+ Reply to Thread
Results 1 to 14 of 14

Thread: Flashback

  1. #1
    Join Date
    Jan 2006
    Location
    In A Nice Comfy Chair
    Posts
    18,773
    Post Thanks / Like

    Flashback

    Here is a link that was provided by a member about Flashback.

    http://www.toolboxtopics.com/Gen%20I...0Flashback.htm

    It happened to me so I thought it's best to make this a stickey..

    Thank you jbmprods for the link!

    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

  2. #2
    Join Date
    Jan 2006
    Location
    chico ca
    Posts
    708
    Post Thanks / Like

    Re: Flashback

    your welcome Zap and glad it was just a wake up call. good idea you have hear to. lots of folks will see it.
    225NT bobcat
    AEAD200LE
    Scott 125
    mm175, mm252 w 30A, PT225
    mm211, TA 181i
    Hyper Therm 380, cut master 52
    9100X & XX, Digital Elite
    6 Victor sets
    smith little torch, meco midget
    kalamazoo band saw
    steel max saw
    evoulution circular saw

  3. #3
    Join Date
    May 2007
    Location
    Okanagan Valley.
    Posts
    875
    Post Thanks / Like

    Re: Flashback

    A good combination is to have flashback arrestors at the regulators and check valves at the torch end.

    The check valves are nice because they don't add a lot of bulk at the torch end.


    And these are the arrestors.

  4. #4
    Join Date
    Aug 2009
    Posts
    4,320
    Post Thanks / Like

    Re: Flashback

    When you inspect torches, keep an eye out for indications of internal fire damage such as heat discoloration.

    This now-much-shorter Victor mixer left parts of itself in the tube when it melted. I guess the Smith and Airco designers have a point. Tip-mix torches don't do this:
    Attached Images Attached Images  

  5. #5
    Join Date
    Apr 2012
    Location
    Michigan
    Posts
    127
    Post Thanks / Like

    Re: Flashback

    good post...this is good to know...i always lite my torch with mixed gas so it does have all the black smoke.

    Quote Originally Posted by zapster View Post
    Here is a link that was provided by a member about Flashback.

    http://www.toolboxtopics.com/Gen%20I...0Flashback.htm

    It happened to me so I thought it's best to make this a stickey..

    Thank you jbmprods for the link!

    ...zap!

  6. #6
    Join Date
    Oct 2010
    Location
    NC
    Posts
    15
    Post Thanks / Like

    Re: Flashback

    I would recommend investing in a newer torch with built-in flashback arrestors and reverse flow check valves. It is too easy to get in a hurry and not take the time to put these in the line to the regulators separately.
    Ranger 225
    Weld Pac 100
    Power Mig 180C
    Magnum 100 Spool Gun
    Hobart EZ Tig 165i



    Surf for cardiovascular exercise. Saltwater is good for you.

  7. #7
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: Flashback

    under what circumstances would anyone use acetylene over 15lbs? i find 10 lbs works fine for everything from sheet metal to 3" plate by changing the cutting tip to the correct size.

  8. #8
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    18,081
    Post Thanks / Like

    Re: Flashback

    This one provides an excellent visual of what takes place during those undesireable conditions.
    [ame]http://www.youtube.com/watch?v=xwOkUxe8Xy8&list=PL47639173BE8AF3F8&featur e=player_embedded[/ame]


    Last edited by DSW; 10-21-2013 at 05:20 PM. Reason: Fixed bad link.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  9. #9
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    18,081
    Post Thanks / Like

    Re: Flashback

    Just reposted it Steve. Someone else did awhile back and I think the entire video series on proper setup and use should be a must watch for newbe OA torch users as well as a refresher for seasoned operators.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  10. #10
    Join Date
    Feb 2013
    Location
    Kentucky
    Posts
    226
    Post Thanks / Like

    Re: Flashback

    Great thread with great info!.. The YouTube was nice too! Showing what can happen during a "flashback''!

    How many on here have the flashback arrestors on their O&A setup ?

    Thanks!
    Hobart Handler 190
    Hobart Spool-Gun 100
    Lincoln 225 AC
    Miller & Pipeliner Hood
    Dewalt 14" Chopsaw, Grinders
    Harris O/A
    Victor Torch
    Custom Built O/A Cart
    Custom Welding Cart
    Heavy Duty 16 Speed Floor Drill Press
    Pipe-Bender
    Drill Doctor

  11. #11
    Join Date
    Apr 2012
    Location
    Western Kentucky
    Posts
    197
    Post Thanks / Like

    Re: Flashback

    Quote Originally Posted by WelderBill View Post
    Great thread with great info!.. The YouTube was nice too! Showing what can happen during a "flashback''!

    How many on here have the flashback arrestors on their O&A setup ?

    Thanks!

    I was first introduced to acetylene welding 47 years ago when my dad welded aircraft tubing. He never had flashback arrestors on his equipment. He never had a flashback because he followed proper procedures. With that being said, I believe he was more lucky than good. This stuff can happen to anyone.
    The older you get, the more safety conscious you become. Some call me paranoid, worry to much, etc. I've installed flashback arrestors on my torches, because I'd rather be a worrywart, than a dead wart.
    Last edited by Gobysky; 10-05-2013 at 09:28 AM.
    Build many useful items for around the home and for friends
    A great and useful retirement hobby

    Syncrowave 200
    Millermatic 252
    Spoolmatic 30A
    Spectrum 625 X-Treme
    Victor O/A torches
    Dewalt angle grinders

  12. #12
    Join Date
    Dec 2011
    Posts
    89
    Post Thanks / Like

    Re: Flashback

    I was thinking of putting flashback arrestors on my Victor med. duty torch handle but the 3/8 sizxe seems nonexistent.
    Maybe I am missing them but all seem to be 9/16.
    Doing the best I can with what I got

  13. #13
    Join Date
    Nov 2011
    Location
    Detroit, MI
    Posts
    236
    Post Thanks / Like

    Re: Flashback

    Thanks to the member that originally provided Zapster with the link that started this thread.

    Way too many guys using torch rigs and don't know how close to a (catastrophic) failure they are at.
    How do you know the blacksmith's dog? When you hollar at him he makes a bolt for the door!

  14. #14
    Join Date
    Sep 2014
    Posts
    2,372
    Post Thanks / Like

    Re: Flashback

    Quote Originally Posted by duaneb55 View Post
    Just reposted it Steve. Someone else did awhile back and I think the entire video series on proper setup and use should be a must watch for newbe OA torch users as well as a refresher for seasoned operators.
    I cannot see the video, youtube says the video does not exist.

    Sincerely,

    William McCormick

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,273,960.51307 seconds with 20 queries