    And the real beauty of it is you don't even need to dig a hole!!!! just roll it ahead a foot or so

  2. Likes DavidR8 liked this post
  3. #652
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    2,949
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by ronsii View Post
    And the real beauty of it is you don't even need to dig a hole!!!! just roll it ahead a foot or so
    Thanks for the tip. Ahead, right? Not back....?
    :

  4. Likes ronsii liked this post
  5. #653
    Join Date
    Apr 2020
    Location
    Canada
    Posts
    137
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by Lis2323 View Post
    Thanks for the tip. Ahead, right? Not back....?
    Me?
    Id roll it back...


    Sent from my iPhone using Tapatalk
    David
    Millermatic 130
    Primeweld 225
    Victor Journeymen

  6. Likes ronsii liked this post
  7. #654
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    2,949
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by DavidR8 View Post
    Me?
    Id roll it back...


    Sent from my iPhone using Tapatalk
    Easier to roll backwards while still sitting. Just watch your step when you get up, right?
    :

  8. Likes ronsii, DavidR8 liked this post
  9. #655
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,690
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by Lis2323 View Post
    Easier to roll backwards while still sitting. Just watch your step when you get up, right?
    Yep... you'll have to do the crabwalk if you roll back... or maybe that should be the crapwalk...

  10. Likes Lis2323, DavidR8 liked this post
  11. #656
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    606
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Here's what my helper and I put together to hold my Miller Dynasty 200DX tig, Hypertherm 45XP and Miller 211 mig. Used a Kennedy base cabinet for general storage, fabricated the cart from steel, and the cable hangars and top from aluminum. Tig wire storage is made from aluminum angle. Machines all plug into a box with a 50' cord. Wheels are ball bearing.




  12. Likes DavidR8, ronsii liked this post
  13. #657
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    2,949
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Heres how I wired my two TAs so that only one cord was plugged in for power.



    :

  14. #658
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    5,587
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by Lis2323 View Post


    I cant wait to see what my maintenance yard tenants think of it
    You should be a pal and fill it up with ice and beer on friday afternoon.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  15. Likes whtbaron liked this post
  16. #659
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    2,949
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by John T View Post
    You should be a pal and fill it up with ice and beer on friday afternoon.
    I was gonna say why wait for Friday??! then realized what day it was.
    :

  17. Likes DavidR8, whtbaron liked this post
  18. #660
    Join Date
    Jun 2010
    Posts
    8
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    This is a test fitup before all the final touches where put on (gun holder, cable holders, tank straps etc). The design was largely influenced by super cheap 14ga 1x2 tube and 1/8" 1 1/2" angles at my local steel supply. Buying drops for the sheet and diamond plate all the materiel including the paint and wheels/casters came in at about $100. The black is spray bed liner

    I had experimented with offsets and angles for a little while and this setup works well for me both sitting on a super low stool and standing. Everything is readable and reachable.

    Between the wire feed and the power supply is a shelf for supplies. Its just 2 1 1/2 angles making a C- there's a backing inside it to keep it from being full length and stuff becoming unreachable. It holds a couple boxes of rods and a small homak parts organizer I found which is perfect for holding the various tips, feed wheels and other gun consumables.

    There's just enough width to hold 2 tanks if I want to add a second, as long as I stay in the 80/125 size range 150 would be pushing it.

    Thinking about cutting up a little more sheet and adding sides to the bottom.


  19. Likes whtbaron liked this post
  20. #661
    Join Date
    Apr 2020
    Location
    Canada
    Posts
    137
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Heres my cart build.

    I built it from a $50, 750 lb capacity warehouse cart.
    Heres the cart in its original form.


    I cut it up into its major pieces for easier storage till I could turn it into a cart. My aim is to reuse the rounded corners as much as possible.


    Heres a shelf cut to 18 wide.


    I narrowed the tall back frame to 18. Wide enough to accommodate two 110 cu ft tanks.


    Here is the frame tacked onto the base. I mitred the corners for a clean look.


    I cut more of the parts up to make the shelf supports and the top shelf side guards.


    Im going to put a drawer for TIG consumables under the top shelf and possibly one on the base to hold grinding wheels and other gear.
    Plus Ill add hose hangers, filler rod holders and pedal holder.
    Oh and wheels


    Sent from my iPhone using Tapatalk
    David
    Millermatic 130
    Primeweld 225
    Victor Journeymen

  21. Likes whtbaron liked this post
  22. #662
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    606
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    8--good use of salvaged materials.

  23. Likes DavidR8 liked this post
  24. #663
    Join Date
    Apr 2020
    Location
    Canada
    Posts
    137
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by ezduzit View Post
    8--good use of salvaged materials.
    Thanks. I thought I might be able to use the base as it was but it wasnt a good fit. I will chop it up for the 1x3 tubing though.


    Sent from my iPhone using Tapatalk
    David
    Millermatic 130
    Primeweld 225
    Victor Journeymen

  25. #664
    Join Date
    Apr 2020
    Location
    Canada
    Posts
    137
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Just about finished the cart.
    @lis2323 provided some excellent tank straps so no chain or ratchet straps required.
    Still need to add a drawer, cable hangers and some rod holders.
    Pretty happy with how it came together.








    Sent from my iPhone using Tapatalk
    David
    Millermatic 130
    Primeweld 225
    Victor Journeymen

  26. Likes ronsii, Lis2323, whtbaron liked this post
  27. #665
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    8,690
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Lookin' good!!!!

  28. Likes DavidR8 liked this post
  29. #666
    Join Date
    Apr 2020
    Location
    Canada
    Posts
    137
    Post Thanks / Like

    Re: The Welding Cart Thread... Post 'Em Up!!

    Quote Originally Posted by ronsii View Post
    Lookin' good!!!!
    Thanks! It was fun to build. I definitely built some skills!


    Sent from my iPhone using Tapatalk
    David
    Millermatic 130
    Primeweld 225
    Victor Journeymen

  30. Likes ronsii liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,199,498.41270 seconds with 12 queries