    Welding 3/8 aluminum with cost in mind

    First off I wanna say I had no idea what to title this thread with...

    I'm looking for a machine to weld some fairly thick aluminum with. Up to 3/8 of an inch is probably as thick as I'll need to go. I priced out a Lincoln 260 mig with a push-pull gun. It's a little more than I'd like to spend right now. I started looking at higher amperage tig welders and I was wondering what would be the best bang for my buck. Going with an older machine, no bells or whistles... but cheaper, or going with a new machine? I already have a 175 square wave that works great for thin stuff, I just need something with a few more amps for the thick stuff... . The work is mostly on rectangular tube, going to be welded in position and there's a fair amount of welding to tie all the tubes together. Just looking for some opinions. Thanks!
    Last edited by Kebab; 12-26-2018 at 11:35 PM.

  2. #2
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Syncrowave 250. It’s a 310 amp machine

  3. #3
    Join Date
    Jun 2018
    Posts
    14
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by motolife313 View Post
    Syncrowave 250. It’s a 310 amp machine
    There's a guy who's somewhat local selling an older syncrowave 250 with a liquid cooler for $3800. I can also get an Everlast 325ext with a cooler brand new for about the same price. Would you recommend the older machine in that case?

  4. #4
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,741
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    That's grossly over priced.

    My mid 90's syncrowave 350 with cooler cost $1800 including freight.

    My Airco 300 was $225...
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  5. #5
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    5,839
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Kebab View Post
    There's a guy who's somewhat local selling an older syncrowave 250 with a liquid cooler for $3800. I can also get an Everlast 325ext with a cooler brand new for about the same price. Would you recommend the older machine in that case?
    Hell For 3800 you can buy a HTP221

    Ive seen used Syncro 250’s for 1500 bucks.




    Sent from my iPhone using Tapatalk Pro
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  6. #6
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,076
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    I'd find a used Lincoln 256 or Millermatic 252 with a spoon gun. You don't necessarily need a push pull gun to MIG aluminum.
    Syncrowave 250
    Purox Metalmaster

  7. #7
    Join Date
    Jun 2018
    Posts
    14
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    I kinda forgot to mention that I'm in canada also... . Our maple syrup dollar isn't that great right now, so all those prices are CAD. However $3800 still does seem a little high

  8. #8
    Join Date
    Jun 2018
    Posts
    14
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    For example the Everlast single phase 325ext on the American site shows $2799 USD... On the Canadian site in Canukbucks is $3700

  9. #9
    Join Date
    Jun 2016
    Location
    Back to the jungle
    Posts
    4,038
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Louie1961 View Post
    I'd find a used Lincoln 256 or Millermatic 252 with a spoon gun. You don't necessarily need a push pull gun to MIG aluminum.
    Yup. I seldom wire up my TIG any more. Too easy to grab my spool and plus into my Mm200

  10. #10
    Join Date
    Dec 2018
    Location
    CT
    Posts
    82
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    FYI i have a syncrowave 250 at home and have welded 1/2" AL in my garage more than a few times. It will require a 100 amp breaker at the panel if you've got the machine cranked up. You will want to AR/helium mix when it gets that thick.
    Welding --- My paid hobby!

  11. #11
    Join Date
    Dec 2015
    Location
    Western New York State, USA
    Posts
    2,000
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Kebab View Post
    First off I wanna say I had no idea what to title this thread with...

    I'm looking for a machine to weld some fairly thick aluminum with. Up to 3/8 of an inch is probably as thick as I'll need to go. I priced out a Lincoln 260 mig with a push-pull gun. It's a little more than I'd like to spend right now. I started looking at higher amperage tig welders and I was wondering what would be the best bang for my buck. Going with an older machine, no bells or whistles... but cheaper, or going with a new machine? I already have a 175 square wave that works great for thin stuff, I just need something with a few more amps for the thick stuff... . The work is mostly on rectangular tube, going to be welded in position and there's a fair amount of welding to tie all the tubes together. Just looking for some opinions. Thanks!
    .
    .
    depends on amount of welding. obviously you can stick weld aluminum but most people know you need bigger rod for anything over 1/4" thick. 5/32 and 3/16" aluminum stick rod is harder to get usually special order.
    .
    for the same reason all aluminum welding requires relatively much much higher amps. if you use 1/8 stick rod usually weld starts are cold and its difficult to easily get a decent weld without some serious preheating. like if you Tig weld thick aluminum at 250 amps or more who could possibly think you can stick weld with a lot less than that in amps and not have lack of heat problems. and 1/8 aluminum stick rod is far too small to use anywhere near those amp levels.

  12. #12
    Join Date
    Jul 2008
    Posts
    2,680
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by John T View Post
    Hell For 3800 you can buy a HTP221
    ...with a whopping 20% DC at 220A!

    Better bring your weed burner!
    Syncrowave 250DX
    Miller 330 A/BP
    Miller Big Blue 251D

  13. #13
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    1,133
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    what's the thinnest aluminium you'll want to weld?

  14. #14
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Kebab View Post
    There's a guy who's somewhat local selling an older syncrowave 250 with a liquid cooler for $3800. I can also get an Everlast 325ext with a cooler brand new for about the same price. Would you recommend the older machine in that case?
    Older ones usually go for 1800+ with bottle and everything making it turn key. You will wanna stick with the known to last brands.

  15. #15
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by John T View Post
    Hell For 3800 you can buy a HTP221

    Ive seen used Syncro 250’s for 1500 bucks.




    Sent from my iPhone using Tapatalk Pro
    Those htp 221’s go for what 2400? Which is a inverter btw and inverters are known to brake much faster then a transformer

  16. #16
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    5,839
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by motolife313 View Post
    Those htp 221’s go for what 2400? Which is a inverter btw and inverters are known to brake much faster then a transformer
    Brilliant


    Sent from my iPhone using Tapatalk Pro
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  17. #17
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Must not of did your homework john

  18. #18
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    5,839
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by motolife313 View Post
    Must not of did your homework john
    If you’re trying to somehow badmouth the HTP221
    Good luck. It’s one of the most well respected tig welders out there.

    Pick another battle, genius


    Sent from my iPhone using Tapatalk Pro
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  19. #19
    Join Date
    Mar 2010
    Location
    East Tennessee
    Posts
    1,234
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by motolife313 View Post
    Must not of did your homework john
    You didn't either, spell check?

  20. #20
    Join Date
    Mar 2010
    Location
    East Tennessee
    Posts
    1,234
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    I'd be looking at a miller dynasty 280dx. The inverter technology makes for much better results and ease of use. Any machine can crap out including the heavy power hungry transformer machines.

  21. #21
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    John doesn’t seem like u know what your taking about 3800 is what a dynasty 200-210 goes for not a htp. And it’s a fact inverters will die long before a transformer. Look how many dynasty’s die. Just ask terry. Sorry John you are getting all defensive and feel this way. I’m just throwing out facts.

  22. #22
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Showdog75 View Post
    I'd be looking at a miller dynasty 280dx. The inverter technology makes for much better results and ease of use. Any machine can crap out including the heavy power hungry transformer machines.
    The inverter has a much higher break down rate

  23. #23
    Join Date
    Jul 2008
    Posts
    2,680
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    I'll never understand why people insist on trying to weld heavy aluminum with $35 Chinee inerter soldering irons...it's like trying to go into the gravel hauling business with a four-cylinder Chevy S-10.

    Just because it can be done, doesn't mean you should try!

  24. #24
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,653
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Showdog75 View Post
    You didn't either, spell check?


    Thanks for letting me know. I’ll keep an eye on it

  25. #25
    Join Date
    Jun 2016
    Location
    Back to the jungle
    Posts
    4,038
    Post Thanks / Like

    Re: Welding 3/8 aluminum with cost in mind

    Quote Originally Posted by Kelvin View Post
    ...with a whopping 20% DC at 220A!

    Better bring your weed burner!
    My weed burner says Victor USA and the ability to pre-heat is an asset to EVERY welderator playing with thicker alumininimum....or a bigass chunk of cast .

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,610,977,068.13232 seconds with 12 queries