+ Reply to Thread
Page 4 of 4 FirstFirst ... 234
Results 76 to 81 of 81

Thread: Anyone make a out door propane cooking griddle top?

  1. #76
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Anyone make a out door propane cooking griddle top?

    Things I would change. Bigger area for grease to flow into. My area was done with .5" ball end mill. Sides are highe enough. There 2" sides that taper down a little. Pretty much just more grease trap area. And yes I've had it at a few friends houses. At first I was making a mess with a onions flying off the front but now I'm carful and lose maybe a piece of onion or 2, then get pissed and try to catch it. Gets up to 300 in about 10 minutes. Name:  image.jpg
Views: 374
Size:  63.8 KBburgers from the other night. There was more then this on thereName:  image.jpg
Views: 379
Size:  91.8 KBit was all build with zero plans. Just in my head

  2. #77
    Join Date
    Nov 2009
    Location
    Tennessee
    Posts
    5,989
    Post Thanks / Like

    Re: Anyone make a out door propane cooking griddle top?

    Tagged - griddle
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

  3. #78
    Join Date
    Oct 2013
    Location
    W. WA
    Posts
    538
    Post Thanks / Like

    Re: Anyone make a out door propane cooking griddle top?

    Nice build! Looks like your getting plenty of use out of it.

    DB

  4. #79
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Anyone make a out door propane cooking griddle top?

    Thanks! Made a couple more burgers tonight.

  5. #80
    Join Date
    Jun 2017
    Location
    Lower Alabama
    Posts
    1
    Post Thanks / Like

    Re: Anyone make a out door propane cooking griddle top?

    Name:  pg base4.jpg
Views: 175
Size:  65.4 KB

    Not finished yet, but should be soon.

  6. #81
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Anyone make a out door propane cooking griddle top?

    Nice welcome to the forum!

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  