Well I cant help Myself...I picked up a Used ( maybe used an Hour) Powermax 30 air. This machine is new. Iím very impressed with the size and with the built in air compressor . I cut some 3/8 plate today like cutting butter. My hats off to Hypertherm on this machine. Well Done ! Ill post a few pics later the week.