+ Reply to Thread
Results 1 to 2 of 2

Thread: Powcon Remote Controller RH-100M

  1. #1
    Join Date
    Dec 2011
    Posts
    21
    Post Thanks / Like

    Powcon Remote Controller RH-100M

    The RH-100M is a hand-held Powcon remote with two knobs; it's shaped sort of like a hammerhead shark. One knob is a rotary switch with off and on positions and the other is a potentiometer with a 1-10 scale. My particular example has a cord with a 17-pin male Amphenol connector.

    Does anyone have experience with this controller or a manual? I'd like to know which Powcon machines and welding processes with which it's compatible.

    I plugged it into a 400smt set to scratch start tig and with its Contactor and Weld Level panel switches both set to Remote. After turning on both the power source and the remote the amps display on the panel did vary with turning the pot on the remote. Haven't tried welding with it yet--didn't want to turn out the lights in San Jose.

    I disassembled the RH-100M thinking I'd duplicate its design or use its components to make a 17-pin tig pedal for the 400smt. Turned out to be a little more intricate than I expected. The pot is an ordinary 10K single turn item, but the rotary switch has two tiers of 12 terminals each. Most of the terminals are jumpered together and the switch isn't wired in a complex way, but it seemed like a fancy component being used for a mundane purpose. There are also two diodes in RH-100M which had me scratching my head.

    Anyway, if you know what these things are supposed to do please let me know.

    Thanks in advance.

    One more related question: Just how is a tig pedal for a 17-pin 400smt wired up?

  2. #2
    Join Date
    Sep 2013
    Location
    whitewater, mt.
    Posts
    879
    Post Thanks / Like

    Re: Powcon Remote Controller RH-100M

    Talk to the guys at arcon welding.
    Arcon Workhorse 300MS
    Powcon 400SMT
    Powcon SM400 x 2
    Powcon SM300
    1968 SA200 Redface
    1978 SA250 Diesel
    Miller Super 32P Feeder
    Pre 1927 American 14" High Duty Lathe
    K&T Milwaukee 2H Horizontal Mill

    Bryan

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,263,954.42834 seconds with 17 queries