    Miller XMT 304 cc/cv multiprocess maching

    hello, I am currently attending a welding class and we are currently using a Miller XMT 304 cc/cv machine. I am having the hardest time with contamination regardless of what I do. I feel like it is the lift-start or scratch start that is causing the tungsten to become contaminated. I have tried using the HF (high-frequency) start but it does not seen to work without touching the tungsten to the work piece. Can anyone help me with either figuring out what is causing the contamination or can you suggest a better way to get the HF start to work I'd greatly appreciate it.

    Justin.

  2. #2
    Join Date
    Jun 2018
    Location
    Florida
    Posts
    616
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    Whatever your paying for that school is too much, where your instructor?
    ***********************

    CR

  3. #3
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,424
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    Welcome!
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  4. #4
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    2,966
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    There s no high frequency start on an XMT304 as far as I know. DC only machine, so no need. Try not using any lift start and just scratch starting. Are you using a pedal, or just setting amperage on the machine?

  5. #5
    Join Date
    Oct 2018
    Posts
    4
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    I was using the pedal at first but that only seem to make it worse as the tungsten would stick if it touched the work piece for to long. I did start to use the amps and that helps a bit but it still gets contaminated and I usually have to grind the tungsten back down after each weld. Super annoying and wasting all my tungsten. I will try switching over to the scratch start and see if that makes a difference. Not really impressed with the machine at all.

  6. #6
    Join Date
    Oct 2018
    Posts
    4
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    I believe it should have HF start as there is a setting just for TIG, then there is two more settings for lift start and scratch start.

  7. #7
    Join Date
    Oct 2014
    Posts
    956
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    If it had HF that was working there would be no need to touch the tungsten to anything.

  8. #8
    Join Date
    May 2007
    Posts
    3,270
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    [QUOTE=walker;8656195]There s no high frequency start on an XMT304

    thats right, find a piece of flat copper plate, place it next to ur location of weld start, scratch start off the copper lightly, and drag ur arc off it to the start point of weld. u/no one, will find any evidence of contination. and like the other(s) said, wheres ur teacher, and tell us about this situation/money being paid?
    Last edited by 123weld; 11-05-2018 at 11:44 PM.

  9. #9
    Join Date
    Oct 2018
    Posts
    4
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    The scratch start seems to help a bit, but still getting contamination, not nearly as bad though. Teacher is there but doesn't seem to care much. School is CNM (Central New Mexico) community college. I thinks this course was $200? It's a split simester. Took oxyweldig/cutting the first half and now taking intro TIG the last half.

  10. #10
    Join Date
    May 2007
    Posts
    3,270
    Post Thanks / Like

    Re: Miller XMT 304 cc/cv multiprocess maching

    Quote Originally Posted by Jmed800 View Post
    The scratch start seems to help a bit, but still getting contamination, not nearly as bad though. Teacher is there but doesn't seem to care much. School is CNM (Central New Mexico) community college. I thinks this course was $200? It's a split simester. Took oxyweldig/cutting the first half and now taking intro TIG the last half.
    sounds like u guys are lil confused. maybe teacher needs to join welding web

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,606,151,535.23815 seconds with 11 queries