    I need TIG welding done to one of the frame rails that had a small crack(1/4 inch crack).Please let me know if anyone would be able to help me with that.
    Attached Images Attached Images  

  2. #2
    Join Date
    Aug 2018
    Posts
    15
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    Frame is fixed now looking for help in replacing radiator support assembly.I will be paying decent price for the help

  3. #3
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    3,741
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    Quote Originally Posted by goodbadboys9 View Post
    Frame is fixed now looking for help in replacing radiator support assembly.I will be paying decent price for the help
    You should probably be speaking with an auto body shop for this type work as the liability exposure is great. Citing that car was a salvage purchase carries inherent risk to/for the repair facility. As a private individual, I wouldn't touch it citing the liability exposure even though the repair is very straightforward and I've done literally dozens of radiator support replacements over the years.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  4. #4
    Join Date
    Aug 2004
    Location
    North Central Indiana
    Posts
    6,160
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    It looks like there may have been a crack, but the smooth straight line on the left side appears to be made by a saw and the roundness of the gap at the bottom right side of the hole suggests a die grinder was used to open up the crack. IMO. Go to settings and enter where you live.
    Last edited by tackit; 09-22-2018 at 10:20 AM.

  5. #5
    Join Date
    Aug 2018
    Posts
    15
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    Got it.Right now car is in hop getting new RAD Support Installed.Thanks for the support

  6. #6
    Join Date
    Aug 2004
    Location
    North Central Indiana
    Posts
    6,160
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    Quote Originally Posted by goodbadboys9 View Post
    Got it.Right now car is in hop getting new RAD Support Installed.Thanks for the support
    Post a pic of the frame repair, it would be interesting to see how it was fixed.

  7. #7
    Join Date
    Jun 2020
    Posts
    1
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    Still relevant proposal?

  8. #8
    Join Date
    Aug 2020
    Posts
    2
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    Sorry to bring up an old topic, it's very interesting what condition the repaired frame is in after two years. I hope the author of the theme is still in the forum and can show you a photo...

  9. #9
    Join Date
    Sep 2020
    Posts
    4
    Post Thanks / Like

    Re: Need welding help in Central,NJ

    It seems to me that it is unlikely that this work can be done qualitatively...

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,603,141,022.21865 seconds with 12 queries