+ Reply to Thread
Results 1 to 7 of 7

Thread: Powcon 300sm w/o feeder--good/bad

  1. #1
    Join Date
    Jan 2016
    Location
    Raleigh area, NC
    Posts
    32
    Post Thanks / Like

    Powcon 300sm w/o feeder--good/bad

    I have a Lincoln tombstone AC/DC (the little one, not idealarc).

    I know someone with a Powcon 300sm, but no feeder, under $300. Is that going to do anything for me? I was thinking more for using it as a scratch tig box, but now and then a wire feeder comes up and might be compatible. I've held off getting a mig only because of limited space, and inverters are pricey. So maybe this plus a feeder gets me a 2-for-1.

    I know these were built well, but they are old. I figure won't outlast my tombstone. Is there any advantage over what I have now? Little lighter weight. Higher output & duty cycle.

    Also, the "power level" knob is strange vs. amps. Seems that would be hard to set.

    What I really want is an inexpensive HF starter so I can use low amps to stick weld thin stock. I know this doesn't get me that.

  2. #2
    Join Date
    Aug 2008
    Location
    Sudbury, Ontario
    Posts
    954
    Post Thanks / Like

    Re: Powcon 300sm w/o feeder--good/bad

    I have used one in the past. One of the nicest arcs for stick welding I ever used. I was really disappointed when it expired.

    For you, definitely a step up from that Lincoln, not a lot of money and you can find a used feeder for it. I'd just get a suitcase feeder for it, Lincoln or Miller.
    "The reason we are here is that we are not all there"

    SA 200
    Idealarc TM 300 300
    MM 200
    MM 251

    30a Spoolgun
    Precision Tig 375
    Invertec V350 Pro
    SC-32 CS 12 Wire Feeder
    Oxweld/Purox O/A
    ArcAir
    Hypertherm Powermax 85
    LN25

  3. #3
    Join Date
    Feb 2015
    Posts
    580
    Post Thanks / Like

    Re: Powcon 300sm w/o feeder--good/bad

    Great welders, I would not hesitate to buy for that price. Almost any feeder will work and eBay always has some old Powerdrive 1 or 2's for sale that plug right in if you want to make it easy. You won't want to use the tombstone after you weld with the Powcon.
    ESAB Rebels 215 and 235, ESAB HELIARC 281i, ESAB ET 301i, Hypertherm 85 and 45XP, Thermal Arc 185, TD 60i, HTP PRO PULSE 300

  4. #4
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,402
    Post Thanks / Like

    Re: Powcon 300sm w/o feeder--good/bad

    It's cheap enough - I'd buy it
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  5. #5
    Join Date
    Jan 2016
    Location
    Raleigh area, NC
    Posts
    32
    Post Thanks / Like

    Re: Powcon 300sm w/o feeder--good/bad

    Wow, unanimous. Thanks guys. Didn't know I would notice any difference in the stick welding, but then I've only used the tombstone so no comparison to anything.

  6. #6
    Join Date
    Jan 2016
    Location
    Raleigh area, NC
    Posts
    32
    Post Thanks / Like

    Re: Powcon 300sm w/o feeder--good/bad

    Looks like the guy blew me off. Had a bad vibe about that one, anyway. I'll keep looking.

  7. #7
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    4,233
    Post Thanks / Like

    Re: Powcon 300sm w/o feeder--good/bad

    Just about any 24 volt wire feeder can be used. You just have to add a relay to reverse the welder control from normally open to normally closed.
    The 200sm takes a closed switch to turn the welder output off. Change the plug to match the powcon.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,277,167.99923 seconds with 17 queries