    I have a powermax 1250 that is about 15-17 years old but with very little use and have discovered the retaining cap has to be loosened about a turn and retightend every time to use the torch or the machine faults. What is going on? T80 torch.

  2. #2
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    375
    Post Thanks / Like

    Re: question for Jim Colt

    Safety feature so that you can't fire the torch with the consumables off or loose. If you take the front end parts off you can see the sensor. May even be the cap.

  3. #3
    Join Date
    Aug 2006
    Location
    St. Paul Park MN
    Posts
    892
    Post Thanks / Like

    Re: question for Jim Colt

    Yeah I had the whole torch head apart thinking I was chasing a broken wire then discovered I have to loosen the retainer cap about a turn and re tighten every time to get it to fire off.

  4. #4
    Join Date
    Aug 2006
    Location
    St. Paul Park MN
    Posts
    892
    Post Thanks / Like

    Re: question for Jim Colt

    I also discovered this morning if the trigger is teased enough times it will eventually light off with out loosening and re tightening retaining cap.

  5. #5
    Join Date
    Oct 2007
    Location
    New Hampshire, North Carolina
    Posts
    3,336
    Post Thanks / Like

    Re: question for Jim Colt

    When the cap is overly tightened it can crush the swirl ring (which controls gas flow and is a slide bearing for the blowback electrode), impeding the movement of the electrode. First...you may want to replace the swirl ring, and make a habit of just snugging the cap until you feel some slight resistance. Jim Colt Hypertherm

  6. #6
    Join Date
    Aug 2006
    Location
    St. Paul Park MN
    Posts
    892
    Post Thanks / Like

    Re: question for Jim Colt

    Thanks Jim. All working fine now. Are all the parts still available for the T-80? Looking around on the internet for parts I see sellers are saying that torch is obsolete.

  7. #7
    Join Date
    Oct 2007
    Location
    New Hampshire, North Carolina
    Posts
    3,336
    Post Thanks / Like

    Re: question for Jim Colt

    Consumables and torch repair parts are still available. The torch assembly is not....as it has been replaced by the Duramax torch...same price, longer consumable life, better cut quality and better long term reliability. Jim Colt

    Quote Originally Posted by lars66 View Post
    Thanks Jim. All working fine now. Are all the parts still available for the T-80? Looking around on the internet for parts I see sellers are saying that torch is obsolete.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,593,839,137.43289 seconds with 13 queries