Join Date
    Jul 2011
    Location
    Melbourne, Australia.
    Posts
    878
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Hi, years ago around '75, we used to melt aluminium in a steel ladle with a propane torch.....the ladle was the type used for melting lead etc, and held about a litre of alluminium.

    The furnace was a collection of fire bricks arranged around the ladle and the propane torch fired in one side and exhausted out the top.

    People say that aluminium does not cast well melted in a steel crucible, but we made many aluminium hammers for the shop and cast them also in a split steel mould......I still have one that I use on the mill for setting up etc.

    Then 10 years ago I melted aluminium in a steel pot using hardwood in a furnace made from a 25 litre drum lined with fire brick.

    The aluminium was scrap offcuts from rolled plate stuff with some chippings from the lathe added too.
    Ian.
    Last edited by puddytat; 08-23-2014 at 05:14 AM.

  14. #14
    Join Date
    Nov 2014
    Location
    Southwestern Ontario
    Posts
    14
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    What would the strength of this aluminium be. Just the same as its original form?

  15. #15
    Join Date
    Mar 2014
    Location
    North East Indiana
    Posts
    447
    Post Thanks / Like

    Re: DC stick = easiest aluminum casting ever

    Aluminum often requires a heat treatment to bring it back to strength. But like any casting, it can only be as strong as the materials used, and quality of the casting.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,611,776,139.50930 seconds with 11 queries