Man it didn't take long for this to go down hill
From the testing I did it worked as well as most tig welders in this price range, they did make thing standard as suggested like the 1/2" dinse and 5/8" x 18 argon fittings as well as updating to a real CK 17FX torch.
Anyway for anyone that would like to have some info on this unit here is some.
10 to 225 amps, AC/DC w/pulse, 120/240 volt, pre and post flow, Ck flex head torch 12 1/2' SF hose with 1/2" dinse with 5/8"x18 standard argon fittings.
Duty cycle 120 volt
TIG 40% @ 140, 100% @ 108
MMA 40% @ 120, 100% @ 76
Duty cycle 240 volt
TIG 40% @ 225, 100% @ 155
MMA 40% @ 180, 100% @ 139
3 Year warranty
For more info contact Primeweld @
primeclickllc@gmail.com
Sold by a seller here in the USA and has been around for a few years has good feedback.