had to cut out some 1/4 inch 6061 from a scrapped project for some stands for a aluminum fuel tank (vids of that project later) so i decided to make one of just the plasma cutter.... its a hi-def cutter and kicks the snot outta my old thermal dynamics cutter
Last edited by longevity-inc.com; 03-14-2011 at 03:31 PM.
migweld 250p
arcmate 205
weldall 250pi
forcecut 80i plasma
'07 pro 300 miller
'08 trailblazer 302
mm350p
dynasty 700
dynasty 200
deltaweld 452
xr-a 50ft push pull feeders and gooseneck
yes, i know... it doesnt use dual gas for plasma, however, it has tons more definition than my cutmaster has. tons more. ive seen plasma machines that cost upwards of quarter mil that are truly hi-def... was only trying to say that for the price tag, this machine has great definition... i should have worded it differently and thanks for pointing this out to me
migweld 250p
arcmate 205
weldall 250pi
forcecut 80i plasma
'07 pro 300 miller
'08 trailblazer 302
mm350p
dynasty 700
dynasty 200
deltaweld 452
xr-a 50ft push pull feeders and gooseneck
Stan, your posts might carry more credibility (especially in a sponsored forum) if you deleted the "No ads - Just Advice" from your signature line.
That video was 100% ad and 0% advice.
Just throwing it out there.
Miller Dynasty 200DX
Millermatic 210 w/ Spoolmate 3035
Hypertherm Powermax 380
JD Squared Model 32
Multiple fabrication tools & equipment
Full Powder Coating Setup
MillerFab,
I take full blame for that line in the signature. Our plan was to have someone credible not pushing our equipment as a sales man. Someone that uses our equipment daily and shows whats is capable off. However, i can see the conflict this may cause as advertising.
Stan did not write that. Our staff did when this performance account was created. We dont want to mislead so it will be removed. You are the second person who complained about this.
Our customers enjoy the videos and hopefully more welding web members will as well.
Simon
narrow kerf. and when hooked up with nitrogen instead of compressed air, it even leaves a glossy finish on aluminum. throw o2 at it and it leaves a glossy finish on carbon steel as well.... ive run both hypertherm and thermal machines and neither would produce the way this one does. only machine ive seen close was a panasonic, but was cost prohibitive
migweld 250p
arcmate 205
weldall 250pi
forcecut 80i plasma
'07 pro 300 miller
'08 trailblazer 302
mm350p
dynasty 700
dynasty 200
deltaweld 452
xr-a 50ft push pull feeders and gooseneck
how much did that plasma cutter cost you