    Nozzle dip & a contentious neighbor

    Searched several times and all my searches for "nozzle dip" turned up so many results that the search is basically futile; so here's the question/issue:

    I'm using nozzle dip for my Mig gun - a petrolatum formula; can't recall the name right now (it's blue). It does seem to help the wire run better through the gun; after a while when it depletes I can feel the wire "chatter" as it runs through the gun...

    SO, YES, it does seem to do what it claims to do. It does make quite a bit of smoke/vapor... which I do my best to get rid of using a draft system + general shop ventilation; plus filter/respirator under the welding hood

    HOWEVER, my shop neighbor- across the hall, shared open air space (who is admittedly sensitive to smells - can smell paint being sprayed in an open air bay of another section of the building 100 yards away...) claims that:

    1) the smoke is giving him a headache

    2) nozzle dip is just a gimmick and doesn't do anything anyhow

    3) the "smoke" from it is toxic (it says 'non toxic/ non-flammable on the container)

    4) he has welded for years without any nozzle dip, and "I should learn how to weld without it too"

    5) he hasn't even changed his Mig tip in 2+ years, and his welds are fine...

    Results are results, in my book, and the dip works for me so I don't really care what anybody thinks about whether it works or not. BUT I would like to maintain a good relationship with my neighbor, so I'd love commentary on the relative merits of nozzle dip, specifically:

    * Is its use common, rare, almost non-existent?

    * Is it, or is it not toxic?

    * Is the "smoke" actually smoke (i.e. combustion) or is it vapor?

    * What are the health implications (medically known/experienced; not conjectural BS) of breathing burned/vaporized petrolatum - essentially, vaseline.

    * Is there a better solution?

    Thanks for your thoughtful, concise, on-topic answers!

  2. #2
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,402
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    That's not what it does.

    What it does is help spatter not stick to the inside of the nozzle - which it does very well and makes the spatter that does stick come off easier.

    If you are mig welding with argon/co2 mix, you don't need it. I use it when I run 100% co2 since it spatters a little more.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  3. #3
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,610
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Once you burn it off its gone, smell wise. There is a white ceramic based stuff that doesn't smoke and lasts longer.

  4. #4
    Join Date
    Dec 2010
    Location
    Piedmont, SD
    Posts
    2,058
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Quote Originally Posted by peanutjar View Post
    I'm using nozzle dip for my Mig gun - a petrolatum formula; can't recall the name right now (it's blue). It does seem to help the wire run better through the gun; after a while when it depletes I can feel the wire "chatter" as it runs through the gun...
    Chatter? Have you a properly sized liner and nozzle installed? The dip wasn't designed to aid in wire travel through your mig gun other than to keep slag buildup at bay.
    Lincoln PrecisionTig 275
    Miller 251
    Miller DialArc 250
    Bridgeport mill
    Hossfeld bender & dies
    Logan shaper
    Jet 14 X 40 lathe
    South Bend 9" 'C'
    Hypertherm 900
    Ellis 3000 band saw
    21"Royersford Excelsior
    Two shops, still too many tools.

  5. #5
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    peanutjar

    MIG Dip/Spatter Spray is often over-used.

    This is a reprint from 11-11-14.

    I take a different approach to nozzle hygiene.

    I have a Miller D60 Dual feeder on a XMT 300.
    I run .024 and .030 Hard Wire in one gun, and .035 and .045
    Dual Shield in the other - without daily Spatter Spray or Dip.

    I have had a 12oz. can of Jokisch LB-100W for over 15 years, it's
    1/3 full, and still has pressure. It is only used for initial coating
    of new contact tips and nozzles.

    You can ‘season’ a tip and nozzle just like a cast-iron kettle, and
    they will last for years.

    Easy as changing an inside dual:

    begin with a new contact tip & nozzle – spray both – then:
    carefully run stringers until the gun is hot,
    immerse in Mig Dip,
    hang the gun so it drains and cools [until the Dip congeals],

    repeat the: weld to heat, dip, hang, cool cycle several times.

    The exercise is to heat the gun, not actually weld, so use clean
    metal, and angle the gun to optimize gas coverage.

    Also key to longevity: is the ongoing treatment of the gun, the
    cleansing mode of the nozzle, and a tight insulator.

    Great care should be taken not to mar the OEM finish of the nozzle.
    Any nick or abrasion is a foot-hold for spatter to stick. I only tap
    the nozzle at it base, and I use a chop-stick to swab the inside.

    With patience and technique - nozzle frustration is manageable.


    Opus

  6. #6
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Your problem is, you are using the wrong gun. I would go for years, and years, and years without ever seeing a can of nozzle dip or spray.
    Attached Images Attached Images  
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  7. #7
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,930
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Quote Originally Posted by peanutjar View Post

    I'm using nozzle dip for my Mig gun - a petrolatum formula; can't recall the name right now (it's blue). It does seem to help the wire run better through the gun; after a while when it depletes I can feel the wire "chatter" as it runs through the gun...
    Are you putting nozzle dip on your wire. That is wrong. Years ago I was using that "Weld-Aid" wire lube as I was too lazy to blow out my liner. Only way to keep the wire from sticking was to use more of that crap. Finally got fed up and put in a new liner and ran it dry. Blew it out at every wire change.

    Yes nozzle dip is smoky, stinky, and overall obnoxious, but it does reduce spatter buildup on the tip and nozzle. I hate it at it too makes me nauseous. I also use the ceramic spray coating on alum and steel mig guns which last hours.

    Be a good neighbor and work on a solution.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  8. #8
    Join Date
    Jan 2004
    Location
    Northern Cal., Shasta County
    Posts
    9,327
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    As mentioned, nozzle dip and/or spray isn't intended to 'lube' anything just keep spatter from sticking. I have a cheap spray I use on new tips, tip size swaps and screw ups. It smells like cod fish being deep fried for awhile. I suppose that could give someone a headache, if so that same person couldn't go into a fish 'n chips place or a greasy spoon resteraunt without gettin a headache.

    Here's the real problem. It starts at birth. When a baby is 1st born it cries,, and those cries get it rewarded by a warm cuddly mother, then it cries more,, gets a warm teat in its mouth. Who wouldn't cry if that happened every time. That baby soon learns that the more and the longer it cries, the more and more it gets its way. It learns to manipulate any body and every body by incessant crying. Then one day it becomes an adult, a welder and has a booth across the hall, very experienced at crying ---- see where I'm going with this?

    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  9. #9
    Join Date
    Jul 2013
    Location
    Pine City mn.
    Posts
    2,493
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    I have a can of nozzle spray in the shop all the time, but the only thing I use it for is on my band saw blade and flap discs when working aluminum as it's the best thing for keeping the aluminum from gumming them up.

    Sent from my VS985 4G using Tapatalk
    Yeah, I know, but it'll be ok!

    Lincoln Square wave 255
    Miller Vintage mig
    30a spoolgun
    Thermal Dynamics Pacmaster 100xl plasma
    Smith mc torch
    Ellis 1600 band saw

  10. #10
    Join Date
    May 2015
    Location
    Barre Town, VT
    Posts
    872
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    While I have never used nozzel dip before I will say that I know it doesn't luberacate the wire. I've never used nozzel dip because spatter build up has never been a huge issue. I'd try to figure out what is causing so much spatter before investing in nozzel dip.
    My "collection":

    Homemade Stick Welder
    Victor O/A Torch
    AC 225
    Ideal Arc 250

    HF 90 Amp Flux Core
    HF Mig 170
    Solar 2020 Plasma Cutter
    Power i-Mig 140E
    Harris O/A torch
    HF Dual Mig 131
    140ST
    Alpha Tig 200x

  11. #11
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    I would imagine when you dip a hot nozzle in that stuff that some of it finds its way inside the tip and reduces chatter until it burns away. We are having lots of trouble with wire chattering in the tip since we switched over to Hobart H4 Megafil. Once that tip gets hot the wire starts hanging up until eventually you get a bird nest if you keep going. We never had any trouble with the Kobelco wire we used to use. We've tried using .052 tips on .045 wire, doesn't really help.
    I think I'm gonna try some of that dip. Even though I never have liked it, it shouldn't matter now that i have the fresh air hood.

    Are you using Hobart H4, peanutjar?

    I would tell your neighbor across the way to pound sand. If he's that sensitive to smells, he's in the wrong profession.


    You can google that stuff and find an MSDS online.
    Last edited by TimmyTIG; 07-16-2015 at 06:39 PM.

  12. #12
    Join Date
    May 2012
    Location
    Ontario, Canada
    Posts
    1,505
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Some folks use pam cooking spray as nozzle spray.

    How can he complain about that ?

  13. #13
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,735
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    The nozzle dip helps for awhile. I finally just got so I clamp a 1/2" drill bit in the vise and when the nozzle gets a lot of buildup in it, I take it off and run the bit thru it to clear it.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  14. #14
    Join Date
    Aug 2014
    Location
    New Orleans
    Posts
    187
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    I can't say much about your nozzle dip....But your neighbor of the shared space needs to get used to it and keep quiet...or move to his own building.

    Its a shared space...and that's the way it is IMO. Kind of like living in an apartment complex and complaining that the neighbor who works the night shift is waking you up when he goes to work at 2 AM.

  15. #15
    Join Date
    Jan 2015
    Location
    Florida
    Posts
    104
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Quote Originally Posted by 12345678910 View Post
    Some folks use pam cooking spray as nozzle spray.

    How can he complain about that ?
    I use Pam.... Jody says Vaseline works too...
    Lincoln PowerMIG 350mp
    Everlast PowerTIG 210EXT
    Hypertherm PowerMax45

    You merely adopted the iron, I was born in it, molded by it.

  16. #16
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,735
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Hand him a nice new white hanky to wipe away all the tears.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  17. #17
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    mla2ofus

    Are you on 'Hooper Water' again!


    Opus

  18. #18
    Join Date
    Sep 2010
    Location
    Sparks Nevada
    Posts
    303
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Quote Originally Posted by doojus View Post
    I use Pam.... Jody says Vaseline works too...
    Jody? Jody Grinder? I haven't heard about him for ever.
    Dan

    I hope that when i'm dead and gone, people will remember me and think; "Boy, that guy sure owed me a lot of money!"

  19. #19
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,735
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    Quote Originally Posted by OPUS FERRO View Post
    mla2ofus

    Are you on 'Hooper Water' again!


    Opus
    Nope, haven't had any for years, LOL!!
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  20. #20
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,930
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    So am I reading this right? The noxxle dip is wicking into the tip for lubrication? And that is helping the feeding? I think the problem lies in the fact that the tip is getting sticky because of the noxxle dip when it gels. Perhaps that and the combination of junk wire could be happening. I found that other than Linlcoln and Esab steel wire, I would have lackluster feeding.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  21. #21
    Join Date
    Apr 2011
    Location
    minnesota
    Posts
    2,098
    Post Thanks / Like

    Re: Nozzle dip & a contentious neighbor

    used to use nozzle dip till I figured out that I didn't need it. I just use a 1/2 lag bolt to clean the nozzle.
    Millermatic 252
    millermatic 175
    miller 300 Thunderbolt
    lincoln ranger 250
    smith torches
    lots of bfh's
    If it dont fit get a bigger hammer

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,279,127.47729 seconds with 20 queries