    Hey everybody. I've got something confusing (at least to me) going back I with my blackface SA200 (Code 7307) ; the ranges don't overlap well. There's at least a 25 amp gap between every range. For example: I can weld in first gear, fine tune on 90 all day long. But if I switch to second gear, fine tune on 10, all I can do is stick my rod to whatever I'm working on. The welder will idle up like it wants to weld but doesn't have enough umph to.

    I've tried replacing my rheostat, replacing my stinger and cleaning the brushes with no results, so advice would be greatly appreciated. Thanks in advance.

  2. #2
    Join Date
    Nov 2010
    Location
    Houston Pennsylvania USA
    Posts
    4,088
    Post Thanks / Like

    Re: Poor gear overlap

    3-10-20? Electrode?

  3. #3
    Join Date
    Mar 2015
    Location
    NE Kansas
    Posts
    40
    Post Thanks / Like

    Re: Poor gear overlap

    Sorry, but not quite sure what you mean by 3-10-20. As far as electrodes go, it does I with 1/8" 5p+ and 3/32" and 1/8" 7018

  4. #4
    Join Date
    Nov 2013
    Location
    Bay Area Cali
    Posts
    914
    Post Thanks / Like

    Re: Poor gear overlap

    90 on first gear should be around 45 on second.

    Sent from my SM-G930T using Tapatalk
    Long after the price is forgotten, the quality will remain.

    Both of my Poppy's 1954 Short Hoods -Third generation to weld with it and teaching a fourth
    SA 2## - Bought and sold more than I can remember or care to list, 8 in the shop right now

  5. #5
    Join Date
    Mar 2015
    Location
    NE Kansas
    Posts
    40
    Post Thanks / Like

    Re: Poor gear overlap

    Thanks, I appreciate it! This is the first pipeliner I've ever owned so I'm still trying to figure things out

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,309,941.59872 seconds with 13 queries