    My other objection to using internet "brokers" is the commission they charge for being the middle man. To make any money off most things, you have to price them in the stratosphere!

    Good tongs, the OC ones. I have two or three and really like them. Andy Blakeney over at Quick and Dirty Tools, Centaur Forge and Pieh Tools' Billy tongs (USA models) are all excellent tongs. I make most all of my tongs, but years ago just starting out, it was easier to buy tongs to make tongs...LOL
    Last edited by shortfuse; 2 Weeks Ago at 09:15 PM.

  2. Likes ronsii liked this post
  3. #1327
    Join Date
    Sep 2013
    Posts
    1,099
    Post Thanks / Like

    Re: Blacksmithing and forging

    Paying those fees does suck, especially since it seems like everyone wants their cut!


    On another note, I just got an inquiry to see if I could make these hooks out of brass rather than good iron.

    Name:  fullsizeoutput_782.jpg
Views: 97
Size:  196.2 KB

    I've never worked with brass before. I'm curious about the project, but have no idea what to look for. Normally, I'd start out with a length of 1/4x1/2" mild steel and forge the end to a taper, then drive in a ball punch to make the countersinks. With brass, though, I have no clue what alloy to buy, if I can buy it in dimensional stock or only round bar, etc.

  4. #1328
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,049
    Post Thanks / Like

    Re: Blacksmithing and forging

    I'm not sure either, but I think it's going to be more prone to cracking and breaking than what you are used to... and far more temperature sensitive.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  5. Likes ronsii liked this post
  6. #1329
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,085
    Post Thanks / Like

    Re: Blacksmithing and forging

    Now here is a man sized forge!!! It has two high pressure 6 million BTU full length burners and it's portable!!!!

    Name:  18wheel-barbecue.jpg
Views: 65
Size:  62.6 KB


    Well ok... it only looks like a forge

  7. Likes VaughnT, whtbaron liked this post
  8. #1330
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    2,697
    Post Thanks / Like

    Re: Blacksmithing and forging

    You got a dash cam for all these cool photos or using your phone ??


    Sent from my iPhone using Tapatalk
    :

  9. Likes ronsii liked this post
  10. #1331
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,085
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by Lis2323 View Post
    You got a dash cam for all these cool photos or using your phone ??


    Sent from my iPhone using Tapatalk
    I do run a pretty decent cheepy cashcam... but these are from my phone sometimes they get a bit blurry if I'm trying to eat while taking the pic and drive with my knee....
    here's the newest overpass in Fife... they started it a few months ago.
    Name:  fife-overpass3.jpg
Views: 70
Size:  50.7 KB

  11. Likes Lis2323, DavidR8 liked this post
  12. #1332
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,342
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by VaughnT View Post
    Paying those fees does suck, especially since it seems like everyone wants their cut!


    On another note, I just got an inquiry to see if I could make these hooks out of brass rather than good iron.

    Name:  fullsizeoutput_782.jpg
Views: 97
Size:  196.2 KB

    I've never worked with brass before. I'm curious about the project, but have no idea what to look for. Normally, I'd start out with a length of 1/4x1/2" mild steel and forge the end to a taper, then drive in a ball punch to make the countersinks. With brass, though, I have no clue what alloy to buy, if I can buy it in dimensional stock or only round bar, etc.
    Have you thought about stopping by a local thrift store and grabbing some brass decorations or items?
    You can practice with that for only a couple dollars. Kind of like practicing with clay before using steel.
    It might be a cheap source of materials that can be reforged into something useful


    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  13. Likes DavidR8, ronsii liked this post
  14. #1333
    Join Date
    Sep 2013
    Posts
    1,099
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by psacustomcreations View Post
    Have you thought about....

    All this talk about brass has got me thinking about it pretty hard, but I don't know that I'd find anything at the flea markets and such.

    I did look online to see what was available and Online Metals has 1/4x1/2 on sale for half off. If I remember right, it was only $12 plus shipping for a 48" bar of the stuff and they tell you the alloy and applications it's suitable for. Almost bought the wrong alloy because I wasn't paying attention!

    The customer balked at the price, though, so I won't have to worry about it for the time being. I might buy a bar or two for myself because it's not really expensive even at full price, and it would be fun to make up a couple hooks just so I could say I did. It certainly wouldn't be something feasible for market, I don't think. The cost of the metal, including the shipping, is very high and prices something like simple hooks right out of anyone's budget! :O

  15. Likes ronsii, Lis2323 liked this post
  16. #1334
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,049
    Post Thanks / Like

    Re: Blacksmithing and forging

    That might be a good thing. Anything used in brass that I've seen tends to get lumped in as an automatic "antique" and the prices go up as well. I can see where you'd want to know the alloy, rather than taking a chance on something made in China 10 yrs ago that was made to look old. I can see where you might be tempted to experiment though...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  17. Likes ronsii, Lis2323 liked this post
  18. #1335
    Join Date
    Sep 2013
    Posts
    1,099
    Post Thanks / Like

    Re: Blacksmithing and forging

    I have some 5/8" brass rod here that I tried forging since... why not. It just crumbled under the hammer even at a low heat. Two or three hits with the hammer and it shattered.

    Apparently alloy matters!

    I might be able to find something at the junk stores, but would it be forgeable or would it be a machining alloy? I've since repurposed that rod into non-marring punches to drive out stuck things.

  19. Likes ronsii, whtbaron liked this post
  20. #1336
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,085
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by VaughnT View Post
    I have some 5/8" brass rod here that I tried forging since... why not. It just crumbled under the hammer even at a low heat. Two or three hits with the hammer and it shattered.

    Apparently alloy matters!

    I might be able to find something at the junk stores, but would it be forgeable or would it be a machining alloy? I've since repurposed that rod into non-marring punches to drive out stuck things.
    Yep.... depends on just how much zinc and how much copper is in the mix.... and if it's chinese how much lead??? Will be a fine line between enough heat to make it putty or water

  21. Likes VaughnT, whtbaron liked this post
  22. #1337
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    3,049
    Post Thanks / Like

    Re: Blacksmithing and forging

    That was what I was thinking when you first mentioned working in brass.... says the guy with no real experience other than fishing out busted parts...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  23. Likes Lis2323, ronsii liked this post
  24. #1338
    Join Date
    Apr 2015
    Location
    N 48 38.680 W 080 40.837
    Posts
    591
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by VaughnT View Post
    I have some 5/8" brass rod here that I tried forging since... why not. It just crumbled under the hammer even at a low heat. Two or three hits with the hammer and it shattered.
    It sounds like what you had was Bronze maybe? And yes, alloy matters.

    As far as "shattering". In my tool box I have an assortment of BRASS punches that I made myself many years ago. They are various diameters and profiles, but they do not shatter. They are very soft, as was the intention when I made them, so they readily deform when hammered and are easily hammered into various shapes, even without heat.

  25. Likes VaughnT liked this post
  26. #1339
    Join Date
    Sep 2013
    Posts
    1,099
    Post Thanks / Like

    Re: Blacksmithing and forging

    Now that you mention it.... could be bronze.

    No idea, really, what's going on with those fancy-pants metals. Gimme good solid American iron any day of the week. That weird French stuff....


  27. Likes ronsii, whtbaron liked this post
  28. #1340
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,342
    Post Thanks / Like

    Re: Blacksmithing and forging

    Some of this is blacksmithing, some scrap metal stuff.

    Over the last month or so, I have had several customers ask for hooks for bells they have purchased. I decided to make several styles. Some are made to go horizontal like on a post, others hanging straight down from a beam. These are in the unfinished form so they need cleaning and treatment of some kind. I may leave them as they are for now until asked for a specific finish.



    Name:  20201020_143928.jpg
Views: 17
Size:  120.0 KB
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  29. Likes ronsii, VaughnT liked this post
  30. #1341
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,085
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by psacustomcreations View Post
    Some of this is blacksmithing, some scrap metal stuff.

    Over the last month or so, I have had several customers ask for hooks for bells they have purchased. I decided to make several styles. Some are made to go horizontal like on a post, others hanging straight down from a beam. These are in the unfinished form so they need cleaning and treatment of some kind. I may leave them as they are for now until asked for a specific finish.



    Name:  20201020_143928.jpg
Views: 17
Size:  120.0 KB
    Nice!!! I'm curious how you shrunk the end of the bottom right rebar hook while keeping the 'look' of rebar... did you somehow stretch it or just really careful striking? or am I just thinking it is tapered smaller for the last inch or two on the tip??

  31. #1342
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,342
    Post Thanks / Like

    Re: Blacksmithing and forging

    Quote Originally Posted by ronsii View Post
    Nice!!! I'm curious how you shrunk the end of the bottom right rebar hook while keeping the 'look' of rebar... did you somehow stretch it or just really careful striking? or am I just thinking it is tapered smaller for the last inch or two on the tip??
    you are correct, careful striking of the last inch or so.
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  32. Likes ronsii liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,308,874.54225 seconds with 14 queries