Results 1 to 10 of 10

Thread: SA200 heat question?

  1. #1
    Join Date
    Dec 2016
    Posts
    24
    Post Thanks / Like

    SA200 heat question?

    So I recently got my SA200 welding and have noticed that when I weld I am a lot hotter than on my buzz box. What I mean is 125 amps on my SA200 feels way colder than 125amps on my buzz box. Is this normal with sa200?

  2. #2
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,453
    Post Thanks / Like

    Re: SA200 heat question?

    The sa will have a much smoother and softer arc than your buzz box. Don't pay too much attention to numbers. If you need more heat, turn it up a little.
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  3. #3
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,407
    Post Thanks / Like

    Re: SA200 heat question?

    I would imagine your buzz box is an AC only machine in which case your arc characteristics are going to be a bit different than the DC of the SA200.

    Also, are the SA exciter and main brushes in good condition and both armature commutators clean? Fine Voltage control rheostat winding surface clean?
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  4. #4
    Join Date
    Dec 2016
    Posts
    24
    Post Thanks / Like

    Re: SA200 heat question?

    Everything is pretty clean, and my buzz box has ex. Thanks guys I will just go on how it feels

  5. #5
    Join Date
    Dec 2016
    Posts
    24
    Post Thanks / Like

    Re: SA200 heat question?

    *DC I mean

  6. #6
    Join Date
    Nov 2013
    Location
    Livingston, New Jersey, United States
    Posts
    1,090
    Post Thanks / Like

    Re: SA200 heat question?

    Quote Originally Posted by duaneb55 View Post
    I would imagine your buzz box is an AC only machine in which case your arc characteristics are going to be a bit different than the DC of the SA200.

    Also, are the SA exciter and main brushes in good condition and both armature commutators clean? Fine Voltage control rheostat winding surface clean?
    Duane how do you go about cleaning the Voltage​ rheostat winding surface. Thank you
    John

    Sent from my XT1254 using Tapatalk

  7. #7
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,407
    Post Thanks / Like

    Re: SA200 heat question?

    Fine sandpaper or Scotch-Brite on the winding surface where the wiper contacts.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  8. #8
    Join Date
    Nov 2013
    Location
    Livingston, New Jersey, United States
    Posts
    1,090
    Post Thanks / Like

    Re: SA200 heat question?

    Quote Originally Posted by duaneb55 View Post
    Fine sandpaper or Scotch-Brite on the winding surface where the wiper contacts.
    Thanks I have never done that so I am going to.
    John

    Sent from my XT1254 using Tapatalk

  9. #9
    Join Date
    Jun 2013
    Location
    BC Canada
    Posts
    113
    Post Thanks / Like

    Re: SA200 heat question?

    Quote Originally Posted by Nathan114312 View Post
    So I recently got my SA200 welding and have noticed that when I weld I am a lot hotter than on my buzz box. What I mean is 125 amps on my SA200 feels way colder than 125amps on my buzz box. Is this normal with sa200?
    Don't forget your 125 amps can be obtained on two different heat settings combined with the appropriate fine currant adjustment. Each will give you different arc characteristics.
    piece of soapstone
    tape measure
    chipping hammer (wire handle type)
    tip cleaners

  10. #10
    Join Date
    May 2014
    Location
    Southern Illinois
    Posts
    846
    Post Thanks / Like

    Re: SA200 heat question?

    I run 7018 Excalibur at around 125. On my Redface SA I usually am in 3rd gear around 50. If I want a drier puddle I go to 4th and 10-20. The fine adjustment controls volts ( heat) in the puddle. For wetter puddle turn volts up, drier puddle turn it down and selecting a higher gear (coarse adjust).


    Sent from my iPhone using Tapatalk
    Steve

    1990 Miller Dialarc 250
    1993 Miller Maxstar 140 STR
    2015 Lincoln MP210
    1966 Lincoln SA200 Redface

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,994,457.59519 seconds with 11 queries