    I was wondering if anyone has had an experience regarding the Weldcraft 17 series flex head compared to the knockoff versions.

  2. #2
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,569
    Post Thanks / Like

    Re: 17 series TIG torch

    I have. I usually don't like flex heads though
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller Maxstar 161STH
    Miller AEAD200LE
    Hobart MIG
    Lincoln Idealarc 250

  3. #3
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,611
    Post Thanks / Like

    Re: 17 series TIG torch

    Is it worth the money to buy the name brand?

  4. #4
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    3,006
    Post Thanks / Like

    Re: 17 series TIG torch

    Who do you consider a knockoff? CK is generally considered superior.

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,930
    Post Thanks / Like

    Re: 17 series TIG torch

    Weldcraft silicon is crap compared to CK's rubber flex heads. I only know because I burned up quite a few so far trying to find one that holds up.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  6. #6
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,611
    Post Thanks / Like

    Re: 17 series TIG torch

    Chinese like weldcity or others. Duty cycle shouldn't be a problem.

  7. #7
    Join Date
    Jan 2014
    Location
    Palmer AK
    Posts
    5,048
    Post Thanks / Like

    Re: 17 series TIG torch

    I have a weldcraft 17 valve, with the flexhead. 25'....
    I've really abused it, and it still is holding up...

  8. #8
    Join Date
    Jul 2014
    Location
    Central fl
    Posts
    544
    Post Thanks / Like

    Re: 17 series TIG torch

    Buy the cheap version. All the consumables are the same. Weld city sells the wp17 flex head with valve and 25' hose and sheath for like $70. I run the same setup on my scratch start rig and have had no problems at all!
    Real welders know how to penetrate!

    (Equipment)
    Whatever can be used to beat my opponent into submission!

  9. #9
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,611
    Post Thanks / Like

    Re: 17 series TIG torch

    Quote Originally Posted by Dantheharleyman99 View Post
    Buy the cheap version. All the consumables are the same. Weld city sells the wp17 flex head with valve and 25' hose and sheath for like $70. I run the same setup on my scratch start rig and have had no problems at all!
    I have a weldcraft 150, same as a 17 non flex head and was looking to get a flex head. Weld city looked to be less than half the price.

  10. #10
    Join Date
    Feb 2009
    Location
    Chicago
    Posts
    6,235
    Post Thanks / Like

    Re: 17 series TIG torch

    I love my $12 china 17 flex head. But the ck ones are nice too. Not worth the money IMO.
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    Esab ET220i
    Razorweld 195 Mig
    Razorweld 200ac/dc Tig
    Tormach 770, Tormach xstech
    Carbide3d Nomad3
    Sherline 4400 CNC Lathe

  11. #11
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,569
    Post Thanks / Like

    Re: 17 series TIG torch

    I broke a couple weldcraft flexheads, also burned a few up. Seem to have better luck with the non flex, maybe its just me though. My next torch will be a CK with superflex hoses.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller Maxstar 161STH
    Miller AEAD200LE
    Hobart MIG
    Lincoln Idealarc 250

  12. #12
    Join Date
    Jan 2004
    Location
    Houston, TX
    Posts
    1,200
    Post Thanks / Like

    Re: 17 series TIG torch

    You can get a CK 17F from HTP/usaweld pretty cheap in several configurations.

  13. #13
    Join Date
    Mar 2013
    Posts
    87
    Post Thanks / Like

    Re: 17 series TIG torch

    Quote Originally Posted by cope View Post
    You can get a CK 17F from HTP/usaweld pretty cheap in several configurations.
    That's what I have. It was really cheap and it had the everything I needed to connected it to my Everlast TIG unit. I would recommended it. I would not recommend the Everlast unit.

  14. #14
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,611
    Post Thanks / Like

    Re: 17 series TIG torch

    Thanks for the replies. A while back I bought a whole bunch of TIG stuff but none of it was for a gas valve. I ordered a weldcity flexible head to go on a cable and handle that I had so I am getting by pretty cheap.

  15. #15
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,611
    Post Thanks / Like

    Re: 17 series TIG torch

    Does anyone know if they make a female 50mm dinse to a 25 mm male dinse adapter.

  16. #16
    Join Date
    Feb 2009
    Location
    Chicago
    Posts
    6,235
    Post Thanks / Like

    Re: 17 series TIG torch

    Yes, I think brwelding supplies has them
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    Esab ET220i
    Razorweld 195 Mig
    Razorweld 200ac/dc Tig
    Tormach 770, Tormach xstech
    Carbide3d Nomad3
    Sherline 4400 CNC Lathe

  17. #17
    Join Date
    Mar 2013
    Posts
    87
    Post Thanks / Like

    Re: 17 series TIG torch

    Here is a link that shows all your options. You can call them also. They are very helpful.

    http://www.lencocanada.com/admin/upl...2005%20291.pdf

  18. #18
    Join Date
    Nov 2009
    Location
    Tennessee
    Posts
    5,989
    Post Thanks / Like

    Re: 17 series TIG torch

    Try weldingsupply.com, they have great prices on name brand stuff. I used to order from them online, now I try to make it to their store whenever I can. I deal with Jim there, and he is a top notch guy.
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

  19. #19
    Join Date
    Apr 2014
    Location
    Greensboro, North Carolina, United States
    Posts
    594
    Post Thanks / Like

    Re: 17 series TIG torch

    If you know what you're looking for, amazon has good deals.
    Thermal arc 211i
    Ck flex-loc 150 & 130
    Clamps, saws & grinders
    Harbor freight 80 amp inverter

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,301,132.03385 seconds with 19 queries